The research of local phosphorus and sulfur distribution in γ and γ'-phases of ZhS36-VI superalloy single-crystals
UDC
669.018.44:621.745.55
DOI
10.18577/2307-6046-2017-0-7-3-3
Article PDF (Russian)
(1.37 MB)
How to cite
Min P.G., Sidorov V.V., Kablov D.E., Vadeev V.E., Zaysev D.V. The research of local phosphorus and sulfur distribution in γ and γ'-phases of ZhS36-VI superalloy single-crystals // Proceedings of VIAM. 2017. No. 7. DOI: 10.18577/2307-6046-2017-0-7-3-3. URL: https://www.viam-works.ru/en/journal/2017/7/3
Keywords
phosphorus, sulfur, superalloy, single-crystal, impurities, neutralization, coherence, structure, lanthanum, long-term strength.
Abstract
The distribution of phosphorus and sulfur impurities in γ and γ'-phases of single-crystals was investigated by high-resolution transmission electron microscopy and micro X-ray spectral analysis. It is proved that impurities concentrates principally in γ-solid solution, and there are local areas of increased content in there. The nature of this distribution remains after high temperature long-term strength tests at that heterogeneity of sulfur content between (γ/γ')-phases becomes more pronounced, especially for alloy with high sulfur content. A mechanism for destruction of coherent coupling between γ- and γ'-phases at high impurities content and reducing of single-crystals high temperature strength was suggested.
Reference list
- Kablov E.N., Ospennikova O.G., Sidorov V.V., Rigin V.E. Proizvodstvo lityh prutkovyh (shihtovyh) zagotovok iz sovremennyh litejnyh vysokozharoprochnyh nikelevyh splavov [Production of cast bar (blend) preparations from modern cast high-heat resisting nickel alloys] // Problemy i perspektivy razvitiya metallurgii i mashinostroeniya s ispolzovaniem zavershennyh fundamentalnyh issledovanij i NIOKR: Tr. Vseros. nauch.-tehnich. konf. k 310-letiyu Uralskoj metallurgii. 2011. S. 31–38.
- Litye lopatki gazoturbinnyh dvigatelej: splavy, tehnologii, pokrytiya /pod red. E.N. Kablova [Cast blades of gas turbine engines: alloys, technologies, coverings / ed. by E.N. Kablov]. M.: Hauka, 2006. 632 s.
- Holt R.T., Wallace W. Impurities and Trace Elements in Nickel-Base Superalloys // Intern. metals reviews. 1976. Vol. 21. No. 1. P. 1–24.
- Kablov D.E., Sidorov V.V., Min P.G., Gerasimov V.V., Bondarenko Yu. A. Vliyanie primesej sery i fosfora na svojstva monokristallov zharoprochnogo splava ZhS36-VI i razrabotka effektivnyh sposobov ego rafinirovaniya [The sulfur and phosphorus influence on properties of single crystals GHS36-VI supperalloy and design of effective methods their refining] // Aviacionnye materialy i tehnologii. 2015. №3 (36). S. 3–9. DOI: 10.18577/2071-9140-2015-0-3-3-9.
- Sidorov V.V., Rigin V.E., Min P.G., Folomejkin Yu.I., Timofeeva O.B., Filonova E.V., Ishodzhanova I.V. Vliyanie primesej na strukturu i svojstva vysokozharoprochnyh litejnyh splavov i razrabotka effektivnyh metodov ustraneniya ih otricatelnogo vliyaniya [Influence of impurity on structure and property of high-heat resisting cast alloys and development of effective methods of elimination of their negative influence] // Novosti materialovedeniya. Nauka i tehnika: elektron. nauch.-tehnich. zhurn. 2014. №2. St. 03. Available at: http://www.materialsnews.ru (accessed: March 07, 2017).
- Min P.G., Sidorov V.V., Kablov D.E., Rigin V.E., Vadeev V.E. Issledovanie sery i fosfora v litejnyh zharoprochnyh nikelevyh splavah i razrabotka effektivnyh sposobov ih rafinirovaniya [Sulfur and phosphorus research in cast heat resisting nickel alloys and development of effective ways of their refinement] // Tehnologiya metallov. 2015. №12. S. 2–9.
- Min P.G., Sidorov V.V., Budinovskij S.A., Vadeev V.E. Vliyanie sery na zharostojkost monokristallov zharoprochnogo nikelevogo splava sistemy Ni–Al–Co–Re–Ta–Mo–W–Ru–Cr [Influence of sulfur on the heat resistance of monocrystals of heat resisting nickel alloy of Ni–Al–Co–Re–Ta–Mo–W–Ru–Cr system] // Materialovedenie. 2016. №7. S. 9–12.
- Kablov D.E., Sidorov V.V., Budinovskij S.A., Min P.G. Vliyanie primesi sery na zharostojkost monokristallov zharoprochnogo splava ZhS36-VI s zashhitnym pokrytiem [The influence of sulfur impurity on heat resistance of single crystals of ZhS36-VI alloy with protective coating] // Aviacionnye materialy i tehnologii. 2016. №1 (40). S. 20–23. DOI: 10.18577/2071-9140-2016-0-1-20-23.
