Electron Back Scatter Diffraction (EBSD) method possibilities for selective laser melted nickel superalloys structure features investigation

Raevskih A.N., Chabina E.B., Filonova E.V., Belova N.A.
Raevskih A.N., Chabina E.B., Filonova E.V., Belova N.A. Electron Back Scatter Diffraction (EBSD) method possibilities for selective laser melted nickel superalloys structure features investigation // Proceedings of VIAM. 2017. No. 12. DOI: 10.18577/2307-6046-2017-0-12-12-12. URL: https://www.viam-works.ru/en/journal/2017/12/12
Keywords
Electron Back Scatter Diffraction (EBSD), selective laser melting, nickel-base superalloy, microstructure, texture, fragments boundaries.
Abstract

By optical and scanning electron microscopy methods together with EBSD-analysis nickel-base superalloy ZhS6K-VI made by a selective laser melting sample structure was investigated. EBSD-analysis application allowed finding structure features, which do not observe during microscopic research: fragments primary orientation existence, which is inherited by melt baths; cracks development on boundaries between fragments with various crystallographic orientations.

Reference list
  1. Shvarc A., Kumar M., Adams B., Fild D. Metod difrakcii otrazhennyh elektronov v materialovedenii [Method of diffraction of the reflected electrons in materials science]. M.: Tehnosfera, 2004. 559 s.
  2. Venables J.A., Harland C.J. Electron back-scattering patterns – A new technique for obtaining crystallographic information in the scanning electron microscope // Philosophic Magazine. 1973. Vol. 2. P. 1193–1200.
  3. Vilaro T., Colinb C., Bartoutb J.D., Naz L., Sennour M. Microstructural and mechanical approaches of the selective laser melting process applied to a nickel-base superalloy // Materials Science and Engineering: A. 2012. Vol. 534. P. 446–451.
  4. Raevskih A.N., Chabina E.B., Filonova E.V., Belova N.A. Issledovanie osobennostej struktury nikelevyh zharoprochnyh splavov, poluchennyh selektivnym lazernym splavleniem, s primeneniem metoda difrakcii obratnootrazhennyh elektronov (EBSD/DOE) [Research of features of structure of the nickel hot strength alloys received by the selection laser fusing, using method of diffraction of back reflected electrons (EBSD/DOE)] // Materialy III Mezhdunar. konf. «Additivnye tehnologii: nastoyashhee i budushhee» (Moskva, 23 mar. 2017 g.). M.: VIAM, 2017. Stat'ya 3016F6F6. 1 elektron. opt. disk (CD-R).
  5. Chabina E.B., Filonova E.V., Raevskih A.N. Vliyanie tehnologicheskih parametrov processa selektivnogo lazernogo splavleniya na formirovanie struktury zharoprochnogo nikelevogo splava [Influence of technological parameters of process of the selection laser fusing on forming of structure of heat resisting nickel alloy] // Materialy II Mezhdunar. konf. «Additivnye tehnologii: nastoyashhee i budushhee» (Moskva, 16 mar. 2016 g.). M.: VIAM, 2016. Stat'ya №4. 1 elektron. opt. disk (CD-R).
  6. Lukina E.A., Bazaleeva K.O., Petrushin N.V., Cvetkova E.V. Osobennosti formirovaniya struktury zharoprochnogo nikelevogo splava ZhS6K-VI pri selektivnom lazernom splavlenii [Features of forming of structure of heat resisting ZhS6K-VI nickel alloy at the selection laser fusing] // Tsvetnye metally. 2016. №3. S. 57–63.
  7. 7 Lapteva M.A., Belova N.A., Raevskih A.N., Filonova E.V. Issledovanie zavisimosti sherohovatosti, morfologii poverhnosti i kolichestva defektov struktury ot moshhnosti lazera, skorosti skanirovaniya i tipa shtrihovki v zharoprochnom splave, sintezirovannom metodom SLS [Dependence of roughness, surface morphology structure and number of defects on the power of the laser, scanning speed and the type of hatching in the high-temperature alloys synthesized by SLS] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №9. St. 09. Available at: http://www.viam-works.ru (accessed: September 21, 2017). DOI: 10.18577/2307-6046-2016-0-9-9-9.
  8. Soula A. Grain Boundary and Intergranular deformations during High Temperature Creep of a PM Nickel-Based Superalloy // Superalloys-2008. Warrendale, PA: The Mineral, Metals and Materials Society, 2008. Р. 387–394.
  9. Muñoz-Moreno R., Divya V.D., Messé O.M.D.M. Effect of heat treatments on the microstructure and texture of cm247lc processed by selective laser melting. Minerals, Metals & Materials Society, 2016. P. 375–382.
  10. Wang Di, Yang Yongqiang, Su Xubin, Chen Yonghua. Study on energy input and its influences on single-track, multi-track, and multi-layer in SLM // The International Journal of Advanced Manufacturing Technology. 2012. Vol. 58. Issue 9. P. 1189–1199.
  11. Carter L.N., Martin C., Withers P.J., Attallah M.M. The influence of the laser scan strategy on grain structure and cracking behavior in SLM powder-bed fabricated nickel superalloy // Journal of Alloys and Compounds. 2014. Vol. 615. P. 338–347.
  12. Evgenov A.G., Rogalev A.M., Nerush S.V., Mazalov I.S. Issledovanie svojstv splava EP648, poluchennogo metodom selektivnogo lazernogo splavleniya metallicheskih poroshkov [A study of properties of EP648 alloy manufactured by the selective laser sintering of metal powders] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №2. St. 02. Available at: http://www.viam-works.ru (accessed: September 21, 2017). DOI: 10.18577/2307-6046-2015-0-2-2-2.
