Quality control of covers of arch elements of elevated parts of support of fast-erected bridge constructions from PСM

Murashov V.V., Slyusarev M.V., Evdokimov A.A.
Murashov V.V., Slyusarev M.V., Evdokimov A.A. Quality control of covers of arch elements of elevated parts of support of fast-erected bridge constructions from PСM // Proceedings of VIAM. 2016. No. 7. DOI: 10.18577/2307-6046-2016-0-7-10-10. URL: https://www.viam-works.ru/en/journal/2016/7/10
Keywords
arch elements, non-destructive testing (NDT), acoustic impedance method (AIM), polymeric composite materials (PCM).
Abstract

Research results on possibility of non-destructive quality testing of PCM covers of arch elements applied in bridges are considered. Applicability of acoustic impedance method for identification of material integrity disturb in the form of zones with poor binder impregnation at formation, exfoliation and filling degree of arch elements by concrete is shown. The work is executed within implementation of the complex scientific direction 2.3. «Methods of nondestructive research and control» («The strategic directions of development of materials and technologies of their processing for the period till 2030»)

Reference list
  1. Kablov E.N. Strategicheskie napravleniya razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda [The strategic directions of development of materials and technologies of their processing for the period to 2030] // Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  2. Kablov E.N. Kontrol kachestva materialov – garantiya bezopasnosti ekspluatacii aviacionnoj tehniki // Aviacionnye materialy i tehnologii [Quality control of materials – security accreditation of operation of aviation engineering]. M.: VIAM, Vyp.: Metody ispytanij i kontrolya kachestva metallicheskih i nemetallicheskih materialov. 2001. S. 3–8.
  3. Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace materials science] // Vse materialy. Enciklopedicheskij spravochnik. 2008. №3. S. 2–14.
  4. Nerazrushayushhij kontrol: spravochnik v 8 t. 2-e izd., ispr. / pod obshh. red. V.V. Klyueva [Non-destructive testing: directory in 8 vol. / gen. ed. by V. V. Kluyev]. M.: Mashinostroenie, 2006. T. 3. Ultrazvukovoj control / I.N. Ermolov, Yu.V. Lange. 864 s.
  5. Murashov V.V., Rumyancev A.F. Defekty monolitnyh detalej i mnogoslojnyh konstrukcij iz polimernyh kompozicionnyh materialov i metody ih vyyavleniya. Chast 1. Defekty monolitnyh detalej i mnogoslojnyh konstrukcij iz polimernyh kompozicionnyh materialov [Defects of monolithic details and multi-layer designs from polymeric composite materials and methods of their identification. Part 1. Defects of monolithic details and multi-layer designs from polymeric composite materials] // Kontrol. Diagnostika. 2007. №4. C. 23–31.
  6. Murashov V.V. Types of production and operational defects of the multilayer glued constructions and polymer composite materials products and methods to detect them // Proc. 5th European-American Workshop on Reliability of NDT. 2013. Available at: http://www.nde-reliability.de/Proceedings/Posters (accessed: July 12, 2015).
  7. Murashov V.V., Mishurov K.S. Opredelenie poristosti ugleplastikov v aviacionnyh konstrukciyah ultrazvukovym metodom [The determinations of carbon fiber reinforced plastics porosity in aircraft constructions by the ultrasonic method] //Aviacionnye materialy i tehnologii. 2015. №2 (35). S. 88–92.
  8. Kablov E., Murashov V., Rumyantsev A. Diagnostics of Polymer Composites by Acoustic Methods // Ultrasound. 2006. №2. Р. 7–10.
  9. Murashov V.V., Rumyancev A.F., Ivanova G.A., Fajzrahmanov N.G. Diagnostika struktury, sostava i svojstv polimernyh kompozicionnyh materialov [Diagnostics of structure, structure and properties of polymeric composite materials] // Aviacionnye materialy i tehnologii. 2008. №1. S. 17–24.
  10. Bobrov V.T., Rozlovenko S.G., Murashov V.V. Materials characterization // Testing. Diagnostics. 2010. №2. S. 42–44.
  11. Murashov V.V. Opredelenie fiziko-mehanicheskih harakteristik i sostava polimernyh kompozicionnyh materialov akusticheskimi metodami [Definition of physicomechanical characteristics and composition of polymeric composite materials acoustic methods] // Aviacionnye materialy i tehnologii. 2012. №S. S. 465–475.
