The research of operational and climatic factors influence on flammability of textile materials used in aviation
Barbotko S.L., Nesterova T.A., Kirienko O.A., Volnyj O.S. The research of operational and climatic factors influence on flammability of textile materials used in aviation // Proceedings of VIAM. 2016. No. 3. DOI: 10.18577/2307-6046-2016-0-3-12-12. URL: https://www.viam-works.ru/en/journal/2016/3/12
Abstract
Researches on impact assessment of some external influencing operational and climatic factors on combustibility characteristics for several types of textile materials are conducted. Influence of thermal-humidity factors on change of registered characteristics of fire safety is shown.
Reference list
- Kablov E.N. Materialy i himicheskie tehnologii dlya aviacionnoj tehniki [Materials and chemical technologies for aviation engineering] // Vestnik Rossijskoj akademii nauk. 2012. T. 82. №6. S. 520–530.
- Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace materials science] // Vse materialy. Jenciklopedicheskij spravochnik. 2008. №3. S. 2–14.
- Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
- Kirillov V.N., Startsev O.V., Efimov V.A. Klimaticheskaya stojkost i povrezhdaemost polimernyh kompozicionnyh materialov, problemy i puti resheniya [Climatic firmness and damageability of polymeric composite materials, problems and solutions] // Aviacionnye materialy i tehnologii. 2012. №S. S. 412–423.
- Barbotko S.L. Ways of providing fire safety of aviation materials // Russian Journal of General Chemistry. 2011. V. 81. №5. P. 1068–1074.
- Barbotko S.L., Kirillov V.N., Shurkova E.N. Ocenka pozharnoj bezopasnosti polimernyh kompozicionnyh materialov aviacionnogo naznacheniya [Assessment of fire safety of polymeric composite materials of aviation assignment] // Aviacionnaya promyshlennost. 2013. №2. S. 55–58.
- Barbotko S.L. Pozharobezopasnost aviacionnyh materialov [Fire safety of aviation materials] // Aviacionnye materialy i tehnologii. 2012. №S. S. 431–439.
- Barbotko S.L., Kirillov V.N., Shurkova E.N. Ocenka pozharnoj bezopasnosti polimernyh kompozicionnyh materialov aviacionnogo naznacheniya [Assessment of fire safety of polymeric composite materials of aviation assignment] // Aviacionnye materialy i tehnologii. 2012. №3. S. 56–63.
- Aviacionnye pravila. Chast 25. Normy letnoj godnosti samoletov transportnoj kategorii; 3-e izd.: utv. Postanovleniem 28-j sessii Soveta po aviacii i ispolzovaniyu vozdushnogo prostranstva 11.12.2008 [Aviation rules. Part 25. Standards of the flight validity of airplanes of transport category; 3rd ed.: are approved by the Resolution of the 28th session of Council for aircraft and use of air space November 12, 2008]. M.: OAO «Aviaizdat», 2009. 274 s.
- Barbotko S.L., Shurkova E.N., Volny O.S., Skrylyov N.S. Ocenka pozharnoj bezopasnosti polimernyh kompozicionnyh materialov dlya vneshnego kontura aviacionnoj tehniki [Evolution of polymer composite fire-safety for the outer contour of aeronautical engineering] // Aviacionnye materialy i tehnologii. 2013. №1. S. 56–59.
- Skryljov N.S., Volnyj O.S., Postnov V.I., Barbotko S.L. Issledovanie vliyaniya teplovyh faktorov klimata na izmenenie harakteristik pozharobezopasnosti polimernyh kompozicionnyh materialov [Research of influence of environment’s thermal factors on fire safety characteristics drift of polymeric composite materials] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2013. №9. St. 05. Available at: http://www.viam-works.ru (accessed: July 15, 2015).
- Pickett B.M., Dierdorf D.S., Wells S.P. Firefighting and emergency response study of advanced composites aircraft. Objective 2: Firefighting Effectiveness of Technologies and Agents on Composite Aircraft Fires // Air force research laboratory materials and manufacturing directorate AFRL-RX-TY-TR-2011-0047. 2012. 36 p.
- N.S. Skrylyov, O.S. Volnyj, D.V. Abramov, E.N. Shurkova Issledovanie vliyaniya teplovlazhnostnyh faktorov na izmenenie harakteristik pozharnoj bezopasnosti PKM, podverzhennyh klimaticheskim vozdejstviyam [Research the influence of temperature and humidity factors on change of fire safety characteristics for polymeric composite materials which are subject to climatic aging] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №7. St. 12. Available at: http://www.viam-works.ru (accessed: July 15, 2015). DOI: 10.18577/2307-6046-2014-0-7-12-12.
- Barbotko S.L., Volnyj O.S., Kirienko O.A., Lutsenko A.N., Shurkova E.N. Sopostavlenie metodov ocenki pozharnoj opasnosti polimernyh materialov v razlichnyh otraslyah transporta i promyshlennosti [Comparison of methods of assessment of fire danger of polymeric materials in the different industries of transport and the industry] // Vse materialy. Enciklopedicheskij spravochnik. 2015. №1. S. 2–9.
- Barbotko S.L. Trebovaniya aviacionnyh norm i metody ocenki pozharnoj bezopasnosti aviacionnyh materialov: istoriya, sovremennoe sostoyanie i perspektivy razvitiya [Requirements of aviation norms and methods of assessment of fire safety of aviation materials: history, current state and development perspectives] // Vestnik Voronezhskogo instituta GPS MChS Rossii. 2014. №3. S. 23–33.
- Barbotko S.L. Pozharnaya opasnost, metody ocenki i trebovaniya k materialam dlya izgotovleniya vneshnego kontura aviacionnoj tehniki [Fire danger, assessment and requirement methods to materials for manufacturing of external circuit of aviation engineering] // Vestnik Voronezhskogo instituta GPS MChS Rossii. 2014. №4. S. 6–15.