  13. Zemin Wang, Kai Guana, Ming Gao et al. The microstructure and mechanical properties of deposited-IN718 by selective laser melting // Journal of Alloys and Compounds. 2012. Vol. 513. P. 518–523.
  14. Amato K.N., Gaytan S.M., Murr L.E. et al. Microstructures and mechanical behavior of Inconel 718 fabricated by selective laser melting // Acta Materialia. 2012. Vol. 60. P. 2229–2239.
  15. Kablov E.N., Ospennikova O.G., Lomberg B.S., Sidorov V.V. Prioritetnye napravleniya razvitiya tehnologij proizvodstva zharoprochnyh materialov dlya aviacionnogo dvigatelestroeniya [The priority directions of development of production technologies of heat resisting materials for aviation engine building] // Problemy chernoj metallurgii i materialovedeniya. 2013. №3. S. 47–54.
  16. Kablov E.N. Razrabotki VIAM dlya gazoturbinnyh dvigatelej i ustanovok [Development of VIAM for gas turbine engines and installations] // Krylya Rodiny. 2010. №4. S. 31–33.
  17. Kablov E.N., Petrushin N.V., Svetlov I.L., Demonis I.M. Nikelevye litejnye zharoprochnye splavy novogo pokoleniya [Nickel foundry heat resisting alloys of new generation] // Aviacionnye materialy i tehnologii. 2012. №S. C. 36–52.
  18. Kablov E.N. Nastoyashhee i budushhee additivnyh tehnologij [Present and future of the additive technologies] //Metally Evrazii. 2017. №1. S. 2–6.
  19. Kablov E.N. Materialy i tehnologii VIAM dlya «Aviadvigatelya» [Materials and technologies of VIAM for «Aircraft engine»] // Permskie aviacionnye dvigateli. 2014. №31. S. 43–47.
  20. Grigorev S.N., Tarasova T.V. Vozmozhnosti tehnologii additivnogo proizvodstva dlya izgotovleniya slozhnoprofilnyh detalej i polucheniya funkcionalnyh pokrytij iz metallicheskih poroshkov [Possibilities of technology of the additive production for manufacturing of of difficult profile details and receiving functional coverings from metal powders] // Metallovedenie i termicheskaya obrabotka metallov. 2015. №10 (724). S. 5–10.
  21. Grigorev S.N. Problemy i perspektivy razvitiya otechestvennogo mashinostroitelnogo proizvodstva [Problems and perspectives of development of domestic machine-building production] // Spravochnik: inzhenernyj zhurnal s prilozheniem. 2011. №12. S. 3–7.
  22. Smurov I.Yu., Movchan I.A., Yadrojcev I.A. i dr. Additivnoe proizvodstvo s pomoshhyu lazera [The additive production by means of the laser] // Vestnik MGTU «Stankin». 2011. T. 2. №4. S. 144–146.
  23. Strano G., Hao L., Everson R.M., Evans K.E. Surface roughness analysis, modelling and prediction in selective laser melting // Journal of Materials Processing Technology. 2013. Vol. 213. No. 4. P. 589–597.
  24. Lukina E.A., Bazaleeva K.O., Petrushin N.V., Treninkov I.A., Cvetkova E.V. Vliyanie parametrov selektivnogo lazernogo plavleniya na strukturno-fazovoe sostoyanie zharoprochnogo nikelevogo splava ZhS6K-VI [Influence of parameters of the selection laser melting on structural and phase condition of heat resisting ZhS6K-VI nickel alloy] // Metally. 2017. №4. S. 63–71.
  25. Supersplavy II / pod red. Ch.T. Simsa, N.S. Stoloffa, U.K. Hagelya [Superalloys II / ed. by Ch.T. Sims, N.S. Stoloff, U.K. Hagel]. M.: Metallurgiya, 1995. Kn. 1. 384 s.
  26. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  27. Evgenov A.G., Nerush S.V., Vasilenko S.A. Poluchenie i oprobovanie melkodispersnogo metallicheskogo poroshka vysokohromistogo splava na nikelevoj osnove primenitelno k lazernoj LMD-naplavke [The obtaining and testing of the fine-dispersed metal powder of the high-chromium alloy on nickel-base for laser metal deposition] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №5. St. 04. Available at: http://www.viam-works.ru (accessed: September 21, 2017). DOI: 10.18577/2307-6046-2014-0-5-4-4.
  28. Nerush S.V., Evgenov A.G. Issledovanie melkodispersnogo metallicheskogo poroshka zharoprochnogo splava marki EP648-VI primenitelno k lazernoj LMD-naplavke, a takzhe ocenka kachestva naplavki poroshkovogo materiala na nikelevoj osnove na rabochie lopatki TVD [Research of fine-dispersed metal powder of the heat resisting alloy of the EP648-VI brand for laser metal deposition (LMD) and also the assessment quality of welding of powder material on the nickel basis on working blades THP] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №3. St. 01. Available at: http://www.viam-works.ru (accessed: September 21, 2017). DOI: 10.18577/2307-6046-2014-0-3-1-1.
  29. Chabina E.B., Alekseev A.A., Filonova E.V., Lukina E.A. Primenenie metodov analiticheskoj mikroskopii i rentgenostrukturnogo analiza dlya issledovaniya strukturno-fazovogo sostoyaniya materialov [Application of methods of analytical microscopy and X-ray-structural analysis for research of structural and phase condition of materials] // Sb. dokl. Vseros. konf. po ispytaniyam i issledovaniyam svojstv materialov «TestMat–2013». M., 2013. S. 32–37.