The impurities and lanthanum behavior at directional solidification of single-crystal superalloys

Min P.G., Sidorov V.V., Vadeev V.E.
Min P.G., Sidorov V.V., Vadeev V.E. The impurities and lanthanum behavior at directional solidification of single-crystal superalloys // Proceedings of VIAM. 2017. No. 7. DOI: 10.18577/2307-6046-2017-0-7-4-4. URL: https://www.viam-works.ru/en/journal/2017/7/4
Keywords
silicon, phosphorus, ceramic, mold, superalloy, impurities, directional solidification, refinement, neutralization.
Abstract

The silicon, phosphorus and lanthanum behavior during directional solidification of single-crystals ZhS32-VI and VZhM5-VI superalloys for gas turbine blades was studied.

It is proved that saturation with silicon during directional solidification of single-crystals took place for a reason of interaction of carbon with free silicon oxide included in the composition of the ceramic mold. It is founded that saturation with silicon of non-carbon single-crystal alloys occurs four times slower than carbon-containing alloys. The utilization of non-carbon nickel-based superalloys is recommended for high pure provision from silicon impurity and guaranteed high properties of casts.

Experimentally established that lanthanum microalloying of nickel-based superalloys with high phosphorus contain (0,014 wt. %) allows to increase high temperature strength of single-crystals on account strong, refractory compound (lanthanum phosphide) and neutralization harmful phosphorus influence. It is shown that repeated remelting leads to a change in the content of macro- and microalloying elements and consequently reduction in the amount of γ¢-phase and single-crystals service life.

It is recommended to remelt nickel-based superalloys in vacuum induction furnace with optimal composition control by chemical express analysis for provision guaranteed high operational of single-crystals.

Reference list
  1. Tigrova G.D., Korkka S.I., Grebcova T.M. Vliyanie kremniya na fazovyj sostav splavov na nikelevoj osnove [Influence of silicon on phase composition of nickel-based alloys] // Metallovedenie i termicheskaya obrabotka metallov. 1980. №4. S. 38–41.
  2. Sidorov V.V., Morozova G.I., Petrushin N.V. i dr. Fazovyj sostav i termostabilnost litejnogo zharoprochnogo nikelevogo splava s kremniem [Phase structure and thermostability of cast heat resisting nickel alloy with silicon] // Metally. 1990. №1. S. 94–98.
  3. Sidorov V.V., Rigin V.E., Min P.G., Folomejkin Yu.I., Timofeeva O.B., Filonova E.V., Ishodzhanova I.V. Vliyanie primesej na strukturu i svojstva vysokozharoprochnyh litejnyh splavov i razrabotka effektivnyh metodov ustraneniya ih otricatelnogo vliyaniya [Influence of impurity on structure and property of high-heat resisting cast alloys and development of effective methods of elimination of their negative influence] // Novosti materialovedeniya. Nauka i tehnika: elektron. nauch.-tehnich. zhurn. 2014. №2. St. 03. Available at: http://www.materialsnews.ru (accessed: March 07, 2017).
  4. Sidorov V.V., Rigin V.E., Min P.G., Folomejkin Yu.I. Vliyanie fosfora i kremniya na strukturu i svojstva vysokozharoprochnyh litejnyh splavov i razrabotka effektivnyh metodov ustraneniya ih otricatelnogo vliyaniya [Influence of phosphorus and silicon on structure and properties of high-heat resisting cast alloys and development of effective methods of elimination of their negative influence] // Metallovedenie i termicheskaya obrabotka metallov. 2015. №6 (720). S. 55–59.
  5. Sidorov V.V., Rigin V.E., Min P.G., Folomeikin Yu.I. Effect of phosphorus and silicon on structure and properties of highly refractory cast alloys and development of effective methods for eliminating their unfavorable effect // Metal Science and Heat Treatment. 2015. Vol. 57. No. 5–6. P. 364–368.
  6. Chao Yuan, Fengshi Yin. Effect of Phosphorus on Microstructure and High Temperature Properties of a cast Ni-base Superalloy // J. mater Sci. Technol. 2002. Vol. 18. No. 6. P. 555–557.
