VIAM experience in development and research of new generation low-cost titanium alloys

Nochovnaya N.A., Panin P.V., Kochetkov A.S., Bokov K.A.
Nochovnaya N.A., Panin P.V., Kochetkov A.S., Bokov K.A. VIAM experience in development and research of new generation low-cost titanium alloys // Proceedings of VIAM. 2016. No. 9. DOI: 10.18577/2307-6046-2016-0-9-5-5. URL: https://www.viam-works.ru/en/journal/2016/9/5
Keywords
low-cost titanium alloys, ingot, casting, combined thermo mechanical treatment, phase combination, structure, mechanical properties.
Abstract

The issues of development and research of prospective titanium alloys are in focus from the point of view of «economical» alloyage approach. The properties of low-cost titanium alloys developed in FSUE «VIAM» are shown in comparison with foreign analogues. The features of cast alloy VT40L (Ti–Al–V–Mo–Fe–Si) and new structural alloys VT44 (Ti–Al–REE) and VT45 (Ti–Al–V–Fe–REE) are considered, the two latter alloys are designed both for independent use in low- and medium-strained constructions and for titanium-polymer laminates which give opportunity to provide with 20 percent weight reduction comparing to that of bulk-metal constructions with the same load bearing capacity. It is shown that the new near-α and (α+β) REE-containing alloys have improved mechanical and service properties.

Reference list
  1. Kablov E.N. Strategicheskie napravleniya razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda [The strategic directions of development of materials and technologies of their processing for the period to 2030] // Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  2. Kablov E.N. Rossii nuzhny materialy novogo pokoleniya [Materials of new generation are necessary to Russia] // Redkie zemli. 2014. №3. S. 8–13.
  3. Antipov V.V., Senatorova O.G., Lukina N.F. i dr. Sloistye metallopolimernye kompozicionnye materialy [Layered metalpolymeric composite materials] // Aviacionnye materialy i tehnologii. 2012. №S. S. 226–230.
  4. Sokolov I.I., Raskutin A.E. Ugleplastiki i stekloplastiki novogo pokoleniya [Coalplastics and fibreglasses of new generation] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №4. St. 09. Available at: http://www.viam-works.ru (accessed: July 14, 2016).
  5. Nochovnaya N.A., Panin P.V., Alekseev E.B., Bokov K.A. Sovremennye ekonomnolegirovannye titanovye splavy: primenenie i perspektivy razvitiya [The modern economically alloyed titanium alloys: application and development perspectives] // MiTOM. 2016. №9 (735). S. 8–15.
  6. Nochovnaya N.A., Panin P.V., Alekseev E.B., Bokov K.A. Ekonomnolegirovannye titanovye splavy dlya sloistyh metallopolimernyh kompozicionnyh materialov [Low-cost alloyed titanium alloys for metal-polymer laminates] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №11. St. 02. Available at: http://www.viam-works.ru (accessed: July 14, 2016). DOI: 10.18577/2307-6046-2014-0-11-2-2.
  7. Panin P., Nochovnaya N., Kablov D., Alexeev E. Low-cost titanium alloys for titanium-polymer layered composites // Proc. of 29th Congress of the International Council of the Aeronautical Sciences (ICAS 2014). St.-Petersburg. September 7–12, 2014 (CD).
  8. Ilin A.A., Kolachev B.A., Polkin I.S. Titanovye splavy. Sostav, struktura, svojstva: spravochnik [Titanium alloys. Structure, structure, properties: directory]. M.: VILS–MATI, 2009. 520 s.
  9. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  10. Kablov D.E., Panin P.V., Shiryaev A.A., Nochovnaya N.A. Opyt ispolzovaniya vakuumno-dugovoj pechi ALD VAR L200 dlya vyplavki slitkov zharoprochnyh splavov na osnove aljuminidov titana [The use of ADL VAR L200 vacuum-arc furnace for ingots fabrication of high-temperature titanium aluminides base alloys] // Aviacionnye materialy i tehnologii. 2014. №2. S. 27–33. DOI: 10.18577/2071-9140-2014-0-2-27-33.
  11. Kablov E.N., Ospennikova O.G., Vershkov A.V. Redkie metally i redkozemelnye elementy – materialy sovremennyh i budushhih vysokih tehnologij [Rare metals and rare earth elements – materials of modern and future high technologies] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №2. St. 01. Available at: http://www.viam-works.ru (accessed: July 14, 2016).
  12. Splav na osnove titana i izdelie, vypolnennoe iz nego: pat. 2222627 Ros. Federaciya [Titanium-based alloy and the product which has been executed of it: pat. 2222627 Rus. Federation]; opubl. 27.01.04.
  13. Skvorcova S.V., Filatov A.A., Dzunovich D.A., Panin P.V. Vliyanie soderzhaniya alyuminiya na deformiruemost titanovyh splavov pri normalnoj temperature [Influence of the content of aluminum on deformability of titanium alloys at normal temperature] // Tehnologiya legkih splavov. 2008. №3. S. 40–45.
  14. Titanium-aluminum-vanadium alloys and products made therefrom: pat. 5980655 US; publ. 09.11.99 (Y. Kosaka; Titanium Metals Corp.).
  15. High strength Ti alloy and its production method: pat. JP 2004010963; publ. 15.02.2004 (A. Suzuki, T. Noda).
  16. Kosaka Y. et al. Recent development of titanium and its alloys in automotive and motorcycle applications // Proc. of 11th World Conf. on Titanium. 2007. Vol. II. P. 1383–1386.
  17. Alpha plus beta type titanium alloy: appl. US 2009/0169416; publ. 02.07.09 (Morris Manning Martin LLP).
  18. Titanium alloy part and method of manufacturing same: pat. 2508643 EP; publ. 10.10.12 (K. Takahashi et al.; Nippon Steel Corp.).
  19. Ilin A.A., Skvorcova S.V., Dzunovich D.A., Panin P.V., Shalin A.V. Vliyanie parametrov termicheskoj i termomehanicheskoj obrabotki na teksturoobrazovanie v listovyh polufabrikatah iz titanovyh splavov [Influence of parameters of thermal and thermomechanical processing on structure produced in sheet semi-finished products from titanium alloys] // Tehnologiya mashinostroeniya. 2012. №8. S. 8–12.