Electrolytic-plasma polishing of titanium alloys VT6 and VT8M-1

Dobrynin D.A.
Dobrynin D.A. Electrolytic-plasma polishing of titanium alloys VT6 and VT8M-1 // Proceedings of VIAM. 2017. No. 7. DOI: 10.18577/2307-6046-2017-0-7-2-2. URL: https://www.viam-works.ru/en/journal/2017/7/2
Keywords
electrolytic-plasma polishing, titanium alloy, vapor-gas shell, microdischarge.
Abstract

In the article, a comparative analysis of traditional methods of surface polishing (mechanical, chemical and electrochemical methods) with the electrolytic-plasma treatment method was carried out. Electrolytic-plasma polishing of the surface of samples from titanium alloys VT6 and VT8M-1 in a two-component electrolyte on the basis of hydrofluoric acid salts with a total concentration of no more than 5% by weight was carried out. The polishing rates of titanium alloys VT6 and VT8M-1 in the proposed electrolyte are determined. The influence of the duration of electrolytic-plasma polishing of the surface of samples from titanium alloys VT6 and VT8M-1 on the surface roughness parameter Ra was studied. The qualitative dependences of the polishing rates of the surface of titanium alloys VT6 and VT8M-1 on the concentration of electrolyte, its temperature and operating voltage are established.

Reference list
  1. Kablov E.N., Muboyadzhyan S.A. Erozionnostojkie pokrytiya dlya lopatok kompressora gazoturbinnyh dvigatelej [Erosion resistant coverings for compressor blades of gas turbine engines] // Elektrometallurgiya. 2016. №10. S. 23–38.
  2. Kablov E.N., Muboyadzhyan S.A., Budinovskij S.A., Pomelov Ya.A. Ionno-plazmennye zashhitnye pokrytiya dlya lopatok gazoturbinnyh dvigatelej [Ion-plasma protecting covers for blades of gas turbine engines] // Konversiya v mashinostroenii. 1999. №2. S. 42–47.
  3. Kablov E.N., Muboyadzhyan S.A. Ionno-plazmennye zashhitnye pokrytiya dlya lopatok GTD // Litye lopatki gazoturbinnyh dvigatelej: splavy, tehnologii, pokrytiya [Ion-plasma protecting covers for GTE blades]. M.: Nauka, 2006. S. 531–608.
  4. Kablov E.N., Muboyadzhyan S.A., Budinovskij S.A., Lucenko A.N. Ionno-plazmennye zashhitnye pokrytiya dlya lopatok gazoturbinnyh dvigatelej [Ion-plasma protecting covers for blades of gas turbine engines] // Metally. 2007. №5. S. 23–34.
  5. Muboyadzhyan S.A., Aleksandrov D.A., Gorlov D.S., Egorova L.P., Bulavinceva E.E. Zashhitnye i uprochnyayushhie ionno-plazmennye pokrytiya dlya lopatok i drugih otvetstvennyh detalej kompressora GTD [Protective and strengthening ion-plasma coverings for blades and other responsible details of the GTE compressor] // Aviacionnye materialy i tehnologii. 2012. №S. S. 71–81.
  6. Matveev P.V., Budinovskij S.A., Chubarov D.A. Tehnologiya polucheniya ionno-plazmennyh zharostojkih podsloev s povyshennym soderzhaniem alyuminiya dlya perspektivnyh TZP [Technology for production of ion-plasma heat-resistant bonding sub-layers with increased aluminum content for advanced TBCs] // Aviacionnye materialy i tehnologii. 2014. №S5. S. 56–60. DOI: 10.18577/2071-9140-2014-0-s5-56-60.
  7. Muboyadzhjan S.A., Galoyan A.G. Kompleksnye termodiffuzionnye zharostojkie pokrytiya dlya bezuglerodistyh zharoprochnyh splavov na nikelevoj osnove [Complex thermodiffusion heat resisting coatings for carbon-free hot strength alloys on nickel basis] // Aviacionnye materialy i tehnologii. 2012. №3. S. 25–30.
  8. Kablov E.N., Muboyadzhyan S.A. Zharostojkie i teplozashhitnye pokrytiya dlya lopatok turbiny vysokogo davleniya perspektivnyh GTD [Heat resisting and heat-protective coverings for turbine blades of high pressure of perspective GTE] // Aviacionnye materialy i tehnologii. 2012. №S. S. 60–70.
  9. Kablov E.N., Muboyadzhyan S.A., Budinovskij S.A., Yagodkin Yu.D. Perspektivy primeneniya ionno-plazmennoj tehnologii vysokih energij dlya mezhresursnogo remonta lopatok turbin [Perspectives of application of ion-plasma technology of high energy for interresource repair of blades of turbines] // Aviacionnye materialy i tehnologii. 2002. №1. S. 6–13.
  10. Galvanicheskie pokrytiya v mashinostroenii: spravochnik v 2 t. / pod red. M.A. Shlugera [Galvanic coverings in mechanical engineering: directory in 2 vol. / ed. by M.A. Shluger]. M.: Mashinostroenie, 1985. T. 1. 240 s.
  11. Kulikov I.S., Vashhenko S.V., Kamenev A.Ya. Elektrolitno-plazmennaya obrabotka materialov [Electrolit-plasma processing of materials]. Minsk: Belarus. navuka, 2010. 232 s.
  12. Grilihes S.Ya. Obezzhirivanie, travlenie i polirovanie metallov. 5-e izd., pererab. i dop. [Degreasing, etching and polishing of metals. 5th ed., rev. and add.]. L.: Mashinostroenie, 1983. 101 s.
  13. Pogrebnyak A.D., Tyurin Yu.N., Bojko A.G. i dr. Elektrolitno-plazmennaya obrabotka i nanesenie pokrytij na metally i splavy Electrolit-plasma processing and drawing coverings on metals and alloys] // Uspehi fiz. met. 2005. T. 6. S. 273–344.
  14. Volenko A.P., Bojchenko O.V., Chirkunova N.V. Elektrolitno-plazmennaya obrabotka metallicheskih izdelij [Electrolit-plasma processing of metal products] // Vektor nauki TGU. 2012. №4 (22). C. 144–147.
  15. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.