Efficiency of complex alloying AlSi10Mg type alloy with transition metals for selective laser melting technologies
Ivanova A.O., Zavodov A.V., Dynin N.V., Fomina M.A. Efficiency of complex alloying AlSi10Mg type alloy with transition metals for selective laser melting technologies // Proceedings of VIAM. 2017. No. 7. DOI: 10.18577/2307-6046-2017-0-7-1-1. URL: https://www.viam-works.ru/en/journal/2017/7/1
Keywords
AlSi10Mg alloy, SLM, transition metals, additive manufacturing, mechanical properties, microstructure.
Abstract
Аdditive manufacturing allows to obtain complex parts with improved material efficiency. Powders of AlSi10Mg alloy are the most widely used for production of various structural elements by selective laser melting (SLM) technology. For the expansion of application and improving service characteristics it is necessary to add small amount of transition metals into the alloys. This paper describes the efficiency of copper, cerium and zirconium additives for improving mechanical properties of AlSi10Mg type alloy.
Reference list
- Kablov E.N. Additivnye tehnologii – dominanta nacionalnoj tehnologicheskoj iniciativy [The additive technologies are the dominant of national technological initiative] // Intellekt i tehnologii. 2015. №2 (11). S. 52–55.
- Ryabov D.K., Antipov V.V., Korolev V.A., Medvedev P.N. Vliyanie tehnologicheskih faktorov na strukturu i svojstva silumina, poluchennogo s ispolzovaniem tehnologii selektivnogo lazernogo sinteza [Effect of technological factors on structure and properties of Al–Si alloy obtained by selective laser melting] // Aviacionnye materialy i tehnologii. 2016. №S1. S. 44–51. DOI: 10.18577/2071-9140-2016-0-S1-44-51.
- Ryabov D.K., Morozova L.V., Korolev V.A., Ivanova A.O. Izmenenie mehanicheskih svojstv splava AK9ch., poluchennogo po tehnologii selektivnogo lazernogo splavleniya [Alternation of mechanical features of alloy AK9ch manufactured by selective laser melting] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №9 (45). St. 02. Available at: http://www.viam-works.ru (accessed: May 25, 2017). DOI: 10.18577/2307-6046-2016-0-9-2-2.
- Ryabov D.K., Zajcev D.V., Dynin N.V., Ivanova A.O. Izmenenie struktury splava AK9ch., poluchennogo selektivnym lazernym spekaniem, v processe termicheskoj obrabotki [Alternation of structure of selective laser melted aluminum alloy AK9ch during heat treatment] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №9. St. 03. Available at: http://www.viam-works.ru (accessed: May 25, 2017). DOI: 10.18557/2307-6046-2016-0-9-3-3.
- Sercombe T., Schaffer G. Rapid manufacturing of aluminum components // Science, 2003. Vol. 301 (5637). Р. 1225–1227.
- Bremen S., Meiners W., Diatlov A. Selective Laser Melting // Laser Technik Journal. 2012. Vol. 9 (2). P. 33–38.
- Kablov E.N. Iz chego sdelat budushhee? Materialy novogo pokoleniya, tehnologii ih sozdaniya i pererabotki – osnova innovacij [What is the future to make of? Materials of new generation, technology of their creation and processing are the base of innovations] // Krylya Rodiny. 2016. №5. S. 8–18.
- Ivanova A.O., Ryabov D.K., Antipov V.V., Pahomkin S.I. Vozmozhnost' primeneniya programmnogo kompleksa Thermo-Calc dlya opredeleniya parametrov termicheskoj obrabotki splava 1913 i temperatur atomizacii alyuminievyh splavov [Application of Thermo-Calc software for determination of parameters of heat treatment 1913 alloy and temperatures of gas atomization for aluminium alloys] // Aviacionnye materialy i tehnologii. 2016. №S1. S. 52–59. DOI: 10.18577/2071-9140-2016-0-S1-52-59.
- Akopyan T.K., Zolotorevskij V.S., Hvan A.V. Raschet fazovyh diagramm sistem Al–Cu–Zn–Mg i Al–Cu–Zn–Mg–Fe–Si [Calculation of phase charts of Al-Cu-Zn-Mg and Al-Cu-Zn-Mg-Fe-Si systems] // Cvetnaya metallurgiya. 2013. №3. S. 44–51.
- Ivanova A.O., Vahromov R.O., Grigor'ev M.V., Senatorova O.G. Issledovanie vliyaniya malyh dobavok serebra na strukturu i svojstva resursnyh splavov sistemy Al–Cu–Mg [Effect of small additive of silver on structure and properties of Al–Cu–Mg alloys] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №10. St. 01. Available at: http://www.viam-works.ru (accessed: May 25, 2017). DOI: 10.18577/2307-6046-2014-0-10-1-1.
- Kablov E.N. Shestoj tehnologicheskij uklad [Sixth technological way] // Nauka i zhizn. 2010. №4. S. 2–7.
- Kolobnev N.I., Mahsidov V.V., Samohvalov S.V., Ryabov D.K. Vliyanie soderzhaniya antirekristallizatorov na strukturu i svojstva listov iz splava 1370 sistemy Al–Mg–Si–Cu–Zn [Influence of the contents anti recrystallizers on structure and properties of sheets from alloy 1370 Al-Mg-Si-Cu-Zn system] // Tehnologiya legkih splavov. 2012. №1. S. 18–24.
- Ryabov D.K., Kolobnev N.I., Kochubej A.Ya., Zavodov A.V. Izmenenie mehanicheskih svojstv listov iz splava 1913 pri vvedenii skandiya [Changing of mechanical properties of 1913 alloy sheets after scandium addition] // Aviacionnye materialy i tehnologii. 2014. №4. S. 3–8.
- Elagin V.I. Legirovanie deformirovannyh alyuminievyh splavov perehodnymi metallami [Alloying of the deformed aluminum alloys transition metals]. M.: Metallurgiya, 1975. 321 s.
- Ryabov D.K., Vakhromov R.O., Ivanova A.O. [An effect of small additions of elements with high solubility in aluminium on microstructure of ingots and cold-rolled sheets made of Al–Mg–Sc alloy] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №9. St. 05. Available at: http://www.viam-works.ru (accessed: May 25, 2017). DOI: 10.18577/2307-6046-2015-0-9-5-5
- Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Belov N.A., Savchenko S.V., Hvan A.V. Fazovyj sostav i struktura siluminov [Phase structure and structure of silumins]. M.: MISiS, 2008. S. 10–12.
- Galdin N.M., Cherenega D.F. Cvetnoe lite [Non-ferrous molding]. M.: Mashinostroenie, 1989. S. 20.
- Yali Li, Dongdong Gu. Parametric analysis of thermal behavior during selective laser smelting additive manufacturing of aluminum alloy powder // Materials and Design, 2014. Vol. 63. P. 856–867.
- Prashanth K.G., Scudino S., Klauss H.J. Microstructure and mechanical properties of Al–12Si produced by selective laser melting: Effect of heat treatment // Materials Science and Engineering, 2014. Vol. 590. P. 153–160.