Influence of the mode of roasting on structure and property of high-porous ceramic mullite materials

Buchilin N.V., Lyulyukina G.Yu., Varrik N.M.
Buchilin N.V., Lyulyukina G.Yu., Varrik N.M. Influence of the mode of roasting on structure and property of high-porous ceramic mullite materials // Proceedings of VIAM. 2017. No. 5. DOI: 10.18577/2307-6046-2017-0-5-4-4. URL: https://www.viam-works.ru/en/journal/2017/5/4
Abstract

Creation of high-temperature high-porous ceramic materials is one of actual problems now. The oxide porous ceramics has low heat conductivity, high resistance to oxidation and satisfactory durability therefore it is especially demanded in the metallurgical foundry fields of the industry as foam ceramic filters. The results of researches of sintering mullite porous ceramics with use of discrete mullite fibers are presented in this article. It is shown that the optimum range of temperatures of calcining for producing materials with open cellular porous structure is 1300–1350°C. It is determined that the essential role on mechanical characteristics of materials is rendered by the mode of preliminary heat treatment of fibers, and also composition of the sintering aid. Materials with the reported porosity to 85% and durability are produced at compression to 0,7 MPa.

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Buntushkin V.P., Kablov E.N., Bazyleva O.A., Morozova G.I. Splavy na osnove alyuminidov nikelya [Alloys on the basis of nickel aluminides] // MiTOM. 1999. №1. S. 32–34.
  3. Kablov E.N., Petrushin N.V., Svetlov I.L., Demonis I.M. Nikelevye litejnye zharoprochnye splavy novogo pokoleniya [Nickel foundry heat resisting alloys of new generation] // Aviacionnye materialy i tehnologii. 2012. №S. C. 36–52.
  4. Shliker dlya izgotovleniya penokeramicheskih filtrov: pat. 2084428 Ros. Federaciya. №93008852/03 [Slip for manufacturing of foam ceramic filters: pat. 2084428 Rus. Federation. №93008852/03]; zayavl. 18.02.93; opubl.20.07.97.
  5. Usovershenstvovannyj penokeramicheskij filtr dlya uluchsheniya filtrovaniya rasplavlennogo chuguna: pat. 2380138 Ros. Federaciya. №2008108220/15 [The advanced foam ceramic filter for improvement of filtering of molten iron: pat. 2380138 Rus. Federation. №2008108220/15]; zayavl. 04.08.06; opubl.27.01.10.
  6. High strength SiC filter and method for the manufacture thereof: pat. 6663776 USA. No. 10/256844; field 27.09.02; publ. 16.12.03.
  7. Keramicheskij filtr, soderzhashhij uglerodnoe pokrytie, i sposob ego izgotovleniya: pat. 2456056 Ros. Federaciya. №2010118514/03 [The ceramic filter containing carbon covering, and way of its manufacturing: pat. 2456056 Rus. Federation. №2010118514/03]; zayavl. 28.01.08; opubl. 20.07.12.
  8. Anciferov V.N. Problemy poroshkovogo materialovedeniya. Chast II [Problems of powder materials science. Part II]. Ekaterinburg: UrO RAN, 2002. 263 s.
  9. Sandoval M.L., Camerucci M.A. Foaming performance of aqueous albumin and mullite-albumin systems used in cellular ceramic processing // Ceramics International. 2014. Vol. 40. P. 1675–1686.
  10. Magnani G., Brentari A., Burresi E., Raiteri G. Pressureless sintered silicon carbide with enhanced mechanical properties obtained by the two-step sintering method // Ibid. P. 1759–1763.
  11. Yang W., Jiang B., Wang A., Shi H. Effect of Negatively Charged Ions on the Formation of Microarc Oxidation Coating on 2024 Aluminium Alloy // Journal of Material Science and Technology. 2012. Vol. 28 (8). P. 707–712.
  12. Aminzare M., Mazaheri M., Golestanifard F. et al. Sintering behavior of nano alumina powder shaped by pressure filtration // Ceramics International. 2011. Vol. 37. P. 9–14.
  13. Himicheskaya tehnologiya keramiki: uch. posobie dlya vuzov / pod red. I.Ya. Guzmana [Chemical technology of ceramics: the manual for higher education institutions ]. M.: Strojmaterialy, 2003. 496 s.
