Development of binding, not sustaining combustion of CFRP, for manufacturing of thick-walled products from polymeric composite materials by method of press formation
Pavlovsky K.A., Yamshchikova G.A., Gunyaeva A.G., Ulkin M.Yu. Development of binding, not sustaining combustion of CFRP, for manufacturing of thick-walled products from polymeric composite materials by method of press formation // Proceedings of VIAM. 2016. No. 4. DOI: 10.18577/2307-6046-2016-0-4-8-8. URL: https://www.viam-works.ru/en/journal/2016/4/8
Abstract
The overview on application of different substances for decrease in combustibility of polymeric materials is provided. Results of researches on development of binding, not sustaining combustion of CFRP are provided. Results of researches on development and optimization of manufacture modes of CFRP samples of different thickness are provided. Researches of electrophysical, thermo - and physicomechanical characteristics of samples of CFRP are conducted. Work is executed within implementation of the complex scientific direction 13.1. «Binding for polymeric and composite materials of structural and special purpose» («The strategic directions of development of materials and technologies of their processing for the period till 2030»)
Reference list
- Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
- Gunyaev G.M., Kablov E.N. Konstrukcionnye ugleplastiki na rubezhe vekov [Constructional plastics coal at turn of centuries] / V kn. Aviacionnye materialy. Izbrannye trudy «VIAM» 1932–2002: yubilejnyj nauch.-tehnich. sb. M.: MISIS–VIAM, 2002. S. 242–247.
- Kablov E.N. Rossii nuzhny materialy novogo pokoleniya [Materials of new generation are necessary to Russia] // Redkie zemli. 2014. №3. S. 8–13.
- Plyudeman E. Poverhnosti razdela v polimernyh kompozitah [Interfaces in polymeric composites]. M.: Mir. Kompozicionnye materialy, 1978. T. 6. 296 s.
- Bobylev V.A. Otverditeli jepoksidnyh smol [Hardeners of epoxies] // Kompozitnyj mir. 2006. №4. S. 20–24.
- Gunyaev G.M., Kablov E.N., Aleksashin V.M. Modificirovanie konstrukcionnyh ugleplastikov uglerodnymi nanochasticami [Modifying constructional coal of plastics carbon nanoparticles] // Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 5–11.
- Barbotko S.L. Pozharobezopasnost aviacionnyh materialov [Fire safety of aviation materials] // Aviacionnye materialy i tehnologii. 2012. №S. S. 431–439.
- Kopylov V.V., Novikov S.N. Polimernye materialy ponizhennoj goryuchesti [Polymeric materials of the lowered combustibility]. M.: Himiya, 1986. 224 s.
- Kodolov V.I. Goryuchest i ognestojkost polimernyh materialov [Combustibility and fire resistance of polymeric materials]. M.: Himiya, 1976. 160 s.
- Mihajlin Yu.A. Teplo-, termo- i ognestojkost polimernyh materialov [Warm, thermo- and fire resistance of polymeric materials]. SPb.: NOT, 2011. 416 s.
- Sposob polucheniya ognestojkogo svyazuyushhego dlya sozdavaemyh v pultruzionnom tehnologicheskom processe kompozicionnyh materialov, ognestojkoe svyazuyushhee i izdelie: pat. 2420542 Ros. Federaciya [Way of receiving fire-resistant binding for composite materials created in pultruzics technological process, fire-resistant binding and product: pat. 2420542 Rus. Federation]; opubl. 10.11.10.
- Kodolov V.I. Zamedliteli goreniya polimernyh materialov [Decelerators of burning of polymeric materials]. M.: Himiya, 1980. 274 s.
- Zheleznyak V.G., Chursova L.V. Modifikaciya svyazujushhih i matric na ih osnove s celyu povysheniya vyazkosti razrusheniya [Modification of binders and matrixes based on them to increase fracture toughness] // Aviacionnye materialy i tehnologii. 2014. №1. S. 47–50.
- Fedoseev M.S., Devyaterikov D.M., Sheludyakov V.D. Sintez i svojstva polimerov, poluchennyh pri otverzhdenii epoksidnyh oligomerov razlichnoj funkcionalnosti metilendikovym angidridom [Synthesis and properties of the polymers received at curing of epoxy oligomers of different functionality marked endikov anhydride] // Himicheskaya tehnologiya. 2013. T. 14. №12. S. 739–744.
- Muhametov R.R., Ahmadieva K.R., Chursova L.V., Kogan D.I. Novye polimernye svyazujushhie dlya perspektivnyh metodov izgotovleniya konstrukcionnyh voloknistyh PKM [New polymeric binding for perspective methods of manufacturing of constructional fibrous PCM] //Aviacionnye materialy i tehnologii. 2011. №2. S. 38–42.
- Moshinskij L.M. Epoksidnye smoly i otverditeli [Epoxies and hardeners]. Tel-Aviv: Arkadiya press LTD, 1995. 370 s.
- Aleksashin V.M., Antyufeeva N.V. Razvitie metodov termicheskogo analiza v issledovaniyah polimernyh kompozicionnyh materialov [Development of methods of the thermal analysis in researches of polymeric composite materials] / V kn. 75 let. Aviacionnye materialy. Izbrannye trudy «VIAM» 1932–2007: yubilejnyj nauch.-tehnich. sb. M.: VIAM, 2007. S. 245–249.
- Dushin M.I., Hrulkov A.V., Raskutin A.E. K voprosu udaleniya izlishkov svyazuyushchego pri avtpklavnim formovanii izdeliy iz polimernyh kompozitsionnyh materialov [To question of removal of excesses binding at avtoklavny formation of products from polymeric composite materials] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №1. St. 03. Available at: http://viam-works.ru (accessed: September 03, 2015).
- Chursova L.V., Kim M.A., Panina N.N., Shvetsov E.P. Nanomodificirovannoe epoksidnoe svyazuyushhee dlya stroitelnoj industrii [Nanomodified epoxy binder for the construction industry] // Aviacionnye materialy i tehnologii. 2013. №1. S. 40–47.
- Alyamovskij A.A. Inzhenernye raschety v SolidWorks Simulation [Engineering calculations in SolidWorks Simulation]. M.: DKM-press, 2013. 464 s.
- Birger I.A., Iosilevich G.B. Rezbovye i flancevye soedineniya [Threaded and flanged couplings]. M.: Mashinostroenie, 1990. 368 s.
- Paharenko V.A., Paharenko V.V., Yakovleva R.A. Plastmassy v stroitelstve [Plastic in construction]. SPb.: Nauchnye osnovy i tehnologii, 2010. 350 s.