Natural tests of metal materials in sea water: key approaches to estimation of resistance to corrosion and biodeterioration

Varchenko E.A., Kurs M.G.
Varchenko E.A., Kurs M.G. Natural tests of metal materials in sea water: key approaches to estimation of resistance to corrosion and biodeterioration // Proceedings of VIAM. 2017. No. 11. DOI: 10.18577/2307-6046-2017-0-11-12-12. URL: https://www.viam-works.ru/en/journal/2017/11/12
Keywords
corrosion, biological stability of materials, fouling, marine tests.
Abstract

The paper covers the problems of methodological support in the part of assessing the resistance to corrosion and biofouling of metallic materials during full-scale marine tests, as well as a review of the research work of the GCTC VIAM, aimed at developing, improving, clarifying and supplementing the methods of marine testing. Attention is focused on the impact of ecological and biological aspects on complex technical systems and the need for testing materials for biological resistance as an integral part of climate testing.

Reference list
  1. Kablov E.N., Shchetanov B.V., Grashhenkov D.V., Shavnev A.A., Nyafkin A.N. Metallomatrichnye kompozicionnye materialy na osnove Al–SiC [Metalmatrix composite materials on the basis of Al–SiC] // Aviacionnye materialy i tehnologii. 2012. №S. S. 373–380.
  2. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  3. Kablov E.N., Startsev O.V., Medvedev I.M. Obzor zarubezhnogo opyta issledovanij korrozii i sredstv zashhity ot korrozii [Review of international experience on corrosion and corrosion protection] // Aviacionnye materialy i tehnologii. 2015. №2 (35). S. 76–87. DOI: 10.18577/2071-9140-2015-0-2-76-87.
  4. Kurs M.G., Karimova S.A. Naturno-uskorennye ispytaniya: osobennosti metodiki i sposoby ocenki korrozionnyh harakteristik alyuminievyh splavov [Salt-accelerated outdoor corrosion testing: methodology and evaluation of corrosion susceptibility of aluminum alloy] // Aviacionnye materialy i tehnologii. 2014. №1. S. 51–57. DOI: 10.18577/2071-9140-2014-0-1-51-57.
  5. Laptev A.B. S uchetom posledstvij izmenenij klimata [Taking into account consequences of climate changes] // Industriya. Inzhenernaya gazeta. 2017. №5. S. 5.
  6. Karpov V.A. Biokorroziya v morskoj srede i osnovy primeneniya zashhitnyh pokrytij: avtoref. dis. … d-r tehn. nauk [Biocorrosion in the marine environment and bases of application of protecting covers: thesis, Dr. Sc. (Tech.)]. M., 2012. 48 s.
  7. Lebedev E.M., Permitin Yu.E., Karaeva N.I. K voprosu ob obrastanii plastin na Chernom more [To question of overgrowing of plates on Black Sea] // Trudy IOAN. 1963. T. 10. S. 82–93.
  8. Lebedev E.M. Nekotorye aktualnye voprosy izucheniya obrastaniya i zashhity ot nego [Some topical issues of studying of overgrowing and protection against it] // Izuchenie processov morskogo bioobrastaniya i razrabotka metodov borby s nim. L.: ZIN, 1987. S. 62–64.
  9. Miheev A.I. Vliyanie obrastaniya i nizkih temperatur na bezopasnuyu ekspluataciyu sudov [Influence of overgrowing and low temperatures on safe operation of vessels] // Vodnyj transport. 2013. Vyp. 3. S. 56–61.
  10. Shkabara N.A. Ekologo-tehnologicheskoe izuchenie pokrytiya bar'ernogo tipa dlya zashhity ot korrozii i morskogo obrastaniya neftegazoprovodov, plavuchih sredstv i portovyh sooruzhenij (na primere Gelendzhikskoj buhty): avtoref. dis. … kand. tehn. nauk [The ecologist technological studying of covering of barrier type for corrosion protection and sea overgrowing of oil and gas pipelines, watercrafts and port installations (on example of the Gelendzhiksky bay): thesis, PhD (Tech.)]. Krasnodar, 2015. 113 s.
  11. Panchenko Yu.M., Strekalov P.V., Nikulina T.V. Vliyanie uderzhannyh produktov korrozii na tormozhenie korrozionnogo processa. Ch. I. Pervye dva goda [Influence of the withheld products of corrosion on braking of corrosion process. H. I. First two years] // Korroziya: materialy, zashhita. 2013. №2. S. 9–18.
  12. Borodavkin P.P. Morskie neftegazovye sooruzheniya: uchebnik dlya vuzov [Sea oil and gas constructions: the textbook for higher education institutions]. M.: Nedra-Biznescentr, 2006. Ch. 1: Konstruirovanie. 555 s.
  13. Starokon I.V. O vliyanii korrozionnogo vozdejstviya na razvitie ustalostnyh treshhin na morskih neftegazovyh sooruzheniyah (MNGS) [About influence of corrosive attack on development of fatigue cracks on sea oil and gas constructions (SOGC)] // Fundamentalnye issledovaniya. 2012. №11. Ch. 5. S. 1214–1219.
