Usage of aromatic amine curing agents for epoxy resins binders for production of structural PCM

Chursova L.V., Babin A.N., Panina N.N., Tkachuk A.I., Terekhov I.V.
Chursova L.V., Babin A.N., Panina N.N., Tkachuk A.I., Terekhov I.V. Usage of aromatic amine curing agents for epoxy resins binders for production of structural PCM // Proceedings of VIAM. 2016. No. 6. DOI: 10.18577/2307-6046-2016-0-6-4-4. URL: https://www.viam-works.ru/en/journal/2016/6/4
Keywords
aromatic amines, epoxy resins, composite materials, heat resistance, binders.
Abstract

Technological and mechanical properties of epoxy binders suitable for producing structural composite materials based on such aromatic curing agents as 4,4'-methylene-bis-(2,6-diisopropylaniline), 4,4'-methylene-bis-(2-isopropyl-6-methylaniline), bis-(4-amino-2-chloro-3,5-diethylphenyl) methane and 4,4'-diaminodiphenylsulfone are studied. Particle size distribution of the samples of 4,4' diaminodiphenylsulfone curing agent and its impact on the process of dissolution in epoxy resins are studied as well. Work is executed within implementation of the complex scientific directions 13.1. «Binding for polymeric and composite materials of structural and special purposes », 13.2. «Structural PСM» («The strategic directions of development of materials and technologies of their processing for the period till 2030»)

