Research of corrosion damage of wrought aluminium alloys at laboratory and full-scale tests

Kurs M.G., Kutyrev A.E., Fomina M.A.
Kurs M.G., Kutyrev A.E., Fomina M.A. Research of corrosion damage of wrought aluminium alloys at laboratory and full-scale tests // Proceedings of VIAM. 2016. No. 8. DOI: 10.18577/2307-6046-2016-0-8-10-10. URL: https://www.viam-works.ru/en/journal/2016/8/10
Keywords
corrosion, aluminum alloys, full-scale and laboratory corrosion testing.
Abstract

By certification of aluminium alloys the investigation of their liability to isolated types of corrosion determined in laboratory conditions is obligatory as well as investigation of corrosion resistance of materials determined in the course of full-scale exposition. Regularly environmental tests of aluminium alloys are carried out under the conditions of open areas. This paper shows that investigations under the roof are more significant for the given class of materials as they provide amplification of monitoring factors of corrosive process – damping duration of the surface and expansion in the number of chlorides. Also this paper throws light on correlation problems of laboratory and full-scale corrosion testing and presents the procedure of full-scale accelerated tests allowing to reduce the time of environmental tests by 4–5 times in comparison with the exposition under full-scale conditions.

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  2. Grinevich A.V., Lutsenko A.N., Karimova S.A. Dolgovechnost izdeliy i korrozionnaya ustalost konstruktsionnykh materialov [Durability of products and corrosion fatigue of constructional materials] // Voprosy materialovedeniya. 2013. №1. S. 220–229.
  3. Zhuk N.P. Kurs teorii korrozii i zashchity metallov [Course of the theory of corrosion and protection of metals]. M.: Metallurgiya, 1976. 472 s.
  4. GOST 9.913–90. Edinaya sistema zashchity ot korrozii i stareniya. Alyuminiy, magniy i ikh splavy. Metody uskorennykh korrozionnykh ispytaniy / Gos. komitet SSSR po standartam [GOST 9.913-90. Uniform system of corrosion protection and aging. Aluminum, magnesium and their alloys. Methods of the accelerated corrosion tests / State committee of the USSR on standards]. M., 1990. 10 s.
  5. GOST 9.021–74. Edinaya sistema zashchity ot korrozii i stareniya. Alyuminiy i splavy alyuminievye. Metody uskorennykh ispytaniy na mezhkristallitnuyu korroziyu / Gos. komitet SSSR po standartam [GOST 9.021-74. Uniform system of corrosion protection and aging. Aluminum and alloys aluminum. Methods of accelerated tests on between crystalline corrosion / State committee of the USSR on standards]. M., 1974. 4 s.
  6. GOST 9.904–82. Edinaya sistema zashchity ot korrozii i stareniya. Splavy alyuminievye. Metod uskorennykh ispytaniy na rasslaivayushchuyu korroziyu / Gos. komitet SSSR po standartam [GOST 9.904-82. Uniform system of corrosion protection and aging. Alloys aluminum. Method of accelerated tests on stratifying corrosion / State committee of the USSR on standards]. M., 1982. 10 s.
  7. GOST 9.019–74. Edinaya sistema zashchity ot korrozii i stareniya. Splavy alyuminievye i magnievye. Metody uskorennykh ispytaniy na korrozionnoe rastreskivanie / Gos. komitet SSSR po standartam [GOST 9.019-74. Uniform system of corrosion protection and aging. Alloys aluminum and magnesian. Methods of accelerated tests on corrosion cracking / State committee of the USSR on standards]. M., 1974. 18 s.
  8. Moran J.P., Bovard F.S., Chrzan J.D., Rioja R.J., Colvin E.L. Improvements in corrosion resistance offered by newer generation 2x99 aluminum-lithium alloys for aerospace applications // Proceedings of the12th International Conference on Aluminium Alloys. Yokohama, Japan. 2010. P. 1492–1497.
  9. Kablov E.N., Startsev O.V., Medvedev I.M. Obzor zarubezhnogo opyta issledovanij korrozii i sredstv zashhity ot korrozii [Review of international experience on corrosion and corrosion protection] // Aviacionnye materialy i tehnologii. 2015. №2 (35). S. 76–87.