  12. Karabutov A.A., Murashov V.V., Oraevsky A.A., Podymova N.B. Nondestructive characterization of layered composite materials with a laser optoacoustic sensor // Conf. Nondestructive Evaluation of Materials and Composites II. San Antonio: Published by SPIE, 1998. V. 3396. Р. 103–111.
  13. Karabutov A.A., Murashov V.V., Podymova N.B. Diagnostika sloistyh kompozitov s pomoshh'yu lazernogo optiko-akusticheskogo preobrazovatelya [Diagnostics of layered composites by means of the laser optics-acoustic converter] // Mehanika kompozitnyh materialov. 1999. T. 35. №1. S. 125–134.
  14. Sposob opredeleniya fiziko-mehanicheskih harakteristik polimernyh kompozicionnyh materialov i ustrojstvo dlya ego osushhestvleniya: pat. 2214590 Ros. Federaciya [Way of definition of physicomechanical characteristics of polymeric composite materials and the device for its implementation: stalemate. 2214590 Rus. Federation]; opubl. 20.10.03 Byul. №29.
  15. Murashov V.V. K voprosu opredeleniya uprugih i prochnostnyh svojstv polimernyh kompozicionnyh materialov akusticheskim kompleksnym metodom [To question of determination of elastic and strength properties of polymeric composite materials acoustic complex method] // Deformaciya i razrushenie materialov. 2014. №11. S. 39–45.
  16. Murashov V.V., Rumyancev A.F. Diagnostika sostava i svojstv polimernyh kompozitov v detalyah i konstrukciyah [Diagnostics of structure and properties of polymeric composites in details and designs] // Kontrol. Diagnostika. 2008. № 8. S. 13–17.
  17. Murashov V.V. Opredelenie sostava i plotnosti konstrukcionnyh ugleplastikov lazerno-akusticheskim sposobom ul'trazvukovogo kontrolya [Definition of structure and density constructional ugleplastikov in the laser and acoustic way of ultrasonic control] // Materialovedenie. 2014. №11. S. 24–29.
  18. Murashov V. The determinations of CFRP porosity by laser-acoustic method of ultrasonic control // Proc. of the 4th International Conference on Thermosets 2015. Berlin: Fraunhofer Research Institution for Polymeric Materials and Composites PYCO. 2015. P. 58–60. URL: http://www.thermosets.de/Proceedings (дата обращения: 20.12.2015).
  19. Rose J.L., Soley L.E. Ultrasonic guided waves for anomaly detection in aircraft components // Materials Evaluation. 2000. V. 58. №9. Р. 1080–1086.
  20. Hsu D.K., Dayat V., Barnard D.J. Technology of production of samples to configure and control of the equipment for the control of glue joints // Materials Evaluation. 2009. V. 67. №7. P. 843–850.
  21. Armstrong N. Control of honeycomb panels and products made of foam by amplitude method of passing // Materials Evaluation. 2010. V. 68. №12. P. 27–31.
  22. Murashov V.V., Rumyancev A.F. Defektoskopiya i diagnostika polimernyh kompozicionnyh materialov akusticheskimi metodami [Defectscopy and diagnostics of polymeric composite materials by acoustic methods] // 75 let. Aviacionnye materialy. Izbrannye trudy «VIAM» 1932–2007: yubilejnyj nauch.-tehnich. sb. M.: VIAM, 2007. S. 342–347.
  23. Murashov V.V., Rumyancev A.F. Defekty monolitnyh detalej i mnogoslojnyh konstrukcij iz polimernyh kompozicionnyh materialov i metody ih vyyavleniya. Chast 2. Metody vyyavleniya defektov monolitnyh detalej i mnogoslojnyh konstrukcij iz polimernyh kompozicionnyh materialov [Defects of monolithic details and multi-layer designs from polymeric composite materials and methods of their identification. Part 2. Methods of detection of defects of monolithic details and multi-layer designs from polymeric composite materials] // Kontrol. Diagnostika. 2007. №5. S. 31–42.
  24. Gunasekera A.M. Monitoring of impact damage products from PCM // Materials Evaluation. 2010. V. 68. №8. Р. 880–887.
  25. Murashov V.V., Trifonova S.I. Kontrol kleevyh soedinenij v konstrukciyah i izdeliyah iz PKM ul'trazvukovym tenevym metodom [Control of glued joints in designs and products from PKM ultrasonic shadow method] // Klei. Germetiki. Tehnologii. 2015. №5. S. 15–23.
