The influence of ion implantation on the damping ability of the composition «аlloy–ion-plasma coating»

Gorlov D.S., Muboyadzhyan S.A., Shchepilov A.A., Aleksandrov D.A.
Gorlov D.S., Muboyadzhyan S.A., Shchepilov A.A., Aleksandrov D.A. The influence of ion implantation on the damping ability of the composition «аlloy–ion-plasma coating» // Proceedings of VIAM. 2017. No. 2. DOI: 10.18577/2307-6046-2017-0-2-4-4. URL: https://www.viam-works.ru/en/journal/2017/2/4
Keywords
ion implantation, assisted deposition, ion-plasma coating damping, damping capacity, good quality, metallographic researches.
Abstract

The possibility to use ion implantation in assistiveware deposition of ion-plasma damping coatings in one technological cycle is shown. The influence of ion implantation of argon on the damping ability of the composition of titanium alloy VT6 with damping coating and without it to reduce the oscillation amplitude of the free end of the samples during vibrodynmic bench tests on the first flexural mode is analyzed. The surface roughness of the samples of titanium alloy VT6 before and after applying the damping covering are studied. Metallographic researches of titanium alloy VT6 with a damping coating before and after tests on damping ability are carried out. This work was performed within the framework of strategic directions 17. «Comprehensive anticorrosion protection, hardening, wear-resistant protective and heat-resistant coatings», сomplex problem 17.3. «Multilayer heat-resistant and heat-resistant coatings, nanostructural hardening erosion and corrosion-resistant, wear-resistan

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Hirvonen Dzh.K. Ionnaya implantaciya [Ion implantation]. M.: Metallurgiya, 1985. 19 s.
  3. Shorr B.F., Serebryakov N.N. Raschetno-eksperimentalnyj analiz amplitudno-zavisimyh harakteristik dempfirovaniya v detalyah i materialah [The rated and experimental analysis of amplitude and dependent characteristics of damping in details and materials] // Problemy mashinostroeniya i nadezhnosti mashin. №3. 2011. S. 91–99.
  4. Muravchenko F.M., Sheremetev A.V. Aktualnye problemy dinamiki, prochnosti i nadezhnosti sovremennyh aviadvigatelej [Actual problems of dynamics, durability and reliability of modern aircraft engines] // Vibracii v tehnike i tehnologiyah. 2001. №4 (20). S. 2–5.
  5. Ustinov A.I., Movchan B.A., Skorodzievskij V.S. Issledovanie dempfiruyushhej sposobnosti ploskih obrazcov iz titanovogo splava Ti–6%Al–4%V s pokrytiyami iz olova i ittriya [Research of damping capacity of flat samples from Ti-6%Al-4%V titanium alloy with coverings from tin and yttrium] // Problemy prochnosti. 2001. №4. S. 55–61.
  6. Muboyadzhyan S.A., Pomelov Ya.A. Zashhitnye pokrytiya dlya lopatok kompressora GTD [Protecting covers for GTE compressor blades] // Aviacionnye materialy i tehnologii. M.: VIAM, 2003. Vyp.: Vysokozharoprochnye materialy dlya sovremennyh i perspektivnyh gazoturbinnyh dvigatelej i progressivnye tehnologii ih proizvodstva. S. 116–131.
  7. Sposob polucheniya litogo trubnogo katoda iz splavov na osnove alyuminiya dlya ionno-plazmennogo naneseniya pokrytij: pat. 2340426 Ros. Federaciya [Way of receiving the cast pipe cathode from alloys on the basis of aluminum for ion-plasma drawing coverings: pat. 2340426 Rus. Federation]; opubl. 16.04.07.
  8. Sposob polucheniya lityh trubnyh izdelij iz splavov na osnove nikelya i/ili kobalta: pat. 2344019 Ros. Federaciya [Way of receiving cast tubular goods from alloys on the basis of nickel and/or cobalt: pat. 2344019 Rus. Federation]; opubl. 16.04.07.
  9. Kablov E.N., Ospennikova O.G., Bazyleva O.A. Materialy dlya vysokonagruzhennyh detalej gazoturbinnyh dvigatelej [Materials for the high-loaded details of gas turbine engines] // Vestnik MGTU im. N.E. Baumana. Ser.: Mashinostroenie. 2011. №SP2. S. 13–19.
  10. Ospennikova O.G. Strategiya razvitiya zharoprochnyh splavov i stalej specialnogo naznacheniya, zashhitnyh i teplozashhitnyh pokrytij [Strategy of development of hot strength alloys and steels special purpose, protective and heat-protective coverings] // Aviacionnye materialy i tehnologii. 2012. №S. S. 19–36.
  11. Ustanovka dlya naneseniya zashhitnyh pokrytij: pat. 2318078 Ros. Federaciya [Installation for drawing protecting covers: pat. 2318078 Rus. Federation]; opubl. 26.06.06.
  12. Kablov E.N., Ospennikova O.G., Vershkov A.V. Redkie metally i redkozemelnye elementy – materialy sovremennyh i budushhih vysokih tehnologij [Rare metals and rare-earth elements are materials for modern and future high technologies] // Aviacionnye materialy i tehnologii. 2013. №S2. S. 3–10.
  13. Sibileva S.V., Karimova S.A. Obrabotka poverhnosti titanovyh splavov s celyu obespecheniya adgezionnyh svojstv [Surface treatment of titanium alloys to provide adhesion properties] // Aviacionnye materialy i tehnologii. 2013. №S2. S. 25–35.
  14. Muboyadzhyan S.A., Aleksandrov D.A., Gorlov D.S., Egorova L.P., Bulavinceva E.E. Zashhitnye i uprochnyayushhie ionno-plazmennye pokrytiya dlya lopatok i drugih otvetstvennyh detalej kompressora GTD [Protective and strengthening ion-plasma coverings for blades and other responsible details of the GTE compressor] //Aviacionnye materialy i tehnologii. 2012. №S. S. 71–81.
  15. Kashapov O.S., Pavlova T.V., Nochovnaya N.A. Vliyanie rezhimov termicheskoj obrabotki na strukturu i svojstva zharoprochnogo titanovogo splava dlya lopatok KVD [Influence of modes of thermal processing on structure and property of heat resisting titanium alloy for KVD blades] // Aviacionnye materialy i tehnologii. 2010. №2. S. 8–14.
  16. Kablov E.N., Muboyadzhyan S.A. Ionnoe travlenie i modificirovanie poverhnosti otvetstvennyh detalej mashin v vakuumno-dugovoj plazme [Ion etching and modifying of surface of responsible details of machines in vacuum and arc plasma] // Vestnik MGTU im. N.E. Baumana. Ser.: Mashinostroenie. 2011. №SP2. S. 149–163.
  17. Ustinov A.I. Dissipativnye svojstva nanostrukturirovannyh materialov [Dissipative properties of the nanostructured materials] // Problemy prochnosti. 2008. №5. S. 96–104.