Nonstick coating is used for molds and cores of the CTS used in the casting magnesium alloys (review)

Trofimov N.V., Leonov A.A.
Trofimov N.V., Leonov A.A. Nonstick coating is used for molds and cores of the CTS used in the casting magnesium alloys (review) // Proceedings of VIAM. 2017. No. 12. DOI: 10.18577/2307-6046-2017-0-12-10-10. URL: https://www.viam-works.ru/en/journal/2017/12/10
Keywords
magnesium alloys, non-stick coatings, aqueous coatings, self-drying coatings, fillers, binding components.
Abstract

We consider non-stick protective coatings that prevent the mold material from adhering to the metal surface of the casting, which ensures its easy extraction. The main task of the non-stick coating is to reduce the mold or rod to mold castings. For this use materials on water or alcohol basis. Paints for molds and rods from cold-hardening mixtures contain gluing additives and refractory components, which makes it possible to increase the strength of the working surface and reduce the scattering of shapes and rods. Coatings are applied with a brush or an atomizer, the rods are painted in one layer, and the molds, depending on the mass of the casting, are in several layers.

Reference list
  1. Kablov E.N. Aviacionnoe materialovedenie: itogi i perspektivy [Aviation materials science: results and perspectives] // Vestnik Rossijskoj akademii nauk. 2002. T. 72. №1. S. 3–12.
  2. Kablov E.N. VIAM: prodolzhenie puti [VIAM: way continuation] // Nauka v Rossii. 2012. №3. S. 36–44.
  3. Kablov E.N. Sovremennye materialy – osnova innovacionnoj modernizacii Rossii [Modern materials are the base of innovative modernization of Russia] // Metally Evrazii. 2012. №3. S. 10–15.
  4. Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace materials science] // Vse materialy. Enciklopedicheskij spravochnik. 2008. №3. S. 2–14.
  5. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  6. Kablov E.N., Ospennikova O.G., Vershkov A.V. Redkie metally i redkozemelnye elementy – materialy sovremennyh i budushhih vysokih tehnologij [Rare metals and rare earth elements – materials of modern and future high technologies] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №2. St. 01. Available at: http://www.viam-works.ru (accessed: October 16, 2017).
  7. Duyunova V.A., Goncharenko N.S., Muhina I.Yu., Uridiya Z.P., Volkova E.F. Nauchnoe nasledie akademika I.N. Fridlyandera. Sovremennye issledovaniya magnievyh i litejnyh alyuminievyh splavov v VIAM [Scientific heritage of academician I.N.Fridlyander. Modern researches of magnesium and cast aluminum alloys in VIAM] // Tsvetnye metally. 2013. №9. S. 71–78.
  8. Duyunova V.A. Metody zashhity magnievyh splavov v otechestvennom litejnom proizvodstve s 1930-h gg. do nastoyashhego vremeni [Methods of protection of magnesium alloys in domestic foundry production since the 1930th till nowadays] // Litejshhik Rossii. 2010. №10. S. 35–37.
  9. Duyunova V.A., Uridiya Z.P. Issledovanie vosplamenyaemosti litejnyh magnievyh splavov sistemy Mg–Zn–Zr [Research of inflammability of cast magnesium alloys of Mg–Zn–Zr system] // Litejshhik Rossii. 2012. №11. S. 21–23.
  10. Kablov E.N., Muhina I.Yu., Korchagina V.A. Prisadochnye materialy dlya formovochnyh smesej pri lite magnievyh splavov [Additive materials for forming mixes when molding magnesium alloys] // Litejnoe proizvodstvo. 2007. №5. S. 15–18.
  11. Duyunova V.A., Muhina I.Yu., Uridiya Z.P. Novye protivoprigarnye prisadochnye materialy dlya litejnyh form magnievyh otlivok [New antiburn additive materials for molding molds of magnesian cast] // Litejnoe proizvodstvo. 2009. №9. S. 18–21.
  12. Duyunova V.A., Kozlov I.A. Holodnotverdeyushhie formovochnye smesi: perspektivy ispolzovaniya pri lite magnievyh splavov [Cold hardening forming mixes: use perspectives when molding magnesium alloys] // Vse materialy. Enciklopedicheskij spravochnik. 2011. №1. S. 41–43.
  13. Muhina I.Yu., Duyunova V.A., Uridiya Z.P. Perspektivnye litejnye magnievye splavy [Perspective cast magnesium alloys] // Litejnoe proizvodstvo. 2013. №5. S. 2–5.
  14. Leonov A.A., Duyunova V.A., Stupak E.V., Trofimov N.V. Lite magnievyh splavov v razovye formy, poluchennye novymi metodami [Casting of magnesium alloys in disposable moulds produced by new methods] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №12. St. 01. Available at: http://www.viam-works.ru (accessed: October 20, 2017). DOI: 10.18577/2307-6046-2014-0-12-1-1.
  15. Trofimov N.V., Leonov A.A., Duyunova V.A., Uridiya Z.P. Litejnye magnievye splavy (obzor) [Cast magnesium alloys (review)] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №12. St. 01. Available at: http://www.viam-works.ru (accessed: October 20, 2017). DOI: 10.18577/2307-6046-2016-0-12-1-1.
  16. Muhina I.Yu., Uridiya Z.P. Magnij – osnova sverhlegkih materialov [Magnesium is the base of extralight materials] // Metallurgiya mashinostroeniya. 2005. №6. S. 29–31.
  17. Muhina I.Yu. Bobryshev B.L., Antipov V.V., Koshelev A.O., Bobryshev D.B. Struktura i svojstva splavov sistemy Mg–Al–Zr pri lite v kokil i formy iz HTS [Structure and properties of alloys of Mg–Al–Zr system at chill casting and forms from HTS] // Litejnoe proizvodstvo. 2014. №8. S. 6–10.
  18. Volkova E.F., Muhina I.Yu. Novye materialy na magnievoj osnove i vysokoresursnye tehnologii ih proizvodstva [New materials on magnesian basis and high-resource technologies of their production] // Tehnologiya legkih splavov. 2007. №2. S. 28–34.