  14. Pravila klassifikacii, postrojki i oborudovaniya plavuchih burovyh ustanovok i morskih stacionarnyh platform [Ruled classifications, construction and the equipment of floating drilling rigs and offshore fixed platforms]. SPb.: Morskoj registr sudohodstva, 2008. 483 s.
  15. Markovich R.A., Kan M.K., Mihajlov S.V. Korroziya i metody zashhity zony peremennogo smachivaniya metallokonstrukcij gidrotehnicheskih sooruzhenij estakadnogo tipa [Corrosion and methods of protection of zone of variable wetting of metalwork of hydraulic engineering constructions of platform type ] // Gidrotehnika. 2014. №4. S. 71.
  16. Microbially Influenced Corrosion of Materials: Scientific and Engineering Aspects / eds. E. Heitz, H.-C. Flemming, W. Sand. Springer-Verlag, Berlin, Heidelberg, 1996. 475 p.
  17. Dazhang Yang, Jianhua Liu, Xiaoxue E, Linlin Jiang. Experimental study of composition and influence factors on fouling of stainless steel and copper in seawater // Annals of Nuclear Energy. 2016. Vol. 94. P. 767–772.
  18. Al-Muhanna K., Habib K. Marine bio-fouling of different alloys exposed to continuous flowing fresh seawater by electrochemical impedance spectroscopy // Journal of Saudi Chemical Society. 2016. Vol. 20. Issue 4. P. 391–396.
  19. Mansfeld F., Little B. Microbiologically influenced corrosion of copper-based materials exposed to natural seawater // Electrochimica Acta. 1992. Vol. 37. Issue 12. P. 2291–2297.
  20. Koryakova M.D., Filonenko N.Yu., Kaplin Yu.M. Issledovanie korrozii vysokolegirovannyh stalej v morskoj vode pod balyanusami [Research of corrosion high-alloy steel in sea water under barnacles] // Zashhita metallov. 1995. T. 31. №2. S. 219–221.
  21. Kaplin Yu.M., Koryakova M.D., Nikitin V.M., Suponina A.P. Mehanizm korrozii stali pod osnovaniem balyanusa [The mechanism of corrosion of steel under the basis barnacles] // Zashhita metallov. 1998. T. 34. №1. S. 89–93.
  22. Koryakova M.D., Nikitin V.M., Speshneva N.V. Rol bakterialnoj plenki pod balyanusami v korrozii vysokolegirovannoj stali v morskoj vode [Role of bacteriemic film under barnacles in corrosion of high-alloy steel in sea water // Zashhita metallov. 1998. T. 34. №2. S. 208–211.
  23. Karpov V.A., Kovalchuk Yu.L., Beleneva I.A., Petrosyan V.G. Issledovanie korrozii metallov v tropicheskih morskih vodah [The study of the corrosion of metals in tropical marine waters] // Novosti materialovedeniya. Nauka i tehnika: elektron. nauch.-tehnich. zhurn. 2016. №6 (24). St. 03. Available at: http://www.materialsnews.ru (accessed: November 08, 2017).
  24. Lebedev E.M., Ilin I.H. Metody issledovanij morskogo i okeanicheskogo obrastaniya [Methods of researches of sea and oceanic overgrowing] // Obrastanie i biopovrezhdeniya. Ekologicheskie problemy. M.: Nauka, 1992. S. 65–76.
  25. Zinova A.D. Opredelitel zelenyh, buryh i krasnyh vodoroslej yuzhnyh morej SSSR [Determinant of green, brown and red algas of the southern seas of the USSR]. M.–L., 1967. 397 s.
  26. Gluhenkij I.Yu., Lavrentev A.V., Popova G.G. Modelirovanie avarijnyh razlivov nefti v Kerchenskom prolive [Modeling of emergency oil spillages in the Strait of Kerch] // Bezopasnost v tehnosfere. 2014. №6. S. 3–6.
  27. Cvetkov V.Ya. Geoinformacionnye sistemy i tehnologii [Geoinformation systems and technologies]. M.: Finansy i statistika, 1998. 230 s.
  28. Morskaya korroziya [Sea corrosion]. M.: Metallurgiya, 1983. 512 s.
  29. Protasov V.N. Teoriya i praktika primeneniya polimernyh pokrytij v oborudovanii i sooruzheniyah neftegazovoj otrasli [The theory and practice of application of polymer coatings in the equipment and constructions of the oil and gas industry]. M.: Nedra-Biznescentr, 2007. 374 s.
  30. Dolgopolskaya M.A. Eksperimentalnoe izuchenie processa obrastaniya v more [Experimental studying of process of overgrowing in the sea] // Trudy Sevastopolskoj biologicheskoj stancii. 1954. T. 8. S. 157–173.
  31. Dolgopolskaya M.A., Degtyarev P.F. Biologicheskoe obosnovanie dlya stendovyh ispytanij sredstv zashhity ot obrastaniya [Biological justification for stand tests of security features from overgrowing] // Biologicheskie issledovaniya Chernogo morya i ego promyslovyh resursov. M.: Nauka, 1968. S. 132–136.
  32. Izuchenie processov morskogo bioobrastaniya i razrabotka metodov borby s nim [Studying of processes of sea biofouling and development of methods of fight against it]. L.: Zoologicheskij institut AN SSSR, 1987. 132 s.
  33. Ilin I.N. Metody izucheniya obrastaniya v okeane [Methods of studying of overgrowing at the ocean] // Ekologicheskie aspekty zashhity tehniki i materialov. Teoriya i praktika naturnyh ispytanij. M.: IPEE RAN, 2000. Ch. 2. S. 32–36.