Hydrophobic structures for additional protection of carbon steel in fuel systems of aviation engineering

Kravchenko N.G., Petrova V.A., Mikov D.A.
Kravchenko N.G., Petrova V.A., Mikov D.A. Hydrophobic structures for additional protection of carbon steel in fuel systems of aviation engineering // Proceedings of VIAM. 2016. No. 5. DOI: 10.18577/2307-6046-2016-0-5-9-9. URL: https://www.viam-works.ru/en/journal/2016/5/9
Abstract

In this work functional polymer coatings which can be used as hydrophobic processing for increase of protective properties of carbon steel working in fuels at influence of condensate are investigated. Data on resistance of functional polymer coatings on carbon steels in the salt spray chamber (SSC) and aviation fuel TS-1 are obtained. Method of measurement of interfacial angle (IFA) by water was used as an express method of estimation of hydrophobic behavior of the surface. The most effective hydrophobic agents for receiving polymer coatings are functional fluorinated oligomers. On the basis of the researches structures of functional polymer coatings which can be used in fuel systems of aircraft for additional protection of carbon steel have been chosen. Work is executed within implementation of the complex scientific direction 2.2. «Qualification and researches of materials» («The strategic directions of development of materials and technologies of their processing for the period

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  2. Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace materials science] // Vse materialy. Enciklopedicheskij spravochnik. 2008. №3. C. 2–14.
  3. Kablov E.N., Startsev O.V., Medvedev I.M. Obzor zarubezhnogo opyta issledovanij korrozii i sredstv zashhity ot korrozii [Review of international experience on corrosion and corrosion protection] // Aviacionnye materialy i tehnologii. 2015. №2 (35). S. 76–87.
  4. Kablov E.N. Korroziya ili zhizn [Corrosion or life] // Nauka i zhizn. 2012. №11. S. 16–21.
  5. Mikov D.A., Kutyrev A.E., Petrova V.A. Gidrofobiziruyushhie sostavy dlya dopolnitelnoj zashhity alyuminievyh splavov v toplivnyh sistemah izdelij aviatehniki [Hydrophobic compositions for additional protection of aluminum alloys in fuel systems of aviation equipment] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №10. St. 08. Available at: http://www.viam-works.ru (accessed: October 11, 2015). DOI: 10.18577/2307-6046-2015-0-9-8-8.
  6. Kablov E.N., Starcev O.V., Medvedev I.M., Panin S.V. Korrozionnaya agressivnost primorskoj atmosfery. Ch. 1. Faktory vliyaniya (obzor) [Corrosion aggression of the seaside atmosphere. P.1. Factors of influence (review)] // Korroziya: materialy, zashhita. 2013. №12. S. 06–18.
  7. Salahova R.K. Korrozionnaja stojkost stali 30HGSA s «trehvalentnym» hromovym pokrytiem v estestvennyh i iskusstvennyh sredah [Corrosion resistance of steel 30ХГСА with «trivalent» chrome plating in natural and artificial environments] // Aviacionnye materialy i tehnologii. 2012. №2. S. 59–66.
  8. Emelyanenko A.M., Bojnovich L.B. Analiz smachivaniya, kak jeffektivnyj metod izucheniya harakteristik pokrytij, poverhnostej i proishodyashhih na nih processov [The wetting analysis, as effective method of studying of characteristics of coverings, surfaces and processes occurring on them] // Zavodskaya laboratoriya. 2010. №9. S. 27–36.
  9. Sostav dlya polucheniya supergidrofobnogo pokrytiya: pat. 2400510 Ros. Federaciya [Structure for receiving superhydrophobic coating: pat. 2400510 Rus. Federation]; opubl. 27.09.10. Byul. №27.
  10. Gnedenkov S.V., Egorkin V.S., Sinebryuhov S.L., Vyalyj I.E., Pashinin A.S., Emelyanenko A.M., Bojnovich L.B. [Superhydrophobic composition coatings on surface of magnesium alloy] Supergidrofobnye kompozicionnye pokrytiya na poverhnosti magnievogo splava // Vestnik DVO RAN. 2013. №5. S. 3–11.
  11. Zhilikov V.P., Karimova S.A., Leshko S.S., Chesnokov D.V. Issledovanie dinamiki korrozii alyuminievyh splavov pri ispytanii v kamere solevogo tumana (KST) [Research of dynamics of corrosion of aluminum alloys when testing in the salt spray chamber (SSC)] // Aviacionnye materialy i tehnologii. 2012. №4. S. 18–22.
  12. Karimova S.A., Kutyrev A.E., Fomina M.A., Chesnokov D.V. Modelirovanie processa vozdejstviya agressivnyh komponentov promyshlennoj atmosfery na metallicheskie materialy v kamere solevogo tumana [Modeling of process of influence of aggressive components of the industrial atmosphere on metal materials in the salt spray chamber] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S.86–94.
  13. Shkolnikova V.M. Topliva. Smazochnye materialy. Tehnicheskie zhidkosti. Assortiment i primenenie [Lubricants. Technical liquids. Range and application]. M.: Izdatelsлшн centr «Tehinform», 1999. S. 62–75.
  14. Mikov D.A., Kravchenko N.G., Petrova V.A., Kutyrev A.E. Opredelenie soderzhaniya medi v aviacionnyh toplivah metodom atomno-absorbcionnoj spektrometrii [Quantitative analysis of copper in aviation fuel by atomic absorption spectrometry] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №10. St. 12. Available at: http://www.viam-works.ru (accessed: October 11, 2015). DOI: 10.18577/2307-6046-2015-0-10-12-12.
  15. Privalenko A.N., Balak G.M., Bagramova E.K. Opredelenie soderzhaniya metallov v neftyanyh toplivah metodom atomno-absorbcionnoj spektrometrii [Definition of the content of metals in oil fuels method of nuclear and absorbing spectrometry] // Tez. dokl. Mezhdunar. nauch.-tehnich. konf. M.: 25 GOSNII Himmotologii, 2014. C. 298–306.
  16. Mansfild F. Use of electrochemical impedance spectroscopy for the study of corrosion protection by polymer coating // Journal of Applied Electrochemistry. 1995. V. 25. P. 187–202.