Comparative analysis of stickiness determination methods of prepreg

Orlov E.V., Gusev Y.A., Khrulkov A.V., Korotkov I.A.
Orlov E.V., Gusev Y.A., Khrulkov A.V., Korotkov I.A. Comparative analysis of stickiness determination methods of prepreg // Proceedings of VIAM. 2016. No. 7. DOI: 10.18577/2307-6046-2016-0-7-9-9. URL: https://www.viam-works.ru/en/journal/2016/7/9
Keywords
ATL, AFP, polymer composite material, prepreg, resin, tack.
Abstract

ATL and AFP methods of automated placement are widely used worldwide to increase the productivity and accuracy of prepregs placement in manufacture of large PCM-based parts. However conventional prepregs are not always suitable for processing by these methods - they are subject to specific requirements in technological tack providing with precise fixation and orientation of layers and easy separation from backing paper. There is no standard method for the tack determination, so this article reviews various widely used in Russian and international industry tack determination methods, conclusions are made on their precision, efficiency and usability for different prepreg laying methods. The work was executed within implementation of the complex scientific direction 13.2. «Constructional PCM» («The strategic directions of development of materials and technologies of their processing for the period till 2030»)

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  2. Kablov E.N. Aviacionnoe materialovedenie: itogi i perspektivy [Aviation materials science: results and perspectives] // Vestnik Rossijskoj akademii nauk. 2002. T. 72. №1. S. 3–12.
  3. Kablov E.N. Materialy i himicheskie tehnologii dlya aviacionnoj tehniki [Materials and chemical technologies for aviation engineering] // Vestnik Rossijskoj akademii nauk. 2012. T. 82. №6. S. 520–530.
  4. Kablov E.N. Shestoj tehnologicheskij uklad [Sixth technological way] // Nauka i zhizn. 2010. №4. S. 2–7.
  5. Epoksidnaya kompoziciya: pat. 2447104 Ros. Federaciya [Epoxy composition: pat. 2447104 Rus. Federation]; opubl. 05.10.10.
  6. Muhametov R.R., Ahmadieva K.R., Kim M.A., Babin A.N. Rasplavnye svyazujushhie dlya perspektivnyh metodov izgotovleniya PKM novogo pokoleniya [Melt binding for perspective methods of production of PCM of new generation] // Aviacionnye materialy i tehnologii. 2012. №S. S. 260–265.
  7. Shaghaghi S., Beheshty M.H., Rahimi H. Preparation and rheological characterization of phenolic/glass prepregs // Iranian Polymer Journal. 2011. V. 20 (12). P. 969–977.
  8. Muhametov R.R., Ahmadieva K.R., Chursova L.V., Kogan D.I. Novye polimernye svyazujushhie dlya perspektivnyh metodov izgotovleniya konstrukcionnyh voloknistyh PKM [New polymeric binding for perspective methods of manufacturing of constructional fibrous PCM] //Aviacionnye materialy i tehnologii. 2011. №2. S. 38–42.
  9. Timoshkov P.N., Hrulkov A.V. Sovremennye tehnologii pererabotki polimernyh kompozitsionnyh materialov, poluchaemyh metodom propitki rasplavnym svyazuyushchim [Modern technologies of hotmelt polymer composite materials processing] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №8. St. 04. Available at: http://www.viam-works.ru (accessed: January 19, 2016). DOI: 10.18577/2307-6046-2014-0-8-4-4.
  10. Grimshaw M.N. Automated Tape Laying // Composites. 2001. V. 21. P. 480–500.
  11. Gusev Yu.A., Borshhev A.V., Khrulkov A.V. Osobennosti prepregov dlya avtomatizirovannoj vykladki metodami ATL i AFP [Features of prepregs intended for automated laying by ATL and AFP technologies] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №3. St. 06. Available at: http://www.viam-works.ru (accessed: January 20, 2016). DOI: 10.18577/2307-6046-2015-0-3-6-6.
  12. Platonov A.A., Dushin M.I. Konstrukcionnyj ugleplastik VKU-25 na osnove odnonapravlennogo preprega [Carbon composites VKU-25 based on unidirectional prepregs] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №11. St. 06. Available at: http://www.viam-works.ru (accessed: January 20, 2016). DOI: 10.18577/2307-6046-2015-0-11-6-6.
  13. Banks R. et al. Development of a new structural prepreg: characterisation of handling, drape and tack properties // Composite Structures. 2004. V. 66 (1–4). P. 169–174.
  14. Crossley R.J., Schubel P.J., Warrior N.A. The experimental determination of prepreg tack and dynamic stiffness // Composites. Part A. 2012. V. 43. P. 423–434.
  15. Crossley R.J., Schubel P.J., Warrior N.A. The experimental characterisation and Investigate on of prepreg tack / In Proceedings of ICCM-18. Edinburgh. 2009. P. 1–11.
  16. Postnov V.I., Nikitin K.E., Petuhov V.I., Burhan O.L., Orzaev V.G. Metod i ustrojstvo dlya opredeleniya lipkosti prepregov [Method and the device for determination of stickiness of prepregs] // Aviacionnye materialy i tehnologii. 2009. №3. S. 29–33.