Processing reinforcing filler from PCM for recycling purposes

Doriomedov M.S., Petrov A.V., Daskovskiy M.I., Skripachyov S.Yu.
Doriomedov M.S., Petrov A.V., Daskovskiy M.I., Skripachyov S.Yu. Processing reinforcing filler from PCM for recycling purposes // Proceedings of VIAM. 2016. No. 8. DOI: 10.18577/2307-6046-2016-0-8-12-12. URL: https://www.viam-works.ru/en/journal/2016/8/12
Keywords
polymer composite material, recycling, secondary use, fiber reinforced plastic.
Abstract

The analysis of various tissues of fibrous fillers to create polymer composite materials (PCM) is performed, their structure and possible technology of their destruction with the aim of further processing of the fibers is considered. It is suggested to process recycled fiber from PCM into nonwoven materials as the most convenient and universal direction for further processing. The technology of producing nonwoven fabrics of carbon fibers and their application are considered. The work was executed within implementation of the complex scientific direction 13.1. «Binding for polymer and composite materials of constructional and special purpose» («The strategic directions of development of materials and technologies of their processing for the period till 2030») [1].

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  2. Petrov A.V., Doriomedov M.S., Skripachev S.Yu. Tehnologii utilizacii polimernyh kompozicionnyh materialov (obzor) [Recycling technologies of polymer composite materials (review)] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №8. St. 09. Available at: http://viam-works.ru (accessed: February 01, 2016). DOI: 10.18577/2307-6046-2015-0-8-9-9.
  3. Available at: http://www.cordis.europa.eu/project/rcn/90590_en.html (accessed: February 10, 2016).
  4. Daskovskij M.I., Doriomedov M.S., Skripachev S.Yu. Sistematizaciya bazisnyh faktorov, prepyatstvuyushhih vnedreniyu polimernyh kompozicionnyh materialov v Rossii (obzor) [Underlying factors preventing the introduction of polymer composite materials in Russia (review)] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №5 St. 06. Available at: http://www.viam-works.ru (accessed: May 24, 2016). DOI: 10.18577/2307-6046-2016-0-5-6-6.
  5. Doriomedov M.S., Daskovskij M.I., Skripachev S.Yu., Shein E.A. Polimernye kompozicionnye materialy v zheleznodorozhnom transporte Rossii [Polymeric composite materials in railway transport of Russia] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №7. St. 12. Available at: http://www.viam-works.ru (accessed: July 25, 2016). DOI: 10.18577/2307-6046-2016-0-7-12-12.
  6. Petrov A.V., Doriomedov M.S., Skripachev S.Yu. Zarubezhnyj opyt razvitiya proizvodstva izdelij s ispolzovaniem vtorichno pererabotannyh polimernyh kompozicionnyh materialov (obzor) [Foreign experience of manufacturing products using recycled polymer composites (review)] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №12. St. 12. Available at: http://www.viam-works.ru (accessed: February 01, 2016). DOI: 10.18577/2307-6046-2015-0-12-12-12.
  7. Kiryuhin S.M., Shustov Yu.S. Tekstilnoe materialovedenie [Textile materials science]. M.: KolosS, 2011. 360 s.
  8. Bershev E.N., Smirnov G.P., Zametta B.V., Nazarov Yu.P., Korneev V.N. Netkanye tekstilnye polotna: spravochnoe posobie [Nonwoven textile cloths: handbook]. M.: Legprombytizdat, 1987. 400 s.
  9. Gorchakova V.M., Sergeenkov A.P., Voloshhik T.E. Oborudovanie dlya proizvodstva netkanyh materialov [The equipment for production of nonwoven materials]. M.: MGTU im. A.N. Kosygina, 2006. Ch. 2. 776 s.
  10. Available at: http://www.cfk-recycling.com (accessed: February 10, 2016).
  11. Kablov E.N. Kompozity: segodnya i zavtra [Composites: today and tomorrow] // Metally Evrazii. 2015. №1. S. 36–39.
  12. Kablov E.N. Sovremennye materialy – osnova innovacionnoj modernizacii Rossii [Modern materials – basis of innovative modernization of Russia] // Metally Evrazii. 2012. №3. S. 10–15.
  13. Kablov E.N. Aviacionnoe materialovedenie: itogi i perspektivy [Aviation materials science: results and perspectives] // Vestnik Rossijskoj akademii nauk. 2002. T. 72. №1. S. 3–12.
  14. Kablov E.N. Materialy – osnova lyubogo dela [Materials – basis of any business] // Delovaya slava Rossii. 2013. №2 (40). S. 4–9.
  15. Kablov E.N. Innovacionnoe razvitie – vazhnejshij prioritet gosudarstva [Innovative development – the most important priority of the state] // Metally Evrazii. 2010. №2. S. 6–11.