Polymer composite materials in the Russian railways
UDC
678.8: 656.02
DOI
10.18577/2307-6046-2016-0-7-12-12
Article PDF (Russian)
(709.41 KB)
How to cite
Doriomedov M.S., Daskovskiy M.I., Skripachyov S.Yu., Shein E.A. Polymer composite materials in the Russian railways // Proceedings of VIAM. 2016. No. 7. DOI: 10.18577/2307-6046-2016-0-7-12-12. URL: https://www.viam-works.ru/en/journal/2016/7/12
Keywords
polymer composite material, railways.
Abstract
Companies engaged in development and introduction of polymer composite materials in the rail transport in Russia are presented. Structures based on composites are exemplified. Brief analysis of main advantages of their application comparing with traditional materials and recommendations on improvement of composite materials implementation in railway are provided. The work is executed within the frames of the complex scientific direction 13.1. «Binders for polymer and composite materials for structural and special purpose» («The strategic directions of development of materials and technologies of their processing for the period till 2030»)
Reference list
- Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
- Bogdanov A. Plastiki na relsah [Plastics on rails] // Plastik. 2013. №8 (126). S. 16–22.
- G. Welty. «Railway Age», 1997, N 8, pр. 41, 43–45. Available at: http://center-science.ru/files/zgd.pdf (accessed: January 20, 2016).
- Daskovskij M.I., Doriomedov M.S., Skripachev S.Yu. Sistematizaciya bazisnyh faktorov, prepyatstvuyushhih vnedreniyu polimernyh kompozicionnyh materialov v Rossii (obzor) [Underlying factors preventing the introduction of polymer composite materials in Russia (review)] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2016. №5 St. 06. Available at: http://www.viam-works.ru (accessed: May 20, 2016). DOI: 10.18577/2307-6046-2016-0-5-6-6.
- Petrov A.V., Doriomedov M.S., Skripachev S.Yu. Zarubezhnyj opyt razvitiya proizvodstva izdelij s ispolzovaniem vtorichno pererabotannyh polimernyh kompozicionnyh materialov (obzor) [Foreign experience of manufacturing products using recycled polymer composites (review)] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №12. St. 12. Available at: http://www.viam-works.ru (accessed: January 20, 2016). DOI: 10.18577/2307-6046-2015-0-12-12-12.
- Petrov A.V., Doriomedov M.S., Skripachev S.Yu. Tehnologii utilizacii polimernyh kompozicionnyh materialov (obzor) [Recycling technologies of polymer composite materials (review)] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №8. St. 09. Available at: http://www.viam-works.ru (accessed: January 20, 2016). DOI: 10.18577/2307-6046-2015-0-8-9-9.
- Kablov E.N. Kompozity: segodnya i zavtra [Composites: today and tomorrow] // Metally Evrazii. 2015. №1. S. 36–39.
- Kablov E.N. Materialy – osnova lyubogo dela [Materials – basis of any business] // Delovaya slava Rossii. 2013. №2 (40). S. 4–9.
- Kablov E.N. Innovacionnoe razvitie – vazhnejshij prioritet gosudarstva [Innovative development – the most important priority of the state] // Metally Evrazii. 2010. №2. S. 6–11.
- Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace materials science] // Vse materialy. Enciklopedicheskij spravochnik. 2008. №3. S. 2–14.
- Kablov E.N., Karimova S.A., Semenova L.V. Korrozionnaya aktivnost ugleplastikov i zashhita metallicheskih silovyh konstrukcij v kontakte s ugleplastikom [Corrosion activity carbon plastics and protection of metal load bearing structures in contact with the carbon plastics] // Korroziya: materialy, zashhita. 2011. №12. S. 1–7.
- Vlasenko F.S., Raskutin A.E. Primenenie polimernyh kompozicionnyh materialov v stroitelnyh konstrukcijah [Applying FRP in building structures] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №8. St. 03. Available at: http://www.viam-works.ru (accessed: January 20, 2016).
- Kablov E.N. Sovremennye materialy – osnova innovacionnoj modernizacii Rossii [Modern materials – basis of innovative modernization of Russia] // Metally Evrazii. 2012. №3. S. 10–15.
- Kablov E.N. VIAM: prodolzhenie puti [VIAM: way continuation] // Nauka v Rossii. 2012. №3. S. 36–44.
- Kablov E.N., Grashhenkov D.V., Erasov V.S., Anchevskij I.E., Il'in V.V., Valter R.S. Stend dlya ispytaniya na klimaticheskoj stancii GCKI krupnogabaritnyh konstrukcij iz PKM [The stand for testing for the GTsKI climatic stations of large-size designs from PKM] // Sb. dokl. IX Mezhdunar. nauch. konf. po gidroaviacii «Gidroaviasalon-2012». 2012. S. 122–123.