Properties and application of polymer composite materials based on glue prepregs

Kutsevich K.E., Dement’eva L.A., Lukina N.F.
Kutsevich K.E., Dement’eva L.A., Lukina N.F. Properties and application of polymer composite materials based on glue prepregs // Proceedings of VIAM. 2016. No. 8. DOI: 10.18577/2307-6046-2016-0-8-7-7. URL: https://www.viam-works.ru/en/journal/2016/8/7
Keywords
composite materials, adhesive prepregs, adhesive matrix, carbon and glass fillers, strength characteristics, the honeycomb structure.
Abstract

The properties of composite adhesive materials (CAM) based on wide range of adhesive prepregs on glass- and carbon fillers are presented. The information about benefits and features of PCM elements manufacturing process from adhesive prepregs is presented. The CAM application for manufacturing parts from PCM including the honeycomb structure, single or double curvature designed for operation at temperatures 80–175°C is shown. The research work is executed within implementation of the complex scientific direc-tion 13.2. «Constructional polymer composite materials» («The strategic directions of development of materials and technologies of their processing for the period up to 2030») [1].

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Istoriya aviacionnogo materialovedeniya. VIAM – 80 let: gody i lyudi / pod obshh. red. E.N. Kablova [The history of aviation materials science. VIAM – 80 years: years and people/ gen. ed. by E.N. Kablov]. M.: VIAM. 2012. 520 s.
  3. Batizat V.P., Anikhovskaya L.I., Dementeva L.A. Klei dlya skleivaniya konstrukcij iz metallov i kompozicionnykh materialov [Adhesives for structural gluing from metals and composite materials] // Aviacionnaya promyshlennost. 1983. №11. S. 15–17.
  4. Petrova A.P., Lukina N.F. Primenenie adgezionnykh gruntov i sistem modifikacii poverkhnosti pri skleivanii [Application of adhesive soils and systems of surface modification when agglutinating] // Klei. Germetiki. Tehnologii. 2013. №9. S. 24–28.
  5. Petrova A.P., Lukina N.F. Vliyanie adgezionnykh gruntov na resursnye kharakteristiki kleevykh soedinenij [Impact of adhesive soils on life characteristics of adhesive bindings] // Klei. Germetiki. Tehnologii. 2015. №11. S. 20–23.
  6. Prepreg i izdelie, vypolnennoe iz nego: pat. 2427594 Ros. Federaciya [Prepreg and product made from it: pat. 2427594 Russian Federation]; opubl. 23.07.13.
  7. Kablov E.N. Strategicheskie napravleniya razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda [The strategic directions of development of materials and technologies of their processing for the period to 2030] // Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  8. Grashhenkov D.V., Chursova L.V. Strategiya razvitiya kompozicionnyh i funkcionalnyh materialov [Strategy of development of composite and functional materials] // Aviacionnye materialy i tehnologii. 2012. №S. S. 231–242.
  9. Petrova A.P., Donskoj A.A., Chalykh A.E., Shherbina A.A. Kleyashhie materialy. Germetiki: spravochnik / pod red. A.P. Petrovoj [Adhesive materials. Sealants: reference book/ ed. by A.P. Petrova]. SPb.: Professional, 2008. S. 589.
  10. Lukina N.F., Dementeva L.A., Petrova A.P., Serezhenkov A.A. Konstrukcionnye i termostojkie klei [Constructional and heat-resistant glues] // Aviacionnye materialy i tehnologii. 2012. №S. S. 328–335.
  11. Antyufeeva N.V., Zhuravleva P.L., Aleksashin V.M., Kucevich K.E. Vliyanie stepeni otverzhdeniya svyazuyushhego na fiziko-mekhanicheskie svojstva ugleplastika i mikrostrukturu mezhfaznogo sloya uglerodnoe volokno/matrica [Influence of degree of curing binding on physical and mechanical properties of carbon fiber and microstructure of interphase layer of carbon fiber/matrix] // Klei. Germetiki. Tehnologii. 2014. №12. S. 26–30.