  7. Kablov E.N., Ospennikova O.G., Sidorov V.V., Rigin V.E. Proizvodstvo lityh prutkovyh (shihtovyh) zagotovok iz sovremennyh litejnyh vysokozharoprochnyh nikelevyh splavov [Production of cast bar (blend) preparations from modern cast high-heat resisting nickel alloys] // Problemy i perspektivy razvitiya metallurgii i mashinostroeniya s ispolzovaniem zavershennyh fundamentalnyh issledovanij i NIOKR: Tr. Vseros. nauch.-tehnich. konf. k 310-letiyu Uralskoj metallurgii. 2011. S. 31–38.
  8. Sidorov V.V., Rigin V.E., Timofeeva O.B., Min P.G. Vliyanie kremniya i fosfora na zharoprochnye svojstva i strukturno-fazovye prevrashheniya v monokristallah iz vysokozharoprochnogo splava VZhM4-VI [An effect of silicon and phosphorus on high temperature properties and structure-phase transformations of single crystals of VGM4-VI superalloy] // Aviacionnye materialy i tehnologii. 2013. №3. S. 32–38.
  9. Litye lopatki gazoturbinnyh dvigatelej: splavy, tehnologii, pokrytiya /pod red. E.N. Kablova [Cast blades of gas turbine engines: alloys, technologies, coverings / ed. by E.N. Kablov]. M.: Hauka, 2006. 632 s.
  10. Sidorov V.V., Min P.G., Burcev V.T., Kablov D.E., Vadeev V.E. Kompyuternoe modelirovanie i eksperimentalnoe issledovanie reakcij rafinirovaniya v vakuume slozhnolegirovannyh renijsoderzhashhih nikelevyh rasplavov ot primesej sery i kremniya [Computer modeling and pilot study of reactions of refinement in vacuum of complex-alloyed rhenium containing nickel melt from sulfur and silicon impurity] // Vestnik RFFI. 2015. №1 (85). S. 32–36.
  11. Min P.G., Sidorov V.V., Kablov D.E., Vadeev V.E. Rafinirovanie monokristallicheskih zharoprochnyh nikelevyh splavov ot primesej sery i kremniya i nejtralizaciya vrednogo vliyaniya fosfora [Refining of single-crystal superalloys to remove a sulfur and silicon impurity and eliminating unfavorable effect of phosphorus] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2017. №4 (52). St. 04. Available at: http://www.viam-works.ru (accessed: May 25, 2017). DOI: 10.18577/2307-6046-2017- 0-4-4-4.
  12. Sidorov V.V., Kablov D.E., Min P.G., Vadeev V.E. Rafinirovanie slozhnolegirovannogo nikelevogo splava ZhS32-VI ot primesi kremniya i fosfora putem odnonapravlennogo zatverdevaniya rasplava pri malyh skorostyah peremeshheniya fronta kristallizacii [Refinement of complex-alloyed ZhS32-VI nickel alloy from silicon and phosphorus impurity by unidirectional hardening melt with small traverse speeds of the front of crystallization] // Tehnologiya metallov. 2016. №3. S. 2–7.
  13. Min P.G., Sidorov V.V., Vadeev V.E. Rafinirovanie monokristallicheskih nikelevyh zharoprochnyh splavov ot primesej kremniya, fosfora i sery metodom napravlennoj kristallizacii rasplava s vesma nizkoj skorostyu peremeshheniya fronta [The refining of nickel base single-crystal alloys from silicon, phosphorus and sulfur impurities by directed melt solidification with very slowed-up moving rate of the crystallization] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2017. №3 (51). St. 02. Available at: http://www.viam-works.ru (accessed: May 25, 2017). DOI: 10.18577/2307-6046-2017-0-3-2-2.
  14. Min P.G., Sidorov V.V., Kablov D.E., Rigin V.E., Vadeev V.E. Issledovanie sery i fosfora v litejnyh zharoprochnyh nikelevyh splavah i razrabotka effektivnyh sposobov ih rafinirovaniya [Sulfur and phosphorus research in cast heat resisting nickel alloys and development of effective ways of their refinement] // Tehnologiya metallov. 2015. №12. S. 2–9.