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  2. Kablov E.N. Himiya v aviacionnom materialovedenii [Chemistry in aviation materials science] // Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 3–4.
  3. Grashhenkov D.V., Chursova L.V. Strategiya razvitiya kompozicionnyh i funkcionalnyh materialov [Strategy of development of composite and functional materials] // Aviacionnye materialy i tehnologii. 2012. №S. S. 231–242.
  4. Chursova L.V., Dushin M.I., Kogan D.I., Panina N.N., Kim M.A., Gurevich Ya.M., Platonov A.A. Plenochnye svyazuyushhie dlya RFI-tehnologii [Film binding for RFI technology] // Rossijskij himicheskij zhurnal. 2010. T. LΙV. №1. S. 63–66.
  5. Panina N.N., Kim M.A., Gurevich Ya.M., Grigor'ev M.M., Chursova L.V., Babin A.N. Svyazuyushhie dlya bezavtoklavnogo formovaniya izdelij iz polimernyh kompozicionnyh materialov [Binding for autoclave-free formation of products from polymeric composite materials] // Klei. Germetiki. Tehnologii. 2013. №10. S. 18–27.
  6. Grigorev M.M., Hrulkov A.V., Gurevich Ya.M., Panina N.N. Izgotovlenie stekloplastikovyh obshivok metodom vakuumnoj infuzii s ispolzovaniem epoksiangidridnogo svyazuyushhego i polupronicaemoj membrany [Manufacture of fiberglass skins using vacuum infusion using epoksiangidrid resin and a semipermeable membrane] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №2. St. 04. Available at: http://viam-works.ru (accessed: November 30, 2015). DOI: 10.18577/2307-6046-2014-0-2-4-4.
  7. Grigorev M.M., Kogan D.I., Tverdaya O.N., Panina N.N. Osobennosti izgotovleniya PKM metodom RFI [Features of manufacturing of PCM RFI method] // Trudy VIAM: electron. nauch.-tehnich. zhurn. 2013. №4. St. 03. Available at: http://www.viam-works.ru (accessed: November 30, 2015).
  8. Lapitskaya T.V., Lapickij V.A. Epoksidnye materialy [Epoxy materials] // Kompozitnyj mir. 2006. №7. S. 16–17.
  9. Hozin V.G. Usilenie epoksidnyh polimerov [Strengthening of epoxy polymers]. Kazan: PIK «Dom pechati», 2004. S. 446.
  10. Kuznetsova V.A., Deev I.S., Kondrashov E.K., Kuznetsov G.V. Vliyanie otverditelej na mikrostrukturu i svojstva modificirovannogo jepoksidnogo svyazuyushhego dlya toplivostojkogo pokrytiya [Influence of hardeners on microstructure and property modified epoxy binding for toplivostoyky covering] // Vse materialy. Enciklopedicheskij spravochnik. 2012. №11. S. 38–41.
  11. Kozlova A.A., Kondrashov Je.K., Deev I.S., Shchegoleva N.E. Issledovanie vliyaniya frakcionnogo sostava i udelnoj poverhnosti antikorrozionnyh pigmentov na zashhitnye svojstva epoksidnyh pokrytij [Research of influence of fractional structure and specific surface of anticorrosive pigments on protective properties of epoxy coverings] // Korroziya: materialy, zashhita. 2013. №3. S. 42–48.
  12. Available at: http://www.lonza.com (accessed: November 30, 2015).
  13. Available at: http://www.huntsman.com (accessed: November 30, 2015).
  14. Available at: http://www.chemsystem.ru (accessed: November 30, 2015).
  15. Tkachuk A.I., Chursova L.V., Kim M.A., Gurevich Ya.M., Panina N.N., Babin A.N. Diaminodifenilsulfon: poluchenie, primenenie, perspektivy [Diaminodiphenylsulphone: receiving, application, perspectives] // Vse materialy. Eniklopedicheskij spravochnik. 2013. №10. S. 30–42.
  16. Available at: http://www.high-performance-materials.com (accessed: November 30, 2015).
  17. 17. Low moisture absorption epoxy resin systems with alkylated diamine hardeners: pat. 6379799 US; publ. 30.04.02.
  18. Epoksidnoe svyazuyushhee, prepreg na ego osnove i izdelie, vypolnennoe iz preprega: pat. 2184128 Ros. Federaciya [Epoxy binding, prepreg on its basis and the product executed from prepreg: pat 2184128 Rus. Federation]; opubl. 27.06.02.
  19. Vysokoprochnaya epoksidnaya kompoziciya i sposob ee polucheniya: pat. 2363712 Ros. Federaciya [High-strength epoxy composition and way of its receiving: pat. 2363712 Rus. Federation]; opubl.10.08.09.
  20. Epoksidnoe svyazuyushhee, prepreg na ego osnove i izdelie, vypolnennoe iz preprega: pat. 2424259 Ros. Federaciya [Epoxy binding, prepreg on its basis and the product executed from prepreg: pat. 2424259 Rus. Federation]; opubl. 20.07.11.
  21. Epoksidnoe svyazuyushhee, prepreg na ego osnove i izdelie, vypolnennoe iz preprega: pat. 2513916 Ros. Federaciya [Epoxy binding, prepreg on its basis and the product executed from prepreg: pat. 2513916 Rus. Federation]; opubl. 20.04.14.
  22. Epoksidnoe svyazuyushhee, prepreg na ego osnove i izdelie, vypolnennoe iz preprega: pat. 2520543 Ros. Federaciya [Epoxy binding, prepreg on its basis and the product executed from prepreg: pat. 2520543 Rus. Federation]; opubl. 27.06.14.
  23. Hrulkov A.V., Dushin M.I., Popov Yu.O., Kogan D.I. Issledovaniya i razrabotka avtoklavnyh i bezavtoklavnyh tehnologij formovaniya PKM [Researches and development autoclave and out-of-autoclave technologies of formation of PCM] //Aviacionnye materialy i tehnologii. 2012. №S. S. 292–301.
  24. Dushin M.I., Hrulkov A.V., Muhametov R.R. Vybor tehnologicheskih parametrov avtoklavnogo formovaniya detalej iz polimernyh kompozicionnyh materialov [A choice of technological parameters of autoclave formation of details from polymeric composite materials] // Aviacionnye materialy i tehnologii. 2011. №3. S. 20–26.
  25. 25 Muhametov R.R., Ahmadieva K.R., Chursova L.V., Kogan D.I. Novye polimernye svyazujushhie dlya perspektivnyh metodov izgotovleniya konstrukcionnyh voloknistyh PKM [New polymeric binding for perspective methods of manufacturing of constructional fibrous PCM] //Aviacionnye materialy i tehnologii. 2011. №2. S. 38–42.
  26. Kablov E.N., Kondrashov S.V., Yurkov G.Yu. Perspektivy ispolzovaniya uglerodsoderzhashhih nanochastic v svyazuyushhih dlya polimernyh kompozicionnyh materialov [Perspectives of use of carbon-containing nanoparticles in binding for polymeric composite materials] // Rossijskie nanotehnologii. 2013. T. 8. №3–4. S. 28–46.
  27. Gunyaev G.M., Kablov E.N., Aleksashin V.M. Modificirovanie uglerodnyh stekloplastikov uglerodnymi nanochasticami [Modifying of carbon fibreglasses by carbon nanoparticles] // Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 5–11.
  28. Kobets L.P., Deev I.S. Strukturoobrazovanie v termoreaktivnyh svyazuyushhih i matricah kompozicionnyh materialov na ih osnove [Structurization in thermosetting binding and matrixes of composite materials on their basis] // Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 67–78.
  29. Muhametov R.R., Ahmadieva K.R., Kim M.A., Babin A.N. Rasplavnye svyazujushhie dlya perspektivnyh metodov izgotovleniya PKM novogo pokoleniya [Melt binding for perspective methods of production of PCM of new generation] // Aviacionnye materialy i tehnologii. 2012. №S. S. 260–265.
  30. Deev I.S., Kablov E.N., Kobets L.P., Chursova L.V. Issledovanie metodom skaniruyushhej elektronnoj mikroskopii deformacii mikrofazovoj struktury polimernyh matric pri mehanicheskom nagruzhenii [Research of the scanning electron microscopy method deformation of microphase structure of polymeric matrix at mechanical loading] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №7. St. 06. Available at: http://www.viam-works.ru (accessed: November 30, 2015). DOI: 10.18577/2307-6046-2014-0-7-6-6.
  31. Vinogradov G.V., Malkin A.Ya. Reologiya polimerov [Rheology of polymers]. M.: Himiya, 1977. 440 s.
  32. Malkin A.Ya., Kulichihin S.G. Reologiya v processah obrazovaniya i prevrashheniya polimerov [Rheology in processes of education and transformation of polymers]. M.: Himiya, 1985. 240 s.
  33. Simonov-Emelyanov I.D., Trofimov A.N., Surikov P.V., Shheulova L.K. Osobennosti reokinetiki processa otverzhdeniya dianovyh epoksidnyh oligomerov promyshlennyh marok aminnym otverditelem [Features reokinetiki process of curing of dianovy epoxy oligomers of industrial brands by amine hardener] // Vestnik MITHT. 2010. T. 5. №3. S. 102–107.
  34. Strong A.B. Fundamentals of Composites Manufacturing: Materials, Methods and Applications. Dearborn: SME, 2008. 620 p.
  35. Moshinskij L. Epoksidnye smoly i otverditeli [Epoxies and hardeners]. Tel-Aviv: Arkadiya press Ltd, 1995. S. 370.
  36. Deev I.S., Sokolov I.I., Panina N.N. et al. Properties and Structural Features of Nanodisperse Powder Fillers // Polymer Science. Series D. Glues and Sealing Materials. 2013. V. 6. №3. P. 217–222.