Rheological properties of the thermoplastic composition with a reduced fire hazard polycarbonate-based: depending on the temperature processing; effect on mechanical properties and stability dimension objects created software FDM-technology

Petrova G.N., Larionov S.A., Sapego Yu. A., Platonov M.M.
Petrova G.N., Larionov S.A., Sapego Yu. A., Platonov M.M. Rheological properties of the thermoplastic composition with a reduced fire hazard polycarbonate-based: depending on the temperature processing; effect on mechanical properties and stability dimension objects created software FDM-technology // Proceedings of VIAM. 2017. No. 4. DOI: 10.18577/2307-6046-2017-0-4-9-9. URL: https://www.viam-works.ru/en/journal/2017/4/9
Keywords
rheology, melt viscosity, 3D-printing, fused deposition modeling (FDM), polycarbonate, a modification processing.
Abstract

The article presents the results of studies on the dependence of the rheological properties developed by FSUE «VIAM» thermoplastic composition based on modified polycarbonate compared to ABS-plastic and polyamide Nylon-618, widely used nowadays for 3D-printing. It is shown that increase in data processing temperatures of the materials leads to a reduction of melt viscosity. It is found that the modified polycarbonate has a large value of melt viscosity, which determines its higher processing temperature than ABS-plastic. The optimum processing temperature of the materials. It is shown that in the selected temperature range processing strength and deformation properties are maximal, and shrinkage – minimum value. The results will significantly reduce the time to perfect the mode of 3D-printing and to improve the quality of manufactured products.

Reference list
  1. Kablov E.N. Strategicheskie napravleniya razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda [The strategic directions of development of materials and technologies of their processing for the period to 2030] // Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  2. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  3. Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace materials science] // Vse materialy. Enciklopedicheskij spravochnik. 2008. №3. S. 2–14.
  4. Petrova G.N., Bejder E.Ya., Starostina I.V. Litevye termoplasty dlya izdelij aviacionnoj tehniki [Injection molding thermoplastics for products of aviation engineering] // Vse materialy. Enciklopedicheskij spravochnik. 2016. №6. S. 10–15.
  5. Kryzhanovskij V.K., Burlov V.V., Panimatchenko A.D., Kryzhanovskaya Yu.V. Tehnicheskie svojstva polimernyh materialov [Engineering properties of polymeric materials]. SPb.: Professiya, 2005. 240 s.
  6. Petrova G.N., Barbotko S.L., Bejder E.Ya. i dr. Pozharobezopasnye litevye termoplasty [Fireproof injection molding thermoplastics] // Plasticheskie massy. 2006. №1. S. 46–48.
  7. Petrova G.N., Beider E.Ya., Perfilova D.N., Rumyantseva T.V. Pozharobezopasnye litevye termoplasty i termojelastoplastyv [Fire safety of injection molding thermoplastics and TPE materials] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №11. St. 02. Available at: http://www.viam-works.ru (accessed: February 07, 2017).
  8. Mihajlin Yu.A. Termoustojchivye polimery i polimernye materialy na ih osnove [Thermosteady polymers and polymeric materials on their basis] // Polimernye materialy. 2005. №4. S. 29–32
  9. Petrova G.N., Beider E.Yа. Construction materials based on reinforced thermoplastics Chemistry and Materials Science // Russian Journal of General Chemistry. 2011. Vol. 81. No. 5. Р. 1001–1007.
  10. Gryaznov V.I., Petrova G.N., Yurkov G.Yu., Buznik V.M. Smesevye termojelastoplasty so specialnymi svojstvami [Thermoplastic mixtures with special properties] // Aviacionnye materialy i tehnologii. 2014. №1. S. 25–29. DOI: 10.18577/2071-9140-2014-0-1-25-29.
  11. Komarov G.A. Sostoyanie, perspektivy i problemy primeneniya PKM v tehnike [Condition, perspectives and problems of application of PCM in equipment] // Polimernye materialy. 2009. №2. S. 5–9.
  12. Postnov V.I., Pletin I.I., Veshkin E.A., Starostina I.V., Strelnikov S.V. Tehnologicheskie osobennosti proizvodstva tonkolistovyh obshivok lopastej vertoleta iz konstrukcionnogo stekloplastika VPS-53K [Technological features of production of thin sheet coverings of blades of the helicopter from constructional VPS-53K fibreglass] // Izvestiya Samarskogo nauchnogo centra Rossijskoj akademii nauk. 2016. T. 18. №4 (3). S. 619–627.
