Abstract

Despite the increased interest of designers to composite polymer materials (PCM), aluminum alloys are still the basic constructional material of the aviation industry, therefore the questions of their corrosion protection, delivering special properties to their surface remain relevant. Modern ecological regulations of technological processes safety require to exclude application in toxic solutions for surface treatment such as hexavalent chromium. Technological solutions on preparation of aluminum alloys surface for pasting in the solutions which are not containing toxic compounds are provided in the work. The work is executed within the frames of the complex scientific direction 17.1. «Ecologically safe plasma electrolytic coatings for light alloys» («The strategic directions of development of materials and technologies of their processing for the period till 2030»)

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  2. Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace materials science] // Vse materialy. Enciklopedicheskij spravochnik. 2008. №3. S. 2–14.
  3. Kablov E.N. Korroziya ili zhizn [Corrosion or life] // Nauka i zhizn'. 2012. №11. S. 16–21.
  4. Sharova I.A., Petrova A.P. Obzor po materialam mezhdunarodnoj konferencii po kleyam i germetikam (WAC-2012, Franciya) [Review of world adhesive and sealant conference (WAC-2012, France] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №8. St. 06. Available at: http://www.viam-works.ru (accessed: December 14, 2015).
  5. Karimova S.A., Pavlovskaya T.G., Petrova A.P. Podgotovka alyuminievyh splavov s primeneniem anodnogo oksidirovaniya [Preparation of aluminum alloys using anodic oxidation] // Klei. Germetiki. Tehnologii. 2014. №1. S. 34–38.
  6. Karimova S.A., Kutyrev A.E., Pavlovskaya T.G., Zaharov K.E. Nizkotemperaturnoe uplotnenie anodno-oksidnyh pokrytij na detalyah iz alyuminievyh splavov [Low temperature sealing of anodic oxide coatings on parts of aluminum alloys] // Aviacionnye materialy i tehnologii. 2014. №4. S. 9–17.
  7. Shrejder A.V. Oksidirovanie alyuminiya i ego splavov [Oxidation of aluminum and its alloys]. M.: Metallurgizdat, 1960. 220 s.
  8. Fomina M.A., Karimova S.A. Issledovanie korrozionnyh svojstv listov splava V-1461-T1 primenitel'no k vseklimaticheskim usloviyam ekspluatacii aviacionnoj tehniki [Study of corrosion properties of V-1461-T1 aluminum alloy sheets in all-climatic conditions of aerotechnics operation ] // Aviacionnye materialy i tehnologii. 2014. №4. S. 18–22.
  9. Averyanov E.E. Spravochnik po anodirovaniyu [Directory on anodizing]. M.: Mashinostroenie, 1988. 132 s.
  10. Illarionov E.I., Kolobnev N.I., Gorbunov P.Z., Kablov E.N. Alyuminievye splavy v aviakosmicheskoj tehnike [Aluminum alloys in aerospace equipment]. M.: Nauka, 2001. 192 s.
  11. Kozlov I.A., Pavlovskaja T.G., Volkov I.A. Vlijanie poljarizujushhego toka na svojstva plazmennogo jelektroliticheskogo pokrytija dlja magnievyh splavov sistemy Mg–Zn–Zr [Influence of polarizing current on properties of plasma electrolytic covering for magnesium alloys of Mg–Zn–Zr system] //Aviacionnye materialy i tehnologii. 2013. №3. S. 7–12.
  12. De Mejo L.P., Rimai D.S., Sharpe L.H. Fundamentals of Adhesion and Interfaces. London: Taylor & Francis. 1999. 201 p.
  13. Skopintsev V.D. Oksidirovanie alyuminiya i ego splavov [Oxidation of aluminum and its alloys]. M.: RHTU im. D.I. Mendeleeva, 2015. 120 s.
  14. Anihovskaya L.I., Pavlovskaya T.G., Dement'eva P.A., Petrova A.P. Podgotovka poverhnosti pod skleivanie [Подготовка поверхности под склеивание] // Klei. Germetiki. Tehnologii. 2008. №7. S 32–35.
  15. Kutyrev A.E., Karimova S.A., Pavlovskaya T.G., Kuzin Ya.S. Issledovanie degradacii svojstv zashhitnyh kombinirovannyh pokrytij na alyuminievyh splavah s celyu razrabotki metodov prognozirovaniya ih srokov sluzhby [Research of properties degradation of protective combined coatings applied on aluminum alloys to develop methods of forecasting of their service life] // Aviacionnye materialy i tehnologii. 2015. №3 (36). S. 69–78. DOI: 10.18577/2071-9140-2015-0-3-69-78.
  16. Emelyanchenko A.M., Bajkovich L.B. Analiz smachivaniya kak effektivnyj metod izucheniya harakteristik pokrytij, poverhnostej i proishodyashhih na nih processah [Research of degradation of properties of the protective combined coverings on aluminum alloys for the purpose of development of methods of forecasting of their service life] // Zavodskaya laboratoriya. 2010. №9. S. 27–36.