- Min P.G., Sidorov V.V., Budinovskiy S.A., Vadeev V.E. Influence of Sulfur on Heat Resistance of Single Crystals of Heat-Resistant Nickel Alloy of Ni–Al–Co–Re–Ta–Mo–W–Ru–Cr System // Inorganic Materials: Applied Research. 2017. Vol. 8. No. 1. Р. 90–93.
- Sidorov V.V., Rigin V.E., Min P.G., Folomejkin Yu.I. Vliyanie fosfora i kremniya na strukturu i svojstva vysokozharoprochnyh litejnyh splavov i razrabotka effektivnyh metodov ustraneniya ih otricatelnogo vliyaniya [Influence of phosphorus and silicon on structure and properties of high-heat resisting cast alloys and development of effective methods of elimination of their negative influence] // MiTOM. 2015. №6 (720). S. 55–59.
- Kablov D.E., Belyaev M.S., Sidorov V.V., Min P.G. Vliyanie primesej sery i fosfora na malociklovuyu ustalost' monokristallov zharoprochnogo splava ZhS36-VI [The influence of sulfur and phosphorus impurities on low cycle fatigue of GhS36-VI alloy single crystals] // Aviacionnye materialy i tehnologii. 2015. №4 (37). S. 25–28. DOI: 10.18577/2071-9140-2015-0-4-25-28.
- Sidorov V.V., Rigin V.E., Timofeeva O.B., Min P.G. Vliyanie kremniya i fosfora na zharoprochnye svojstva i strukturno-fazovye prevrashheniya v monokristallah iz vysokozharoprochnogo splava VZhM4-VI [An effect of silicon and phosphorus on high temperature properties and structure-phase transformations of single crystals of VGM4-VI superalloy] // Aviacionnye materialy i tehnologii. 2013. №3. S. 32–38.
- Chao Yuan, Fengshi Yin. Effect of Phosphorus on Microstructure and High Temperature Properties of a cast Ni-base Superalloy // J. mater Sci. Technol. 2002. Vol. 18. No. 6. P. 555–557.
- Yaoxiao Zhu, John Radavich et al. Development and Long-Time Structural Stability of a Low Segregation Hf Free Superalloys – DZ 125L // Superalloys-2000. 2000. P. 329–339.
- Sidorov V.V., Min P.G., Burcev V.T., Kablov D.E., Vadeev V.E. Kompyuternoe modelirovanie i eksperimentalnoe issledovanie reakcij rafinirovaniya v vakuume slozhnolegirovannyh renijsoderzhashhih nikelevyh rasplavov ot primesej sery i kremniya [Computer modeling and pilot study of reactions of refinement in vacuum of complex-alloyed rhenium containing nickel melt from sulfur and silicon impurity] // Vestnik RFFI. 2015. №1 (85). S. 32–36.
- Kablov E.N., Sidorov V.V., Kablov D.E., Min P.G., Rigin V.E. Resursosberegayushhie tehnologii vyplavki perspektivnyh litejnyh i deformiruemyh superzharoprochnyh splavov s uchetom pererabotki vseh vidov othodov [Resource-saving smelting technologies of perspective cast and deformable superhot strength alloys taking into account processing of all types of waste] // Elektrometallurgiya. 2016. №9. S. 30–41.
- Min P.G., Vadeev V.E., Kalicev V.A., Kramer V.V. Rafinirovanie nekondicionnyh othodov deformiruemyh nikelevyh splavov v vakuumnoj indukcionnoj pechi [Refinement of unconditioned waste of deformable nickel alloys in the vacuum induction furnace] // Tehnologiya metallov. 2015. №4. S. 8–13.
- Ospennikova O.G., Min P.G., Vadeev V.E., Kalitsev V.A., Kramer V.V. Resursosberegayushhaya tehnologiya pererabotki nekondicionnyh othodov deformiruemogo splava VZh175 dlya diskov GTD [Resource-saving processing technology of off-grade scrap of wrought superalloy VG175 for GTE disks production] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №2. St. 01. Available at: http://www.viam-works.ru (accessed: May 25, 2017). DOI: 10.18577/2307-6046-2016-0-2-1-1.
- Sidorov V.V., Min P.G. Rafinirovanie slozhnolegirovannogo nikelevogo rasplava ot primesi sery pri plavke v vakuumnoj indukcionnoj pechi. Chast 1 [Refinement complex-alloyed nickel melt from sulfur impurity when melting in the vacuum induction furnace. Part 1] // Elektrometallurgiya. 2014. №3. S. 18–23.
