Theoretical calculation and experimental determination of modulus of elasticity and strength of GRP VPS-53/120

Melnikov D.A., Gromova A.A., Raskutin A.E., Kurnosov A.O.
Melnikov D.A., Gromova A.A., Raskutin A.E., Kurnosov A.O. Theoretical calculation and experimental determination of modulus of elasticity and strength of GRP VPS-53/120 // Proceedings of VIAM. 2017. No. 1. DOI: 10.18577/2307-6046-2017-0-1-8-8. URL: https://www.viam-works.ru/en/journal/2017/1/8
Keywords
polymer composite materials, GRP, matrix, elastic-mechanical properties, fiber glass fabric, VPS-53/120, tension.
Abstract

In the article theoretical approaches to calculation of elastic – strength characteristics at tension of composite materials on the basis of woven fillers are given. Manufacturing methods of samples of curing binders for tension tests are described. The influence of manufacturing method of samples on defined elastic and strength characteristics of epoxy resin VSE-34 is investigated. Theoretical calculations are carried out and experimental data of strength and elastic modulus are obtained for VPS-53/120 fiberglass at tension. Comparison of theoretically calculated values with experimental ones is given.

The work is performed within the implementation of the complex scientific direction 13.2. «Constructional PСM» («The strategic directions of development of materials and technologies of their processing for the period till 2030»)

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N., Sivakov D.V., Gulyaev I.N., Sorokin K.V., Fedotov M.Yu., Goncharov V.A. Metody issledovaniya konstrukcionnyh kompozicionnyh materialov s integrirovannoj elektromehanicheskoj sistemoj [Methods of research of constructional composite materials with the integrated electromechanical system] // Aviacionnye materialy i tehnologii. 2010. №4. S. 17–20.
  3. Kablov E.N., Startsev O.V. Fundamentalnye i prikladnye issledovaniya korrozii i stareniya materialov v klimaticheskih usloviyah (obzor) [The basic and applied research in the field of corrosion and ageing of materials in natural environments (review)] // Aviacionnye materialy i tehnologii. 2015. №4 (37). S. 38–52. DOI: 10.18577/2071-9140-2015-0-4-38-52.
  4. Kablov E.N., Kirillov V.N., Zhirnov A.D., Startsev O.V., Vapirov Yu.M. Centry dlya klimaticheskih ispytanij aviacionnyh PKM [The centers for climatic tests of aviation PKM] // Aviacionnaya promyshlennost. 2009. №4. S. 36–46.
  5. Kablov E.N. Konstrukcionnye i funkcionalnye materialy – osnova ekonomicheskogo i nauchno-tehnicheskogo razvitiya Rossii [Constructional and functional materials – basis of economic and scientific and technical development of Russia] // Voprosy materialovedeniya. 2006. №1. S. 64–67.
  6. Vavilova M.I., Kavun N.S. Stekloplastiki na osnove cianefirnyh svyazuyushhih [Glassfibers on the base of cyan-ester resins] // Aviacionnye materialy i tehnologii. 2014. №S2. S. 19–23. DOI: 10.18577/2071-9140-2014-0-s2-19-23.
  7. Kurnosov A.O., Melnikov D.A. Harakteristiki stekloplastikov na osnove vysokodeformativnyh rasplavnyh svyazuyushhih v usloviyah vozdejstviya ekspluatacionnyh faktorov [Characteristics of fibreglasses on the basis of highly deformation molten operational factors binding in the conditions of influence] // Vse materialy. Enciklopedicheskij spravochnik. 2015. №11. S. 14–18.
  8. Ilichev A.V., Raskutin A.E. Issledovanie vliyaniya koncentratora napryazhenij na napryazhenno-deformacionnoe sostoyanie ugleplastika metodom korrelyacii cifrovyh izobrazhenij [Research of stress concentrator influence on stress-strain state of carbon by digital images correlation method] // Aviacionnye materialy i tehnologii. 2014. №3. S. 62–66. DOI: 10.18577/2071-9140-2014-0-3-26-30.
  9. Kargin V.A., Slonimskij G.L. Kratkie ocherki o fiziko-himii polimerov [Short sketches about physical-chemistry of polymers]. M.: Himiya, 1967. 232 s.
  10. Rabinovich A.L. Vvedenie v mehaniku armirovannyh polimerov [Introduction in mechanics of the reinforced polymers]. M.: Himiya, 1970. 482 s.
  11. Roginskij S.L., Kanovich M.Z., Koltunov M.A. Vysokoprochnye stekloplastiki [High-strength fibreglasses]. M.: Himiya, 1979. 144 s.
  12. Kiselev B.A. Stekloplastiki [Fibreglasses]. M.: Gos. nauch.-tehnich. izd-vo him. lit-ry. 1961, 240 s.
  13. Gunyaev G.M. Struktura i svojstva polimernyh voloknistyh kompozitov [Structure and properties of polymeric fibrous composites]. M.: Himiya, 1981. 232 s.
  14. Skudra A.M., Bulave F.Ya. Prochnost' armirovannyh plastikov [Durability of the reinforced plastics]. M.: Himiya, 1982. 216 s.
  15. Voloskov G.A., Morozov V.N. K voprosu ocenki mehanicheskih svojstv materialov na osnove otverzhdayushhihsya sinteticheskih smol [To question of assessment of mechanical properties of materials on basis setting synthetic pitches] // Sintez i issledovanie epoksidnyh oligomerov i polimerov: sb. nauch. tr. Cherkassy: Izd.-poligraf. otdel otdeleniya NIITEHIMa, 1979. S. 85–91.
  16. Gunyaev G.M. Konstruirovanie vysokomodulnyh polimernyh kompozitov [Designing of high-modular polymeric composites]. M.: Mashinostroenie, 1977. 160 s.
  17. Tarnopolskij Yu.M., Zhigun I.G., Polyakov V.A. Prostranstvenno-armirovannye kompozitnye materialy: spravochnik [The space reinforced composite materials: directory]. M.: Mashinostroenie, 1987. 224 s.
  18. Kucher N.K., Dvejrin A.Z., Zemcov M.P., Ankyanec O.K. Harakteristiki uprugosti sloistyh tkanyh stekloplastikov [Characteristics of elasticity of layered woven fibreglasses] // Problemy prochnosti. 2004. №6. S. 26–32.
  19. Kucher N.K., Dvejrin A.Z., Zarazovskij M.N., Zemcov M.P. Deformirovanie sloistyh stekloplastikov, armirovannyh tkanyu satinovoj struktury pri komnatnoj i nizkih temperaturah [Deformation of the layered fibreglasses reinforced by fabric of sateen structure at room and low temperatures] // Mehanika kompozitnyh materialov. 2004. №3. S. 341–354.