  15. Min P.G., Sidorov V.V. Opyt pererabotki litejnyh othodov splava ZhS32-VI na nauchno-proizvodstvennom komplekse VIAM po izgotovleniyu lityh prutkovyh (shihtovyh) zagotovok [The experience of GS32-VI alloy scrap recycling at the VIAM scientific and production complex for cast bars production] // Aviacionnye materialy i tehnologii. 2013. №4. S. 20–25.
  16. Kablov E.N., Ospennikova O.G., Sidorov V.V., Rigin V.E., Kablov D.E. Osobennosti tehnologii vyplavki sovremennyh litejnyh vysokozharoprochnyh nikelevyh splavov [Features of smelting technology of modern cast high-heat resisting nickel alloys] // Vestnik MGTU im. N.E. Baumana. Ser.: Mashinostroenie. 2011. №SP. C. 68–78.
  17. Sidorov V.V., Rigin V.E., Goryunov A.V., Min P.G., Kablov D.E. Poluchenie Re–Ru soderzhashhego splava s ispolzovaniem nekondicionnyh othodov [Receiving Re–Ru of containing alloy with use of unconditioned waste] // Metallurgiya mashinostroeniya. 2012. №3. S. 15–17.
  18. Min P.G., Vadeev V.E., Kramer V.V. Resursosberegayushhaya tehnologiya polucheniya deformiruemogo nikelevogo zharoprochnogo splava VZh175 s primeneniem nekondicionnyh othodov [Resource-saving technology of receiving deformable nickel VZh175 hot strength alloy using unconditioned waste] // Metallurg. 2016. №9. S. 88–94.
  19. Min P.G., Vadeev V.E., Kalicev V.A., Kramer V.V. Tehnologiya polucheniya deformiruemogo splava VZh175 dlya diskov GTD iz kondicionnyh othodov [Technology of receiving deformable alloy VZh 175 for disks GTE from conditioned waste] // Metallurg. 2015. №9. S. 76–80.
  20. Sidorov V.V., Rigin V.E., Goryunov A.V., Min P.G. Opyt pererabotki v usloviyah FGUP «VIAM» litejnyh othodov zharoprochnyh splavov, obrazuyushhihsya na motorostroitelnyh i remontnyh zavodah [Experience of processing in the conditions of FSUE «VIAM» of foundry waste of the hot strength alloys which are forming at engine-building and repair plants] // Metallurg. 2014. №1. S. 86–90.
  21. Min P.G., Vadeev V.E., Kalicev V.A., Kramer V.V. Rafinirovanie nekondicionnyh othodov deformiruemyh nikelevyh splavov v vakuumnoj indukcionnoj pechi [Refinement of unconditioned waste of deformable nickel alloys in the vacuum induction furnace] // Tehnologiya metallov. 2015. №4. S. 8–13.
  22. Min P.G., Goryunov A.V., Vadeev V.E. Sovremennye zharoprochnye nikelevye splavy i effektivnye resursosberegayushhie tehnologii ih izgotovleniya [Modern heat resisting nickel alloys and effective resource-saving technologies of their manufacturing] // Tehnologiya metallov. 2014. №8. S. 12–23.
  23. Kablov E.N., Sidorov V.V., Kablov D.E., Min P.G., Rigin V.E. Resursosberegayushhie tehnologii vyplavki perspektivnyh litejnyh i deformiruemyh superzharoprochnyh splavov s uchetom pererabotki vseh vidov othodov [Resource-saving smelting technologies of perspective cast and deformable superhot strength alloys taking into account processing of all types of waste] // Elektrometallurgiya. 2016. №9. S. 30–41.
  24. Sidorov V.V., Rigin V.E., Goryunov A.V., Min P.G. Processing Superalloy Foundry Waste Generated at Engine Building and Repair Plants: Experience of the All-Russia Research Institute of Aviation Materials // Metallurgist. 2014. Vol. 58. No. 1–2. P. 69–74.
  25. Sidorov V.V., Rigin V.E., Goryunov A.V., Min P.G. Resources-saving technology for recycling off-grade waste products cast from superalloys // Metallurgist. 2014. Vol. 58. No. 5–6. P. 360–366.
