New pressure electroslag remelting furnace PESR-0,1: development and prospects for improvement

Krylov S.А., Evgenov A.G., Shcherbakov A.I., Makarov А.А.
Krylov S.А., Evgenov A.G., Shcherbakov A.I., Makarov А.А. New pressure electroslag remelting furnace PESR-0,1: development and prospects for improvement // Proceedings of VIAM. 2016. No. 5. DOI: 10.18577/2307-6046-2016-0-5-4-4. URL: https://www.viam-works.ru/en/journal/2016/5/4
Abstract

Pressure metallurgy (MD) is actively developed in the world, the effect of higher pressure on the process of alloying, melting, crystallization of ingot is studied. A positive economic effect of MD technologies is noted. MD technologies open possibilities of creating new materials and alloying elements, the use of which in conventional metallurgical processes is impossible. FSUE «VIAM» for the first time in the history of our country produced and put into operation a new pressure electroslag furnace PESR-0,1 of semiindustrial type. The paper presents design data of the furnace, the basic ways of its practical use and materials received with its use. Work is executed within implementation of the complex scientific direction 8.2. «High-strength structural and corrosion-resistant welded steels with high fracture toughness» («The strategic directions of development of materials and technologies of their processing for the period till 2030»)

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  2. Kablov E.N., Lomberg B.S., Ospennikova O.G. Sozdanie sovremennyh zharoprochnyh materialov i tehnologij ih proizvodstva dlya aviacionnogo dvigatelestroeniya [Creation of modern heat resisting materials and technologies of their production for aviation engine building] //Krylya Rodiny. 2012. №3–4. S. 34–38.
  3. Kablov E.N. Sovremennye materialy – osnova innovacionnoj modernizacii Rossii [Modern materials – basis of innovative modernization of Russia] // Metally Evrazii. 2012. №3. S. 10–15.
  4. Kablov E.N., Ospennikova O.G., Lomberg B.S., Sidorov V.V. Prioritetnye napravleniya razvitiya tehnologij proizvodstva zharoprochnyh materialov dlya aviacionnogo dvigatelestroeniya [The priority directions of development of production technologies of heat resisting materials for aviation engine building] // Problemy chernoj metallurgii i materialovedeniya. 2013. №3. S. 47–54.
  5. High Nitrogen steel, HNS 90. Dusseldorf: Stahl und Eisen. 1990.
  6. Poschitz I.N., Kolesov V.A. Use of High-Nitrogen non-magnetic steel for production of steel-aluminum conductor // 5th Int. Conf. High Nitrogen Steels. Espoo – Finland. 1998. Р. 19.
  7. Berns H. Alloy development and processing // Int. Conf. High Nitrogen Steels HNS-2004. 2004. P. 271–281.
  8. Rashev C.V. Vysokoazotistye stali. Metallurgiya pod davleniem [High-nitrogen steels. Metallurgy under pressure]. Sofiya: Izd-vo «Prof. Marin Drinov». 1995. 272 s.
  9. Tonysheva O.A., Voznesenskaya I.M., Eliseev E.A., Shalkevich A.B. Novaya vysokoprochnaya ekonomnolegirovannaya azotsoderzhashchaya stal povyshennoj nadezhnosti [The new high-strength containing steel of increased reliability economically alloyed nitrogen] //Aviacionnye materialy i tehnologii. 2012. №S. S. 84–88.
  10. Tonysheva O.A., Voznesenskaya N.M. Perspektivnye vysokoprochnye korrozionnostojkie stali, legirovannye azotom (sravnitelnyj analiz) [Perspective high-strength corrosion-resistant steels alloyed with nitrogen (comparative analysis] // Aviacionnye materialy i tehnologii. 2014. №3. S. 27–32.
  11. Tonysheva O.A., Voznesenskaja N.M., Shalkevich A.B., Petrakov A.F. Issledovanie vlijanija vysokotemperaturnoj termomehanicheskoj obrabotki na strukturu, tehnologicheskie, mehanicheskie i korrozionnye svojstva vysokoprochnoj korrozionnostojkoj stali pere-hodnogo klassa s povyshennym soderzhaniem azota [Research of influence of high-temperature thermomechanical processing on structure, technological, mechanical and corrosion properties of high-strength corrosion-resistant steel of transitional class with the raised content of nitrogen] // Aviacionnye materialy i tehnologii. 2012. №3. S. 31–36.
  12. Blinov M.V., Bannyh O.A., Lukin E.I., Kostina M.V., Blinov E.V. Vliyanie termicheskoj obrabotki i plasticheskoj deformacii na strukturu i mehanicheskie svojstva azotosoderzhashhej stali 04N9H2A [Influence of thermal processing and plastic strain on structure and mechanical properties of nitrogen-bearing steel 04N9H2A] // Metally. 2014. №6. S. 21–28.
  13. Bratuhin A.G., Demchenko O.F., Dolzhenkov N.N., Krivonogov G.S. Vysokoprochnye korrozionnostojkie stali sovremennoj aviacii [High-strength corrosion-resistant became modern aircraft]. M.: MAI, 2006. S. 112–121, 130–143.
  14. Krivonogov G.S., Kablov E.N. Granicy zeren i ih rol v ohrupchivanii vysokoprochnyh korrozionnostojkih stalej [Borders of grains and their role in okhrupchivaniye high-strength corrosion-resistant the staly] // Metally. 2002. №1. S. 35–45.
  15. Blinov V.M., Andreev Ch., Kostina M.V., Blinov E.V. Struktura i fazovyj sostav lityh zhelezonikelevyh splavov so sverhravnovesnym soderzhaniem azota [Structure and phase composition of cast nickel iron alloys with the superequilibrium content of nitrogen] // Metally. 2009. №4. S. 57–62.