- Sidorov V.V., Min P.G. Rafinirovanie slozhnolegirovannogo nikelevogo rasplava ot primesi sery pri plavke v vakuumnoj indukcionnoj pechi. Chast 2 [Refinement complex-alloyed nickel melt from sulfur impurity when melting in the vacuum induction furnace. Part 2] // Elektrometallurgiya. 2014. №5. S. 26–30.
- Sidorov V.V., Min P.G., Folomejkin Yu.I., Vadeev V.E. Vliyanie skorosti filtracii slozhnolegirovannogo nikelevogo rasplava cherez penokeramicheskij filtr na soderzhanie primesi sery v metalle [Influence of speed of filtering complex-alloyed nickel melt via the foam ceramic filter on the content of impurity of sulfur in metal] // Elektrometallurgiya. 2015. №5. S. 12–15.
- Min P.G., Sidorov V.V., Kablov D.E., Vadeev V.E. Rafinirovanie monokristallicheskih zharoprochnyh nikelevyh splavov ot primesej sery i kremniya i nejtralizaciya vrednogo vliyaniya fosfora [Refining of single-crystal superalloys to remove a sulfur and silicon impurity and eliminating unfavorable effect of phosphorus] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2017. №4. St. 04. Available at: http://www.viam-works.ru (accessed: May 25, 2017). DOI: 10.18577/2307-6046-2017- 0-4-4-4.
- Filippov K.S., Burcev V.T., Sidorov V.V., Rigin V.E. Issledovanie poverhnostnogo natyazheniya i plotnosti rasplava nikelya, soderzhashhego primesi sery, fosfora i azota [Research of surface tension and density melt the nickel containing impurity of sulfur, phosphorus and nitrogen] // Fizika i himiya obrabotki materialov. 2013. №1. S. 52–56.
- Kablov D.E., Sidorov V.V., Min P.G., Puchkov Yu.A. Vliyanie lantana na kachestvo i ekspluatacionnye svojstva monokristallicheskogo zharoprochnogo nikelevogo splava ZhS36-VI [The lanthanum influence on quality and operational properties of single crystal nickel base ZhS36-VI superalloy] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №12. St. 02. Available at: http://www.viam-works.ru (accessed: May 25, 2017). DOI: 10.18577/2307-6046-2015-0-12-2-2.
- Sidorov V.V., Rigin V.E., Min P.G., Folomeikin Yu.I. Effect of phosphorus and silicon on structure and properties of highly refractory cast alloys and development of effective methods for eliminating their unfavorable effect // Metal Science and Heat Treatment. 2015. Vol. 57. No. 5–6. Р. 364–368.
- Sidorov V.V., Rigin V.E., Min P.G., Folomejkin Yu.I. Issledovanie processov rafinirovaniya v vakuume slozhnolegirovannyh nikelevyh rasplavov ot primesi sery [Research of refining processes in vacuum complex-alloyed nickel melt from sulfur impurity] // Metally. 2015. №6. S. 57–63.
- Kablov D.E., Sidorov V.V., Min P.G., Vadeev V.E. Vliyanie primesej i lantana na ekspluatacionnye svojstva splava ZhS36-VI [Influence of impurity and lanthanum on operational properties of alloy ZhS36-VI] // Metallurgiya mashinostroeniya. 2015. №6. S. 19–23.
- Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Yakimovich P.V., Alekseev A.V., Min P.G. Opredelenie nizkih soderzhanij fosfora v zharoprochnyh nikelevyh splavah metodom ISP-MS [Determination of low phosphorus content in heat-resistant nickel alloys by ICP-MS method] // Trudy VIAM : elektron. nauch.-tehnich. zhurn. 2014. №10. St. 02. Available at: http://viam-works.ru (accessed: March 07, 2017). DOI: 10.18577/2307-6046-2014-0-10-2-2.
- Mehanik E.A., Min P.G., Gundobin N.V., Rastegaeva G.Yu. Opredelenie massovoj doli sery v zharoprochnyh nikelevyh splavah i stalyah v diapazone koncentracij ot 0,0001 do 0,0009% (po masse) [Determination of sulfur mass fraction in heat-resistant nickel alloy and steels within the concentration range from 0,0001 to 0,0009% wt.] // Trudy VIAM : elektron. nauch.-tehnich. zhurn. 2014. №9. St. 12. Available at: http://viam-works.ru (accessed: March 23, 2017). DOI: 10.18577/2307-6046-2014-0-9-12-12.
- Bokshtejn S.Z., Ginzburg S.S., Kishkin S.T., Razumovskij I.M., Stroganov G.B. Avtoradiografiya poverhnostej razdela i strukturnaya stabilnost splavov [Autoradiography of interfaces and structural stability of alloys]. M.: Metallurgiya, 1987. 272 s.
- Min P.G., Sidorov V.V., Vadeev V.E. Povedenie primesej i lantana pri napravlennoj kristallizacii monokristallov nikelevyh zharoprochnyh splavov [The impurities and lanthanum behavior at directional solidification of single-crystal superalloys] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2017. №7. URL: http://www.viam-works.ru (v pechati).