Influence of radiation by high-current pulse electronbeams on surface layers of modern heat-resisting nickel alloys with ion-plasma coatings of different composition

Bytsenko O.A., Filonova E.V., Markov A.B., Belova N.A.
Bytsenko O.A., Filonova E.V., Markov A.B., Belova N.A. Influence of radiation by high-current pulse electronbeams on surface layers of modern heat-resisting nickel alloys with ion-plasma coatings of different composition // Proceedings of VIAM. 2016. No. 6. DOI: 10.18577/2307-6046-2016-0-6-10-10. URL: https://www.viam-works.ru/en/journal/2016/6/10
Keywords
radiation by the high-current electron beams, condensed ion-plasma coatings, structural and phase conditions, microstructure research.
Abstract

With use of complex of metallophysical methods the research of physical-chemical, structural and phase conditions of the surface layer before and after modifying is carried out by means of radiation by high-current electron beams of samples with heat-resisting condensed ion-plasma coatings of three different compositions on 5 chosen modes at variation of values of electron energy and pulse number. Work is executed within implementation of the complex scientific direction 2.1. «Fundamental-oriented researches» («The strategic directions of development of materials and technologies of their processing for the period till 2030»)

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  2. Kablov E.N. Sovremennye materialy – osnova innovacionnoj modernizacii Rossii [Modern materials – basis of innovative modernization of Russia] // Metally Evrazii. 2012. №3. S. 10–15.
  3. Kablov E.N., Ospennikova O.G., Lomberg B.S. Strategicheskie napravleniya razvitiya kon-strukcionnyh materialov i tehnologij ih pererabotki dlya aviacionnyh dvigatelej nastoyashhego i budushhego [The strategic directions of development of constructional materials and technologies of their processing for aircraft engines of the present and the future] // Avtomaticheskaya svarka. 2013. № 10. S. 23–32.
  4. Kablov E.N., Muboyadzhyan S.A. Zharostojkie i teplozashhitnye pokrytiya dlya lopatok turbiny vysokogo davleniya perspektivnyh GTD [Heat resisting and heat-protective coverings for turbine blades of high pressure of perspective GTE] //Aviacionnye materialy i tehnologii. 2012. №S. S. 60–70.
  5. Muboyadzhyan S.A., Aleksandrov D.A., Gorlov D.S., Egorova L.P., Bulavinceva E.E. Zashhitnye i uprochnyayushhie ionno-plazmennye pokrytiya dlya lopatok i drugih otvetstvennyh detalej kompressora GTD [Protective and strengthening ion-plasma coverings for blades and other responsible details of the GTE compressor] //Aviacionnye materialy i tehnologii. 2012. №S. S. 71–81.
  6. Budinovskij S.A., Smirnov A.A., Matveev P.V., Chubarov D.A. Razrabotka teplozashhitnyh pokrytij dlja rabochih i soplovyh lopatok turbiny iz zharoprochnyh i intermetallidnyh splavov [Development of thermal barrier coatings for rotor and nozzle turbine blades made of nickel-base super- and intermetallic alloys] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №4. St. 05. Available at: http://www.viam-works.ru (accessed: February 18, 2015). DOI: 10.18577/2307-6046-2015-0-4-5-5.
  7. Litye lopatki gazoturbinnyh dvigatelej: splavy, tehnologii, pokrytiya. 2-e izd. / pod obshh. red. E.N. Kablova [Cast blades of gas turbine engines: alloys, technologies, coverings. 2nd ed. / gen. ed. by E.N.Kablov]. M.: Nauka, 2006. 632 s.
  8. Shulov V.A., Engelko V.I., Gromov A.N., Teryaev D.A., Bycenko O.A. Primenenie silnotochnyh impul'snyh jelektronnyh puchkov dlya modificirovaniya poverhnosti lopatok gazoturbinnogo dvigatelya s perforacionnymi otverstiyami [Application of high-current pulse electronic bunches for modifying of surface of blades of the gas turbine engine with perforation openings] // Uprochnyayushhie tehnologii i pokrytiya. 2013. № 10 (106). S. 23–25.
  9. Pajkin A.G., L'vov A.F., Shulov V.A. i dr. Ispolzovanie silnotochnyh impulsnyh jelektronnyh puchkov dlya modifikacii svojstv lopatok GTD [Use of high-current pulse electronic bunches for updating of properties of blades of GTE] // Problemy mashinostroeniya i avtomatizacii. 2003. №3. S. 41–49.
  10. Novikov A.S., Pajkin A.G., Lvov A.F., Shulov V.A. Perspektivnye tehnologii poverhnostnoj obrabotki pri izgotovlenii i remonte lopatok GTD [Perspective technologies of surface processing during the manufacturing and repair of blades of GTE] // Dvigatel. 2004. №2 (32). S. 18–19.
  11. Pajkin A.G., Shulov V.A., Petuhov A.N., L'vov A.F. Perspektivy primeneniya silnotochnyh impul'snyh elektronnyh puchkov dlya modifikacii poverhnosti pri izgotovlenii i remonte lopatok GTD [Perspectives of application of high-current pulse electronic bunches for surface updating during the manufacturing and repair of blades of GTE] // Voprosy aviacionnoj nauki i tehniki: sb. tr. TsIAM. Ser.: Aviacionnoe dvigatelestroenie. 2006. №4 (1327). S. 5–32.
  12. Chabina E.B., Alekseev A.A., Filonova E.V., Lukina E.A. Primenenie metodov analiticheskoj mikroskopii i rentgenostrukturnogo analiza dlya issledovaniya strukturno-fazovogo sostoyaniya materialov [Application of methods of analytical microscopy and X-ray of the structural analysis for research of structural and phase condition of materials] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №5. St. 06. Available at: http://www.viam-works.ru (accessed: February 18, 2015).
  13. Pajkin A.G., Krajnikov A.V., Shulov V.A., Bytsenko O.A., Engelko V.I., Tkachenko K.I., Chikiryaka A.V. Tehnologicheskie osnovy modificirovaniya poverhnosti detalej iz zharoprochnyh nikelevyh splavov s zharostojkim NiCrAlY pokrytiem s primeneniem silnotochnyh impulsnyh jelektronnyh puchkov [Technological bases of modifying of surface of details from heat resisting nickel alloys with heat resisting NiCrAlY covering using high-current pulse electronic bunches] // Fizika i himiya obrabotki materialov. 2008. №3. S. 56–60.
  14. Shulov V.A., Pajkin A.G., Bytsenko O.A., Teryaev D.A., Engelko V.I., Tkachenko K.I. Razrabotka elektronno-luchevogo tehnologicheskogo processa vosstanovleniya svojstv lopatok turbiny GTD iz splava ZhS26NK s zharostojkim pokrytiem NiCrAlY [Development of electron beam technological process of recovery of properties of turbine blades of GTD from alloy ZhS26NK with heat resisting covering of NiCrAlY] // Uprochnyayushhie tehnologii i pokrytiya. 2010. №3. S. 34–38.
  15. Shulov V.A., Pajkin A.G., Teryaev D.A., Bycenko O.A., Engelko V.I., Tkachenko K.I. Strukturno-fazovye izmeneniya v poverhnostnyh sloyah detalej iz titanovogo splava VT6 pri obluchenii sil'notochnym impul'snym jelektronnym puchkom [Структурно-фазовые изменения в поверхностных слоях деталей из титанового сплава ВТ6 при облучении сильноточным импульсным электронным пучком] // Fizika i himiya obrabotki materialov. 2012. № 3. S. 5–9.