  14. Kablov E.N., Shchetanov B.V., Ivahnenko Yu.A., Balinova Yu.A. Perspektivnye armiruyushhie vysokotemperaturnye volokna dlya metallicheskih i keramicheskih kompozicionnyh materialov [Perspective reinforcing high-temperature fibers for metal and ceramic composite materials] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №2. St. 05. Available at: http://www.viam-works.ru (accessed: April 07, 2017).
  15. Shchetanov B.V., Balinova Yu.A., Lyulyukina G.Yu., Soloveva E.P. Struktura i svojstva nepreryvnyh polikristallicheskih volokon α-Al2O3 [Structure and properties of continuous polycrystalline fibers α-Al2O3] // Aviacionnye materialy i tehnologii. 2012. №1. S. 13–17.
  16. Uvarova N.E., Grashhenkov D.V., Isaeva N.V., Orlova L.A., Sarkisov P.D. Vysokotemperaturnye radioprozrachnye materialy: segodnya i zavtra [High-temperature radio transparent materials: today and tomorrow] // Aviacionnye materialy i tehnologii. 2010. №1. S. 16–21.
  17. Kirienko T.A., Balinova Yu.A. Fiziko-himicheskie svojstva mnogokomponentnyh rastvorov dlya keramicheskih materialov, soderzhashhih polivinilovyj spirt [Physical and chemical properties of multicomponent solutions for ceramic materials containing polyvinyl alcohol] // Aviacionnye materialy i tehnologii. 2014. №1. S. 34–38. DOI: 10.18577/2071-9140-2014-0-1-34-38.
  18. Nikitina V.J., Kolyshev S.G., Kuptsov R.S. Sposoby opredeleniya ploshhadi secheniya monokristallicheskih volokon Al2O3 dlya rascheta prochnosti pri rastyazhenii [The methods of determination of Al2O3 single-crystal fibers cross-section area for tensile strength calculation] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №2. St. 03. Available at: http://www.viam-works.ru (accessed: April 07, 2017). DOI: 10.18577/2307-6046-2014-0-2-3-3.
  19. Balinova Yu.A., Shheglova T.M., Lyulyukina G.Yu., Timoshin A.S. Osobennosti formirovaniya α-Al2O3 v polikristallicheskih voloknah s soderzhaniem oksida alyuminiya 99% v prisutstvii dobavok Fe2O3, MgO, SiO2 [Features of formation α-Al2O3 in polycrystalline fibers containing 99% alumina doped with Fe2O3, MgO, SiO2] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №3. St. 03. Available at: http://www.viam-works.ru (accessed: April 07, 2017). DOI: 10.18577/2307-6046-2014-0-3-3-3.
  20. Evteev A.A., Makarov N.A., Lemeshev D.O., Zhitnyuk S.V. Keramika v sisteme ZrO2–Al2O3 s dobavkami evtekticheskih sostavov [Ceramics in ZrO2-Al2O3 system with additives of eutectic structures] // Steklo i keramika. 2011. №8. S. 23–27.
  21. Tehnologiya stekla / pod red. I.I. Kitajgorodskogo. 3-e izd. [The technology has flown down / ed. by I.I. Kitajgorodskiy. 3rd ed.]. M.: Gos. izd-vo lit. po str-vu, arhit. i stroit. materialam 1961. 517 s.
  22. Buchilin N.V., Prager E.P. Reologicheskie harakteristiki shlikernyh suspenzij na osnove oksida alyuminiya [Rheology of alumina-based slurry suspensions] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №5. St. 06. Available at: http://www.viam-works.ru (accessed: April 07, 2017). DOI: 10.18577/2307-6046-2015-0-5-6-6.
  23. Vogt U.F., Gorbar M. et al. Improving the properties of ceramic foams by a vacuum infiltration process // Journal of the European Ceramic Society. 2010. Vol. 30. P. 3005–3011.
  24. Evteev A.A., Lemeshev D.O., Zhitnyuk S.V., Makarov N.A. Raschet optimalnyh rezhimov obzhiga keramiki na osnove oksidov cirkoniya i alyuminiya [Calculation of optimum modes of roasting of ceramics on the basis of zirconium oxides and aluminum] // Steklo i keramika. 2014. №8. S. 15–21.
  25. Bakunov V.S., Lukin E.S. Osobennosti spekaniya oksidnoj keramiki [Features of agglomeration of the oxidized ceramics] // Steklo i keramika. 2011. №7. S. 9–13.