  12. Petrova A.P., Lukina N.F., Dementeva L.A., Avdonina I.A., Tyumeneva T.Yu., Zhadova N.S. Klei dlya aviacionnoj tekhniki [Adhesives for aviation engineering] // RZhKH. 2010. T. LIV. №1. C. 46–52.
  13. Kablov E.N., Minakov V.T., Anikhovskaya L.I. Klei i materialy na ikh osnove dlya remonta konstrukcij aviacionnoj tekhniki [Adhesives and materials based on them for repair of constructions of aviation engineering] // Aviacionnye materialy i tehnologii. 2002. №1. S. 61–65.
  14. Dement'eva L.A., Serezhenkov A.A., Bocharova L.I., Lukina N.F., Kucevich K.E., Petrova A.P. Svojstva kompozicionnykh materialov na osnove kleevykh prepregov [Properties of composite materials based on glue prepregs] // Klei. Germetiki. Tehnologii. 2012. №6. S. 19–24.
  15. Anikhovskaya L.I., Minakov V.T. Klei i kleevye prepregi dlya perspektivnykh izdelij aviakosmicheskoj tekhniki [Adhesives and glue prepregs for advanced products of aviation engineering] // Aviacionnye materialy. Izbrannye trudy «VIAM» 1932–2002: yubilejnyj nauch.-tekhnich. sb. M.: MISiS–VIAM, 2002. S. 315–326.
  16. Lukina N.F., Dementeva L.A., Petrova A.P., Tyumeneva T.Yu. Svojstva kleev i kleyashhikh materialov dlya izdelij aviacionnoj tekhniki [Properties of adhesives and gluing materials for articles of aviation engineering] // Klei. Germetiki. Tehnologii. 2009. №1.
  17. S. 14–24.
  18. Dementeva L.A., Lukina N.F., Serezhenkov A.A., Kucevich K.E. Osnovnye svojstva i naznachenie PKM na osnove kleevykh prepregov [Main properties and destination of PCM based on adhesive prepregs] // Konstrukcii i tekhnologiya polucheniya izdelij iz nemetallicheskikh materialov: tez. dokl. KHIKH Mezhdunar. nauch.-tekhnich. konf. Obninsk: ONPP «Tekhnologiya», 2010. S. 11–12.
  19. Morozov B.B. Primenenie polimernykh kompozicionnykh materialov v izdeliyakh razrabotki OKB Sukhogo [Application of polymer composite materials in articles produced by experimental design bureau Sukhoi] // Kleyashhie materialy aviacionnogo naznacheniya: sb. dokl. konf. M.: VIAM, 2013. S. 31–36.
  20. KHrychev Yu.I., Shkodinova E.P., Dement'eva L.A. Razrabotka tekhnologicheskogo processa izgotovleniya radioprozrachnogo obtekatelya iz kleevykh prepregov tipa KMKS-2m.120 [Technologies development of manufacturing process of radio transparent fairing from glue prepregs of KMKS-2M.120 type] // Kleyashhie materialy aviacionnogo naznacheniya: sb. dokl. konf. M.: VIAM, 2013. S. 43–47.
  21. Lukina N.F., Dement'eva L.A., Petrova A.P., Kirienko T.A., Chursova L.V. Kleevye svyazuyushhie dlya detalej iz PKM sotovoj konstrukcii [Adhesive bindings for details from PCM of honeycomb] // Klei. Germetiki. Tehnologii. 2016 (v pechati).
  22. Dementeva L.A., Serezhenkov A.A., Lukina N.F., Kucevich K.E. Kleevye prepregi i sloistye materialy na ih osnove [Adhesive prepregs and layered materials on their basis] // Aviacionnye materialy i tehnologii. 2013. №2. S. 19–21.
  23. Dementeva L.A., Serezhenkov A.A., Bocharova L.I., Anikhovskaya L.I., Lukina N.F. Kompozicionnye materialy kleevye na osnove steklyannykh i uglerodnykh napolnitelej [Composite glue materials based on glass and carbon fillers] // Klei. Germetiki. Tehnologii. 2009. №1. S. 24–27.
  24. Lukina N.F., Chursova L.V. Laboratoriya «Klei i kleevye prepregi» – dostizheniya i perspektivy [Laboratory “Adhesives and glue prepregs” – achievements and perspectives] // Kleyashhie materialy aviacionnogo naznacheniya: sb. dokl. konf. M.: VIAM, 2013. S. 1–5.
  25. Lukina N.F., Dementeva L.A., Serezhenkov A.A., Kotova E.V., Senatorova O.G., Sidelnikov V.V., Kutsevich K.E. Adhesive prepregs and composite materials on their basis // Russian Journal of General Chemistry. 2011. V. 81. №5. С. 1022–1024.
  26. Kucevich K.E., Dement'eva L.A., Lukina N.F., Chursova L.V. Vliyanie polisul'fonov razlichnogo stroeniya na svojstva kleevykh materialov [Impact of polysulfones of different structure on properties of adhesive materials] // Klei. Germetiki. Tehnologii. 2014. №4. S. 6–8.