The development of casting heat-resistant aluminum alloys (To the 120th anniversary since the birth of I.F. Kolobnev)

Ogorodov D.V., Trapeznikov A.V., Popov D.A., Pentuykhin S.I.
Ogorodov D.V., Trapeznikov A.V., Popov D.A., Pentuykhin S.I. The development of casting heat-resistant aluminum alloys (To the 120th anniversary since the birth of I.F. Kolobnev) // Proceedings of VIAM. 2017. No. 2. DOI: 10.18577/2307-6046-2017-0-2-12-12. URL: https://www.viam-works.ru/en/journal/2017/2/12
Keywords
casting heat-resistant aluminum alloys, silumin, high-temperature aluminum alloys, high-strength aluminum alloys, corrosion-resistant aluminum alloys.
Abstract

The article presents the main stages of work activities of Ivan Philippovich Kolobnev, as well as alloys developed under his leadership. The prospects of development of casting high-temperature, high-strength and corrosion-resistant aluminum alloys are shown. Experience accumulated by Kolobnev in the development of high-temperature aluminum alloys is now being implemented in the framework of the complex research area 8.4. «High-strength corrosion-resistant weldable magnesium and cast aluminum alloys for the new generation aerospace technologies» («The strategic directions of development of materials and technologies of their reprocessing for the period till 2030»)

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the develop-ment of materials and technologies of their processing for the period until 2030»] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace materials science] // Vse materialy. Entsiklopedicheskiy spravochnik. 2008. №3. S. 2–14.
  3. Kablov E.N. Rossii nuzhny materialy novogo pokoleniya [Materials of new generation are necessary to Russia] // Redkie zemli. 2014. №3. S. 8–13.
  4. Goncharenko E.S., Trapeznikov A.V., Ogorodov D.V. Litejnye alyuminievye splavy (k 100-letiyu so dnya rozhdeniya M.B. Altmana) [Aluminium casting alloys] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №4. St. 02. Available at: http://www.viam-works.ru (accessed: January 25, 2016). DOI: 10.18577/2307-6046-2014-0-4-2-2.
  5. Kornysheva I.S., Volkova E.F., Goncharenko E.S., Muhina I.Yu. Perspektivy primeneniya magnievyh i litejnyh alyuminievyh splavov [Perspectives of application of magnesium and cast aluminum alloys] // Aviacionnye materialy i tehnologii. 2012. №S. S. 212–222.
  6. Antipov V.V. Strategiya razvitiya titanovyh, magnievyh, berillievyh i alyuminievyh splavov [Strategy of development of titanium, magnesium, beryllium and aluminum alloys] //Aviacionnye materialy i tehnologii. 2012. №S. S. 157–167.
  7. Alyuminievye splavy v aviakosmicheskoy tekhnike [Aluminum alloys in aerospace equipment] / pod obshch. red. E.N. Kablova M.: Nauka, 2001. 192 s.
  8. Kolobnev I.F., Altman M.B. Gazovaya poristost i metody borby s ney v alyuminievykh otlivkakh [Gas porosity and methods of fight against it in aluminum casting]. M.: ITEIN, 1948. 49 s.
  9. Kolobnev I.F. Fasonnoe lite alyuminievykh splavov [Shaped casting of aluminum alloys]. M.: Mashgiz, 1953. 266 s.
  10. Lebedev V.M., Melnikov A.V., Postnikov N.S., Cherkasov V.V. Vysokoeffektivnye liteynye alyuminievye splavy [Highly effective cast aluminum alloys] // Aviatsionnye materialy na rubezhe XX–XXI vekov: nauch.-tekhn. sb. M.: VIAM, 1994. S. 101–105.
  11. Kolobnev I.F. Liteynye alyuminievye splavy [Cast aluminum alloys]. M.: Oborongiz, 1961. 112 s.
  12. Altman M.B. Metallurgiya liteynykh alyuminievykh splavov [Metallurgy of cast aluminum alloys]. M.: Metallurgiya, 1972. 153 s.
  13. Kolobnev I.F. Zharoprochnost' liteynykh alyuminievykh splavov [Thermal stability of cast aluminum alloys]. 2-e izd. M.: Metallurgiya, 1973. 320 s.
  14. Kolobnev I.F. i dr. Vysokoprochnyy germetichnyy splav V124 [High-strength tight alloy В124]. M.: GOSNINTI, 1969. 29 s.
  15. Altman M.B., Stromskaya N.P. Povyshenie svoystv standartnykh liteynykh alyuminievykh splavov [Increase of properties of standard cast aluminum alloys]. M.: Metallurgiya, 1984. 128 s.
  16. Goncharenko E.S., Kornysheva I.S. Perspektivy primeneniya otlivok iz alyuminievykh splavov [Perspectives of application of otlivka from aluminum alloys] // Liteynoe proizvodstvo. 2012. №1. S. 21–23.
  17. Goncharenko E.S., Kornysheva I.S. Otlivki iz alyuminievykh splavov. Issledovaniya, materialy, tekhnologii [Casting from aluminum alloys. Researches, materials, technologies] // Liteynoe proizvodstvo. 2013. №2. S. 2–4.
  18. Kolobnev I.F. Termicheskaya obrabotka alyuminievykh splavov [Thermal processing of aluminum alloys]. 2-e izd. M.: Metallurgiya, 1966. 396 s.
  19. Duyunova V.A., Goncharenko E.S., Mukhina I.Yu., Uridiya Z.P., Volkova E.F. Nauchnoe nasle-die akademika I.N. Fridlyandera. Sovremennye issledovaniya magnievykh i liteynykh alyu-minievykh splavov [Scientific heritage of academician I.N.Fridlyandera. Modern researches of magnesium and cast aluminum alloys] // Tsvetnye metally. 2013. №9. S. 71–78.
  20. Goncharenko E.S., Alyabev I.P., Trapeznikov A.V., Ogorodov D.V. Poluchenie otlivok iz splava VAL20 putem optimizatsii konstruktsii detaley izdeliy OAO «Tupolev» [Receiving otlivka from alloy ВАЛ20 by optimization of design of details of products of JSC Tupolev] // Trudy VIAM: elektron. nauch.-tekhnich. zhurn. 2014. №8. St. 01. Available at: http://www.viam-works.ru (accessed: January 25, 2016). DOI: 10.18577/2307-6046-2014-0-8-1-1.