  13. Petrova G.N., Zhuravleva P.L., Iskhodzhanova I.V., Beider E.Ya. Influence of Carbon Fillers on Properties and Structure of Polyethylene-Based Polymer Composites // Nanotechnologies in Russia. 2014. Vol. 9. No. 5–6. Р. 305–310.
  14. Kablov E.N., Semenova L.V., Petrova G.N., Larionov S.A., Perfilova D.N. Polimernye kompozicionnye materialy na termoplastichnoj matrice [Polymeric composite materials on thermoflexible matrix] // Izvestiya vuzov. Ser.: Himiya i himicheskaya tehnologiya. 2016. T. 59. №10. S. 61–71.
  15. Kerber M.L., Vinogradov V.M., Golovkin G.S. i dr. Polimernye kompozicionnye materialy: struktura, svojstva, tehnologiya [Polymeric composite materials: structure, properties, technology]. SPb.: Professiya, 2011. S. 32–33.
  16. Petrova G.N., Starostina I.V., Rumyanceva T.V. Issledovanie vozmozhnosti markirovki detalej iz polikarbonata [Study of the possibility of marking parts of polycarbonate] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №10. St. 11. Available at: http://www.viam-works.ru (accessed: February 08, 2017). DOI: 10.18577/2307-6046-2016-0-10-11-11.
  17. Petrova G.N., Beyder E.Ya. Povyshenie ognestojkosti polibutilentereftalata (obzor) [Increasing of fire resistance of polybutylene terephthalate (review)] // Aviacionnye materialy i tehnologii. 2014. №4. S. 58–64. DOI: 10.18577/2071-9140-2014-0-4-58-64.
  18. Mihajlin Yu.A. Termoustojchivye polimery i polimernye materialy [Thermosteady polymers and polymeric materials]. SPb.: Professiya, 2006. S. 29–30.
  19. Sudarushkin Yu.K., Gudimov M.M., Romanov D.S., Sokolov M.Yu. Primenenie lit'evyh polikarbonatov v aviapriborostroenii [Application of injection molding polycarbonates in avionics] // Aviacionnaya promyshlennost. 2003. №2. S. 48–52.
  20. Smirnov O.I., Skorodumov S.V. Modelirovanie tehnologii poslojnogo sinteza pri razrabotke izdelij slozhnoj formy [Modeling of technology of level-by-level synthesis when developing products of difficult form] // Sovremennye naukoemkie tehnologii. 2010. №4. S. 83–87.
  21. Bikas H., Stavropoulos P., Chryssolouris G. Additive manufacturing methods and modeling approaches: a critical review // International Journal of Advanced Manufacturing Technology. 2016. Vol. 83. C. 389–405. DOI: 10.1007/s00170-015-7576-2.
  22. Platonov M.M., Petrova G.N., Larionov S.A., Barbotko S.L. Polimernaya kompoziciya na osnove polidodekalaktama dlya tehnologii 3D-pechati rasplavlennoj polimernoj nityu [Polymer composition on the basis of polydodecanolactam for 3D-printing technology by melted polymer string] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №10. St. 09. Available at: http://www.viam-works.ru (accessed: February 08, 2017). DOI: 10.18577/2307-6046-2016-0-10-9-9.
  23. Novakova-Marcincinova L., Kuric I. Basic and Advanced Materials for Fused Deposition Modeling Rapid Prototyping Technology // Manufacturing and Industrial Engineering. 2012. Vol. 11(1). P. 24–27.
  24. Croccolo D., De Agostinis M., Olmi G. Experimental characterization and analytical modelling of the mechanical behavior of fused deposition processed parts made of ABS-M30 // Computational Materials Science. 2013. Vol. 79. P. 506–518. DOI: 10.1016/j.commatsci.2013.06.041.
  25. Turner B., Strong R., Gold S. A review of melt extrusion additive manufacturing processes: I. Process design and modeling // Rapid Prototyping Journal. 2014. No. 20/3. P. 192–204. DOI: 10.1108/RPJ-01-2013-0012.