  26. Min P.G., Goryunov A.V., Vadeev V.E. Modern Nickel Superalloys and the Efficient Resource-Saving Technologies of Their Production // Russian Metallurgy (Metally). 2015. Vol. 2015. No. 13. P. 1060–1068.
  27. Kablov E.N., Sidorov V.V., Kablov D.E., Min P.G., Rigin V.E. Resource-Saving Technologies of Making Advanced Cast and Deformable Superalloys with Allowance for Processing All Types of Wastes // Russian Metallurgy (Metally). 2016. Vol. 2016. No. 12. P. 1187–1195.
  28. Ospennikova O.G., Min P.G., Vadeev V.E., Kalitsev V.A., Kramer V.V. Resursosberegayushhaya tehnologiya pererabotki nekondicionnyh othodov deformiruemogo splava VZh175 dlya diskov GTD [Resource-saving processing technology of off-grade scrap of wrought superalloy VG175 for GTE disks production] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №2. St. 01. Available at: http://www.viam-works.ru (accessed: May 25, 2017). DOI: 10.18577/2307-6046-2016-0-2-1-1.
  29. Min P.G., Sidorov V.V., Kablov D.E., Rigin V.E., Vadeev V.E. Vliyanie primesi na strukturu I mehanicheskie svoistva liteinyh nikelevyh zharoprochnih splavov I razrabotka effektivnyh sposobov ih rafinirovaniya [Influence of impurity on structure and mechanical properties of cast nickel hot strength alloys and development of effective ways of their refinement] // Klimovskie chteniya-2015. Perspektivnie napravleniya razvitiya aviadvigatelestroeniya. SPb.: Skifia-print, 2015. S. 275–283.
  30. Kablov D.E., Sidorov V.V., Min P.G., Vadeev V.E. Vliyanie primesej i lantana na ekspluatacionnye svojstva splava ZhS36-VI [Influence of impurity and lanthanum on operational properties of alloy ZhS36-VI] // Metallurgiya mashinostroeniya. 2015. №6. S. 19–23.
  31. Kablov D.E., Sidorov V.V., Min P.G., Puchkov Yu.A. Vliyanie lantana na kachestvo i ekspluatacionnye svojstva monokristallicheskogo zharoprochnogo nikelevogo splava ZhS36-VI [The lanthanum influence on quality and operational properties of single crystal nickel base ZhS36-VI superalloy] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №12. St. 02. Available at: http://www.viam-works.ru (accessed: May 25, 2017). DOI: 10.18577/2307-6046-2015-0-12-2-2.
  32. Kablov D.E., Sidorov V.V., Min P.G., Gerasimov V.V., Bondarenko Yu. A. Vliyanie primesej sery i fosfora na svojstva monokristallov zharoprochnogo splava ZhS36-VI i razrabotka effektivnyh sposobov ego rafinirovaniya [The sulfur and phosphorus influence on properties of single crystals GHS36-VI supperalloy and design of effective methods their refining] // Aviacionnye materialy i tehnologii. 2015. №3 (36). S. 3–9. DOI: 10.18577/2071-9140-2015-0-3-3-9.
  33. Kablov D.E., Belyaev M.S., Sidorov V.V., Min P.G. Vliyanie primesej sery i fosfora na malociklovuyu ustalost' monokristallov zharoprochnogo splava ZhS36-VI [The influence of sulfur and phosphorus impurities on low cycle fatigue of GhS36-VI alloy single crystals] // Aviacionnye materialy i tehnologii. 2015. №4 (37). S. 25–28. DOI: 10.18577/2071-9140-2015-0-4-25-28.
  34. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  35. Yakimovich P.V., Alekseev A.V., Min P.G. Opredelenie nizkih soderzhanij fosfora v zharoprochnyh nikelevyh splavah metodom ISP-MS [Determination of low phosphorus content in heat-resistant nickel alloys by ICP-MS method] // Trudy VIAM : elektron. nauch.-tehnich. zhurn. 2014. №10. St. 02. Available at: http://viam-works.ru (accessed: March 07, 2017). DOI: 10.18577/2307-6046-2014-0-10-2-2.