  10. Semenychev V.V. Korrozionnaya stoykost i svoystva alyuminievykh splavov aviatsionnogo naznacheniya v usloviyakh morskogo subtropicheskogo klimata: dis. … kand. tekhn. nauk [Corrosion resistance and properties of aluminum alloys of aviation assignment in the conditions of sea subtropical climate: thesis … Cand. Tech. Sci.]. M., 2006. 125 s.
  11. Kablov E.N., Startsev O.V., Medvedev I.M., Panin S.V. Korrozionnaya agressivnost primorskoy atmosfery. Ch. 1. Faktory vliyaniya (obzor) [Corrosion aggression of the seaside atmosphere. P.1. Factors of influence (review)] // Korroziya: materialy, zashchita. 2013. №12. S. 6–18.
  12. Karimova S.A., Zhilikov V.P., Mikhaylov A.A., Chesnokov D.V., Igonin T.N., Karpov V.A. Naturno-uskorennye ispytaniya alyuminievykh splavov v usloviyakh vozdeystviya morskoy atmosfery [Natural accelerated tests of aluminum alloys in the conditions of influence of the sea atmosphere] // Korroziya: materialy, zashchita. 2012. №10. S. 1–3.
  13. Sinyavskiy V.S., Kalinin V.D., Aleksandrova T.V. Novyy metod uskorennykh korrozionnykh ispytaniy alyuminievykh splavov [New method of the accelerated corrosion tests of aluminum alloys] // Tekhnologiya legkikh splavov. 2013. №2. S. 89–93.
  14. Semenychev V.V. Korrozionnaya stoykost obraztsov splava 1201 v morskikh subtropikakh [Corrosion resistance of samples of alloy 1201 in sea subtropics] // Korroziya: materialy, zashchita. 2015. №3. S. 1–5.
  15. Panchenko Yu.M., Strekalov P.V., Chesnokov D.V., Zhirnov A.D., Zhilikov V.P., Karimova S.A., Tararaeva T.I. Zavisimost korrozionnoy stoykosti splava D16 ot zasolennosti i meteoparametrov primorskoy atmosfery [Dependence of corrosion resistance of alloy D16 on salinity and meteoparameters of the seaside atmosphere] // Aviacionnye materialy i tehnologii. 2010. №3. S. 8–14.
  16. Semenychev V.V. Korrozionnaya stojkost' listov splava D16ch.-T v morskih subtropikah [Corrosion resistance of alloy D16ch.-T sheets in marine subtropics] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №7. St. 11. Available at: http://www.viam-works.ru (accessed: December 15, 2015). DOI: 10.18577/2307-6046-2014-0-7-11-11.
  17. Rozenfeld I.L., Rubinshteyn F.I., Zhigalova K.A. Zashchita metallov ot korrozii lakokrasochnymi pokrytiyami [Protection of metals against corrosion by paint coatings]. M.: Khimiya, 1987. S. 7–9.
  18. Antipov V.V., Senatorova O.G., Tkachenko E.A., Vahromov R.O. Alyuminievye deformiruemye splavy [Aluminum deformable alloys] //Aviacionnye materialy i tehnologii. 2012. №S. S. 167–182.
  19. Khokhlatova L.B., Kolobnev N.I., Oglodkov M.S., Mikhaylov E.D. Alyuminiylitievye splavy dlya samoletostroeniya [Aluminum lithium alloys for aircraft construction] // Metallurg. 2012. №5. S. 31–35.
  20. Antipov V.V., Kolobnev N.I., Hohlatova L.B. Razvitie alyuminijlitievyh splavov i mnogostupenchatyh rezhimov termicheskoj obrabotki [Development aluminum lithium alloys and multistage modes of thermal processing] // Aviacionnye materialy i tehnologii. 2012. №S. S. 183–195.
  21. Klochkov G.G., Grushko O.E., Popov V.I., Ovchinnikov V.V., Shamraj V.F. Struktura, tehnologicheskie svojstva i svarivaemost listov iz splava V-1341 sistemy Al–Mg–Si [Structure, technological properties and bondability of sheets from alloy V-1341 of Al–Mg–Si system] //Aviacionnye materialy i tehnologii. 2011. №1. S. 3–8.
  22. Ryabov D.K., Kolobnev N.I., Samohvalov S.V., Mahsidov V.V. Vliyanie predvaritelnogo estestvennogo stareniya na svojstva splava 1913 v iskusstvenno sostarennom sostoyanii [Influence of preliminary natural aging on properties of alloy 1913 in artificially made old condition] // Aviacionnye materialy i tehnologii. 2013. №2. S. 8–11.
  23. 23 Kurs M.G., Karimova S.A. Naturno-uskorennye ispytaniya: osobennosti metodiki i sposoby ocenki korrozionnyh harakteristik alyuminievyh splavov [Salt-accelerated outdoor corrosion testing: methodology and evaluation of corrosion susceptibility of aluminum alloy] // Aviacionnye materialy i tehnologii. 2014. №1. S. 51–57.
  24. Andreattaa F., Druartb M.-E., Lanzuttiaandother A. Localized corrosion inhibition by cerium species on clad AA2024 aluminum alloy investigated by means of electrochemical micro-cell // Corrosion Science. 2012. V. 65. P. 376–386.