  26. Murashov V.V., Laptev A.S. Kontaktnye zhidkosti dlya sozdaniya akusticheskogo kontakta pri ul'trazvukovom kontrole mnogoslojnyh konstrukcij iz PKM [Contact liquids for creation of an acoustic contact at ultrasonic control of multi-layer structures from PCM] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №8. St. 10. Available at: http://viam-works.ru (accessed: December 20, 2015). DOI: 10.18577/2307-6046-2015-0-8-10-10.
  27. Murashov V.V., Kosarina E.I., Generalov A.S. Kontrol kachestva aviacionnyh detalej iz polimernyh kompozicionnyh materialov i mnogoslojnyh kleevyh konstrukcij [Quality control of aviation parts made from polymer composite materials and multilayers adhered constructions] // Aviacionnye materialy i tehnologii. 2013. №3. S. 65–70.
  28. Lange Yu.V. Akusticheskie nizkochastotnye metody i sredstva nerazrushayushhego kontrolya mnogoslojnyh konstrukcij [Acoustic low-frequency methods and means of non-destructive testing of multilayer designs]. M.: Mashinostroenie, 1991. 272 s.
  29. Murashov V.V. Kontrol kleenyh konstrukcij [Control of the glued designs] // Klei. Germetiki. Tehnologii. 2005. №1. S. 21–27.
  30. Murashov V.V. Nerazrushayushhij kontrol kleevyh soedinenij [ Non-destructive testing of glued joints] // Klei. Germetiki. Tehnologii. 2008. №7. S. 21–28.
  31. Murashov V.V. Kontrol mnogoslojnyh kleenyh konstrukcij iz polimernyh kompozicionnyh materialov [Control of multi-layer glued designs from polymeric composite materials] // Klei. Germetiki. Tehnologii. 2011. №10. S. 16–23.
  32. Murashov V.V., Generalov A.S. Kontrol mnogoslojnyh kleenyh konstrukcij nizkochastotnymi akusticheskimi metodami [Control of multilayer adhesive structures operating in severe climatic condition] // Aviacionnye materialy i tehnologii. 2014. №2. S. 59–67.
  33. V.V. Murashov, S.I. Trifonova Kontrol kachestva polimernyh kompozicionnyh materialov ultrazvukovym vremennym sposobom velosimetricheskogo metoda [Quality control of polymer composite materials using ultrasonic time-of-flight velocimetric technique] //Aviacionnye materialy i tehnologii. 2015. №4 (37). S. 86–90. DOI: 10.18577/2071-9140-2015-0-4-86-90.
  34. Murashov V.V. Vyyavlenie zon otsutstviya adgezionnogo soedineniya sloev v mnogoslojnyh konstrukciyah [Identification of zones of lack of adhesive connection of layers in multi-layer designs] // Klei. Germetiki. Tehnologii. 2013. №3. S. 29–31.
  35. Murashov V.V. Nerazrushayushhij kontrol zagotovok i detalej iz uglerod-uglerodnogo kompozicionnogo materiala dlya mnogorazovogo kosmicheskogo korablya «Buran» [Non-destructive testing of preparations and details from carbon - carbon composite material for the reusable «Buran» spacecraft] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №4. St. 05. Available at: http://www.viam-works.ru (accessed: October 04, 2015).
  36. Murashov V.V. Attestation of Glued Articles by Acoustic Impedance Method // Polymer Science. Series D: Glues and Sealing Materials. 2010. V. 3. №4. Р. 267–273.
  37. Viktorov I.A. Fizicheskie osnovy primeneniya ultrazvukovyh voln Releya i Lemba v tehnike [Physical bases of application of ultrasonic waves of Reley and Lamb in equipment]. M.: Nauka, 1966. S. 84–87.
  38. Kablov E.N., Grashhenkov D.V., Erasov V.S., Anchevskij I.E., Ilin V.V., Valter R.S. Stend dlya ispytaniya na klimaticheskoj stancii GCKI krupnogabaritnyh konstrukcij iz PKM [The stand for testing for the GTsKI climatic stations of large-size designs from PCM] // Sb. dokl. IX Mezhdunar. nauch. konf. po gidroaviacii. «Gidroaviasalon-2012». 2012. S. 122–123.