Research of layered metal composite material of Ti–TiAl3 system

Krasnov E.I., Shteinberg A.S., Shavnev A.A., Serpova V.M., Zhabin A.N.
Krasnov E.I., Shteinberg A.S., Shavnev A.A., Serpova V.M., Zhabin A.N. Research of layered metal composite material of Ti–TiAl3 system // Proceedings of VIAM. 2016. No. 7. DOI: 10.18577/2307-6046-2016-0-7-3-3. URL: https://www.viam-works.ru/en/journal/2016/7/3
Keywords
layered composite material, titanium, aluminum, intermetallic, surface foil blanks, degassing, diffusion.
Abstract

Research work on synthesis of layered metal composite material of the Ti–TiAl3 system by the method of vacuum reaction synthesis and the method of electrothermal explosion are conducted. The optimal temperature and time parameters of formation of intermetallic phase in the layered composite material are determined. The underlying conditions of gas emission and the possibility of outgassing treatment in the process of preparation to the intermetallides synthesis are considered. The work is performed within the framework of an integrated research direction 12.2. «Metal intermetallic and metal–ceramics systems layered metal matrix composites (MMC) for lightweight protection» («Strategic directions of development of materials and technologies to process them for the period up to 2030»)

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  2. Istoriya aviacionnogo materialovedeniya. VIAM – 80 let: gody i lyudi / pod obshh. red. E.N. Kablova [History of aviation materials science. VIAM – 80 years: years and people / gen. ed. by E.N. Kablov]. M.: VIAM, 2012. S. 143–156.
  3. Kablov E.N. Himiya v aviacionnom materialovedenii [Chemistry in aviation materials science] // Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 3–4.
  4. Kablov E.N. Materialy i himicheskie tehnologii dlya aviacionnoj tehniki [Materials and chemical technologies for aviation engineering] // Vestnik Rossijskoj akademii nauk. 2012. T. 86. №6. S. 520–530.
  5. Tarasov Yu.M., Antipov V.V. Novye materialy VIAM – dlya perspektivnoj aviacionnoj tehkniki proizvodstva OAO «OAK» [The VIAM new materials – for perspective aviation engineering of production of JSC «OAK»] // Aviacionnye materialy i tehnologii. 2012. №2. S. 5–6.
  6. Shmotin Yu.N., Starkov R.Yu., Danilov D.V., Ospennikova O.G., Lomberg B.S. Novye materialy dlya perspektivnogo dvigatelya OAO «NPO „Saturn”» [New materials for the perspective engine of JSC «NPO „Saturn”»] // Aviacionnye materialy i tehnologii. 2012. №2. S. 6–8.
  7. Li T., Fenghun J., Olevsky E.A., Vecchio K.S., Meyers M.A. Damage evolution in Ti6Al4V–Al3Ti metal-intermetallic laminate composites // Materials Science and Engineering: A. V. 443. 2007.
  8. P. 1–15.
  9. Vecchio K.S. Synthetic Multifunctional Metallic-Intermetallic Laminate Composites // JOM. 2005. March. P. 25–31.
  10. Process for making metallic/intermetallic composite laminate materian and materials so produced especially for use in lightweight armor: pat. 6357332 US; publ. 19.03.2002.
  11. Sauthoff G. Intermetallics. Weinheim: VCH Publishers, 1995. P. 14.
  12. Krasnov E.I., Shtejnberg A.S., Shavnev A.A., Berezovskij V.V. Issledovanie sloistogo metallicheskogo kompozicionnogo materiala sistemy Ti–TiAl3 [Study of Ti–TiAl3 laminate metal composite material ] // Aviacionnye materialy i tehnologii. 2013. №3. S. 16–19.
  13. Berlin A.A., Shtejnberg A.S., Krasnov E.I., Shavnev A.A., Lomov S.B., Serpova V.M. Eksperimentalnoe issledovanie polucheniya sloistyh kompozicionnyh materialov metodom elektroteplovogo vzryva. Ocenka ostatochnyh napryazhenij [Experimental study of receipt of layer composite materials by the method of electro-thermal explosion. Аssessment of residual stresses] // Aviacionnye materialy i tehnologii. 2014. №S6. S. 5–10.
  14. Anderson P.M., Bingert J.F., Misra A., Hirth J.P. Rolling textures in nanoscale Cu/Nb multilayers // Acta Material. V. 51. Issue 20. 2003. P. 6059–6075.
  15. Dyer T.S., Munir Z.A. The synthesis of nickel aluminides by multilayer self-propagating combustion // Metallurgical and Materials Transactions B. V. 26. Issue 3. 1995. P. 603–610.
  16. Kalidindi S.R., Smith R.W., Koczak M.J., Hussey T.S. Synthesis of nickel aluminides by vacuum plasma spraying and exothermic in-situ reactions // Materials Science and Engineering: A. V. 229. Issue 1–2. 1997. P. 137–146.