To the question of methodology for testing of polymer materials on resistance to solar radiations effect (review)

Pavlov M.R., Nikolaev E.V., Andreeva N.P., Barbotko S.L.
Pavlov M.R., Nikolaev E.V., Andreeva N.P., Barbotko S.L. To the question of methodology for testing of polymer materials on resistance to solar radiations effect (review) // Proceedings of VIAM. 2016. No. 7. DOI: 10.18577/2307-6046-2016-0-7-11-11. URL: https://www.viam-works.ru/en/journal/2016/7/11
Keywords
polymer materials, outdoor weathering, accelerated weathering test, weathering factors, photochemical stability, irradiance, xenon discharge lamp.
Abstract

An overview of modern methods of polymer materials testing on aging under the influence of natural and artificial weathering factors is presented. The mechanisms of thermal and photo-degradation of polymers under the influence of solar radiation are described. The basic parameters of equipment used for testing are shown. A comparison of the spectral distribution of the intensity of natural sunlight radiation and a radiation generated by the arc xenon lamp is performed. A comparison is conducted and found differences in the methods of accelerated laboratory tests for Russian and foreign standards are presented. The conclusions are made about the need to update the existing regulations in the Russian Federation. The work is executed within the frames of the complex scientific directions 18.2. «Development of methods of climatic tests and instrumental methods of research», 18.3. «Modeling and forecasting of climatic resistance» («The strategic directions of development of materials and t

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  2. Kablov E.N. Sovremennye materialy – osnova innovacionnoj modernizacii Rossii [Modern materials – basis of innovative modernization of Russia] // Metally Evrazii. 2012. №3. S. 10–15.
  3. Kablov E.N. Materialy i himicheskie tehnologii dlya aviacionnoj tehniki [Materials and chemical technologies for aviation engineering] // Vestnik Rossijskoj akademii nauk. 2012. T. 82. №6. S. 520–530.
  4. Mishra G., Mohapatra S.R., Behera P.R., Dash B., Mohanty U.K., Ray B.C. Environmental stability of GFRP laminated composites: an emphasis on mechanical behaviour // Aircraft Eng. and Aerosp. technol. 2010. V. 82. №4. P. 258–266.
  5. Kablov E.N., Gunyaev G.M. Tumanov A.T. – iniciator sozdaniya kompozitov [A.T Tumanov – initiator of creation of composites] // Kompozicionnye materialy v aviakosmicheskom materialovedenii: sb. tez. dokl. Mezhotrasl. nauch.-tehnich. konf. M.: VIAM, 2009. S. 6–9.
  6. Muhametov R.R., Ahmadieva K.R., Chursova L.V., Kogan D.I. Novye polimernye svyazujushhie dlya perspektivnyh metodov izgotovleniya konstrukcionnyh voloknistyh PKM [New polymeric binding for perspective methods of manufacturing of constructional fibrous PCM] //Aviacionnye materialy i tehnologii. 2011. №2. S. 38–42.
  7. 7 Kirillov V.N., Vapirov Yu.M., Drozd E.A. Issledovanie atmosfernoj stojkosti polimernyh kompozicionnyh materialov v usloviyah atmosfery teplogo vlazhnogo i umerenno teplogo klimata [Research of atmospheric firmness of polymeric composite materials in the conditions of the atmosphere of warm wet and moderately warm climate] // Aviacionnye materialy i tehnologii. 2012. №4. S. 31–38.
  8. Sorokin A.E., Bejder E.Ya., Perfilova D.N. Vliyanie klimaticheskih faktorov na svojstva ugleplastika na polifenilensulfidnom svyazuyushhem [Effect of climatic factors on properties of carbon fiber reinforced plastic based on polyphenylenesulfide resin] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №1. St. 10. Available at: http://www.viam-works.ru (accessed: September 20, 2015). DOI: 10.18577/2307-6046-2015-0-1-10-10.
  9. Voinov S.I., Zhelezina G.F., Soloveva N.A., Yamshhikova G.A., Timoshina L.N. Vliyanie vneshnej sredy na svojstva ugleplastika, poluchennogo metodom propitki pod davleniem (RTM) [Environmental effects on properties of CFRP manufactured by RTM method] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №2. St. 08. Available at: http://www.viam-works.ru (accessed: September 20, 2015). DOI: 10.18577/2307-6046-2015-0-2-8-8.
  10. Tkachuk A.I., Grebeneva T.A., Chursova L.V., Panina N.N. Termoplastichnye svyazuyushhie. Nastoyashhee i budushhee [Thermoplastic binders. The present and the future] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №11. St. 07. Available at: http://www.viam-works.ru (accessed: September 20, 2015).
  11. Efimov V.A., Shvedkova A.K., Korenkova T.G., Kirillov V.N. Issledovanie polimernyh konstrukcionnyh materialov pri vozdejstvii klimaticheskih faktorov i nagruzok v laboratornyh i naturnyh usloviyah [Research of polymeric constructional materials at influence of climatic factors and loadings in laboratory and natural conditions] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №1. St. 05. Available at: http://viam-works.ru (accessed: September 20, 2015).
  12. Kuleznev V.N., Ushakova O.B. Struktura i mehanicheskie svojstva polimerov [Structure and mechanical properties of polymers]. M.: MITHT, 2006. 86 s.
  13. Arhireev V.P. Starenie i stabilizaciya polimerov [Aging and stabilization of polymers]. Kazan: KGTU, 2002. 88 s.
  14. Kirillov V.N., Efimov V.A., Nikolaev E.V., Shvedkova A.K., Korenkova T.G., Deev I.S. K voprosu o metodike provedeniya naturnyh klimaticheskih ispytanij polimernyh kompozicionnyh materialov [To question of technique of carrying out natural climatic tests of polymeric composite materials] // Sb. dokladov VIII nauch. konf. po gidroaviacii «Gidroaviasalon–2010». M., 2010. Ch. II. S. 102–106.
  15. Nikolaev E.V., Kirillov V.N., Efimov V.A., Grashhenkov D.V. Moskovskij centr klimaticheskih ispytanij FGUP «VIAM» – regionalnyj centr ispytanij materialov v predstavitelnoj zone umerennogo klimata» [The Moscow center of climatic tests of VIAM Federal State Unitary Enterprise – the regional center of tests of materials in representative zone of temperate climate»] // Sb. dokladov IX nauch. konf. po gidroaviacii «Gidroaviasalon–2012». M. 2012. Ch. II. S. 202–208.