Abstract
Studied the protective properties of polysulfide sealants UT-32NT and VITEF-1NT on the samples of magnesian alloy MA8 after exposure to the tropical chamber during for 7 months, salt spray chamber during for 2 months, andML5 after fuel TS-1. It was found that, when working in an environment of air and tropical climate sealants VITEF-1NT or UT-32NT (film thickness of 1,5–2 mm) are suitable for protecting alloy MA8 oxidized as a sheet and in contact with the rivets on KFО-30 ground or sealant. Sealants VITEF-1NT or UT-32NT after exposure in the fuel TS-1, containing water in the form of a separate phase, have weak adhesion to a magnesian alloy of ML5 oxidized and do not protect it from corrosion.
Reference list
- Kablov E.N. Himiya v aviacionnom materialovedenii [Chemistry in aviation materials science] // Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 3–4.
- Kablov E.N. Shestoj tehnologicheskij uklad [Sixth technological way] // Nauka i zhizn. 2010. №4. S. 2–7.
- Istoriya aviacionnogo materialovedeniya. VIAM – 80 let: gody i lyudi / pod obshh. red. E.N. Kablova [History of aviation materials science. VIAM – 80 years: years and people / gen. ed. by E.N. Kablov]. M.: VIAM, 2012. S. 346–348.
- Grashhenkov D.V., Chursova L.V. Strategiya razvitiya kompozicionnyh i funkcionalnyh materialov [Strategy of development of composite and functional materials] // Aviacionnye materialy i tehnologii. 2012. №S. S. 231–242.
- Savenkova A.V., Chursova L.V., Eliseev O.A., Glazov P.A. Germetiki aviacionnogo naznacheniya [Hermetics of aviation assignment] // Aviacionnye materialy i tehnologii. 2012. №3. S. 40–43.
- Minkin V.S., Hakimullin Yu.N., Deberdeev T.R., Berlin Al.Al. Vliyanie ionov Fe (III) v sostave MnO2 na kinetiku vulkanizacii zhidkih tiokolov [Influence of ions of Fe (III) as a part of MnO2 on kinetics of curing of the liquid it is thiokol] // Klei. Germetiki. Tehnologii. 2009. №4. S. 28–30.
- Zajceva E.I., Chursova L.V. Issledovanie mikrobiologicheskoj stojkosti polisul'fidnogo germetika s novymi antisepticheskimi dobavkami [Research of microbiological firmness of polysulphide hermetic with new antiseptic additives] // Klei. Germetiki. Tehnologii. 2012. №1. S. 16–20.
- Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Zaicheva Е.I., Donskoi А.А. Sealants Based on Polysulfide Elastomers // Polymer Science. Ser. С. 2008. Vol. 1. P. 15–25.
- Zajceva E.I., Donskoj A.A. Germetiki na osnove polisulfidnyh elastomerov [Hermetics on the basis of polysulphide elastomer] // Klei. Germetiki. Tehnologii. 2008. №6–7. S. 15–25.
- Zajceva E.I., Donskoj A.A. Novye polisulfidnye germetiki dlya aviacionnoj promyshlennosti [New polysulphide hermetics for the aviation industry] // Klei. Germetiki. Tehnologii. 2009. №3. S. 18–23.
- Petrova A.P., Donskoj A.A. Kleyashhie materialy, germetiki: spravochnik [Gluing materials, hermetics: directory]. SPb.: Professional, 2008. S. 503–567.
- Zajceva E.I., Chursova L.V., Smirnov D.N. Perspektivy snizheniya plotnosti polisul'fidnyh germetikov [Perspectives of decrease in density of polysulphide hermetics] // Klei. Germetiki. Tehnologii. 2012. №5. S. 10–14.
- Eliseev O.A., Krasnov L.L., Zajceva E.I., Savenkova A.V. Razrabotka i modificirovanie elastomernyh materialov dlya primeneniya vo vseklimaticheskih usloviyah [Development and modifying of elastomeric materials for application in all weather conditions] // Aviacionnye materialy i tehnologii. 2012. №S. S. 309–314
- Karimova S.A., Pavlovskaya T.G. Razrabotka sposobov zashhity ot korrozii konstrukcij, rabotajushhih v usloviyah kosmosa [Development of ways of corrosion protection of the designs working in the conditions of space] // Trudy VIAM: electron. nauch.-tehnich. zhurn. 2013. №4. St. 02. Available at: http://www.viam-works.ru (accessed: August, 01 2017).
- Eliseev O.A., Bryk Ya.A., Smirnov D.N. Modifikaciya polisulfidnyh germetikov ingibitorami korrozii [Polysulfide sealants modification by corrosion inhibitors] // Aviacionnye materialy i tehnologii. 2016. №S2 (44). S. 15–21. DOI: 10.18577/2071-9140-2016-0-S2-15-21.