  26. Durgun I., Ertan R. Experimental investigation of FDM process for improvement of mechanical properties and production cost // Ibid. P. 228–235. DOI: 10.1108/RPJ-10-2012-0091.
  27. Petrova G.N., Platonov M.M., Bolshakov V.A., Ponomarenko S.A. Issledovanie kompleksa harakteristik bazovyh materialov dlya FDM-tehnologii additivnogo sinteza. Fiziko-mehanicheskie i teplofizicheskie svojstva [Research of complex of characteristics of base materials for FDM technology of the additive synthesis. Physicomechanical and heatphysical properties] // Plasticheskie massy. 2016. №5–6. S. 53–59.
  28. Normy letnoj godnosti samoletov transportnoj kategorii [Standards of the flight validity of airplanes of transport category]: AP-25: utv. Postanovleniem 28-j Sessii po aviacii i ispolzovaniyu vozdushnogo prostranstva 11.12.2008. 3-e izd. s popravkami 1–7. M.: Aviaizdat, 2014. 278 s.
  29. Barbotko S.L. Pozharobezopasnost aviacionnyh materialov [Fire safety of aviation materials] // Aviacionnye materialy i tehnologii. 2012. №S. S. 431–439.
  30. Petrova G.N., Rumyanceva T.V., Beyder E.Ya. Vliyanie modificiruyushhih dobavok na pozharobezopasnye svojstva i tehnologichnost polikarbonata [Influence of modifying additives on fireproof properties and technological effectiveness of polycarbonate] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №6. St. 06. Available at: http://www.viam-works.ru (accessed: February 08, 2017).
  31. Mikulenok I.O. Opredelenie reologicheskih svojstv termoplastichnyh kompozicionnyh materialov [Definition of rheological properties of thermoflexible composite materials] // Plasticheskie massy. 2011. №7. S. 26–30.
  32. Golovkin G.S. Sistematizaciya tehnologicheskih svojstv polimerov i materialov na ih osnove [Ordering of technological properties of polymers and materials on their basis] // Polimernye materialy: izdeliya, oborudovanie, tehnologii. 2012. №7. S. 20–31.
  33. Shah V. Spravochnoe rukovodstvo po ispytaniyam plastmass i analizu prichin ih razrusheniya [Reference guide on tests of plastic and the analysis of the reasons of their destruction]. SPb.: NOT, 2009. S. 229–230.
  34. Bortnikov V.G. Raschet reologicheskih harakteristik rasplavov polimerov s ispol'zovaniem pokazatelya tekuchesti [Calculation of rheological characteristics rasplavov polymers with use of indicator of flowability] // Vserossijskaya Molodezhnaya nauchnaya shkola, posvyashhennaya laureatam nobelevskih premij po himii. Kazan, 2011. S. 23–25.
  35. Rao Natti S., Shot Nik R. Tehnologicheskie raschety i pererabotka plastmass: Prakticheskoe rukovodstvo. Per. s angl. [Technological calculations and processing of plastic: Practical guidance. trans from Engl.]. SPb.: Professiya, 2013. S. 198.
  36. Dul S., Fambri L., Pegoretti A. Fused deposition modelling with ABS-graphenenanocomposites // Composites: Part A. 2016. Vol. 85. P. 181–191. DOI: 10.1016/j.compositesa.2016.03.013.
  37. Riddick J.C., Haile M.A., Wahlde R.V. et al. Fractographic analysis of tensile failure of acrylonitrile-butadiene-styrene fabricated by fused deposition modeling // Additive Manufacturing. 2016. Vol. 11. P. 49–59. DOI: 10.1016/j.addma.2016.03.007.
  38. Kablov E.N. Osnovnye itogi i napravleniya razvitiya materialov dlya perspektivnoj aviacionnoj tehniki [The main results and the directions of development of materials for perspective aviation engineering] // Aviacionnye materialy. 75 let. Izbrannye trudy «VIAM» 1932–2007: yubil. nauch.-tehnich. sb. M.: VIAM, 2007. S. 20–26.
  39. Kablov E.N. Rossii nuzhny materialy novogo pokoleniya [Materials of new generation are necessary to Russia] // Redkie zemli. 2014. №3. S. 8–13.