Development of methods for determining small amounts of cerium in alloys of Co–Cr–W–Ta–Ti–Ce

Titov V.I., Goundobin N.V., Pilipenko L.V.
Titov V.I., Goundobin N.V., Pilipenko L.V. Development of methods for determining small amounts of cerium in alloys of Co–Cr–W–Ta–Ti–Ce // Proceedings of VIAM. 2016. No. 3. DOI: 10.18577/2307-6046-2016-0-3-9-9. URL: https://www.viam-works.ru/en/journal/2016/3/9
Abstract

Cobalt-based alloys can be applied as superalloys together with nickel ones for parts operating at high temperatures. Rare earth elements (REM) have positive impact on long-term strength, ductility, viscosity, deformation of the alloy at high temperatures , and reduce the harmful effects of fusible (S, Pb, Sn, Bi), connecting them in refractory compounds. The positive effect of rare-earth elements on the alloys properties is exercises in a fairly narrow range of concentrations. Therefore, to obtain improved material properties it is necessary to strictly control the REM content in the alloys. As a result of this work the technique of determination of cerium in Co–Cr–W–Ta–Ti–Ce alloys in the concentrations range 0,002–0,02 wt. % using a reagent redoksan Ι is de-veloped.

Reference list
  1. Kablov E.N., Petrushin N.V., Svetlov I.L., Demonis I.M. Litejnye zharoprochnye nikelevye splavy dlya perspektivnyh aviacionnyh GTD [Cast heat resisting nickel alloys for perspective aviation GTE] // Tehnologiya legkih splavov. 2007. №2. S. 6–16.
  2. Kablov E.N., Sidorov V.V., Kablov D.E., Rigin V.E., Goryunov A.V. Sovremennye tehnologii polucheniya prutkovyh zagotovok iz litejnyh zharoprochnyh splavov novogo pokoleniya [Modern technologies of receiving the bar stock preparations from foundry heat resisting alloys of new generation] // Aviacionnye materialy i tehnologii. 2012. №S. S. 97–105.
  3. Shmotin Yu.N., Starkov R.Yu., Danilov D.V., Ospennikova O.G., Lomberg B.S. Novye materialy dlya perspektivnogo dvigatelya OAO «NPO „Saturn”» [New materials for the perspective engine of JSC «NPO „Saturn”»] // Aviacionnye materialy i tehnologii. 2012. №2. S. 6–8.
  4. Kablov E.N., Ospennikova O.G., Bazyleva O.A. Materialy dlya vysokoteplonagruzhennyh detalej gazoturbinnyh dvigatelej [Materials for the high-heatloaded details of gas turbine engines] // Vestnik MGTU im. N.E. Baumana. Ser. «Mashinostroenie». 2011. №SP4. C. 13–19.
  5. Kablov E.N., Bondarenko Yu.A., Echin A.B., Surova V.A. Razvitie processa napravlennoj kristallizacii lopatok GTD iz zharoprochnyh splavov s monokristallicheskoj i kompozicionnoj strukturoj [Development of process of the directed crystallization of blades of GTE from hot strength alloys with single-crystal and composition structure] // Aviacionnye materialy i tehnologii. 2012. №1. S. 3–8.
  6. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  7. Sidorov V.V., Timofeeva O.B., Kalitsev V.A., Goryunov A.V. Vliyanie mikrolegirovanija RZM na svojstva i strukturno-fazovye prevrashheniya v intermetallidnom splave VKNA-25-VI [Influence of microalloying of RZM on properties and structural phase changes in intermetallidny alloy VKNA-25-VI] //Aviacionnye materialy i tehnologii. 2012. №4. S. 8–13.
  8. Romanova N.B., Pechishheva N.V., Shunyaev K.Yu., Titov V.I., Gundobin N.V. Opredelenie nizkih soderzhanij Zr, Ce, La, Y v nikelevyh zharoprochnyh splavah metodom ICP OES [Definition of low maintenance of Zr, Ce, La, Y in nickel hot strength alloys the ICP OES method] // Zavodskaya laboratoriya. Diagnostika materialov. 2011. T. 77. №7. S. 5–9.
  9. Gaiduk O.V., Pantaler R.P., Blank A.B. Spektrofotometricheskoe opredelenie ceriya v prisutstvii Ca, Sr i Al [Spectrophotometric definition of cerium in the presence of Ca, Sr and Al] // Zavodskaya laboratoriya. Diagnostika materialov. 2007. T. 73. №3. S. 15–18.
  10. Abrazheev R.V., Gribanova M.V., Dubcova A.A., Makarova D.A., Vojtkevich E.V. Spektrofotometricheskoe issledovanie kompleksoobrazovaniya ionov ceriya i lantana s arsenatami, sulfatami, fosfatami i hloridami s ispolzovaniem konkuriruyushhih reakcij [Spectrophotometric research of complex formation of ions of cerium and lanthanum with arsenatami, sulfates, phosphates and chlorides with use of competing reactions] // Izvestiya vysshih uchebnyh zavedenij. Ser.: Himiya i himicheskaya tehnologiya. 2015. T. 58. №4. S. 18–21.
  11. Gorbatenko A.A., Beketov V.I., Voronina R.D., Zhuravlev D.A., Lyubomirova O.R., Filatova D.G., Revina E.I. Shemy vozbuzhdeniya monooksidov redkozemelnyh jelementov v lazerno-inducirovannoj molekulyarno-ionizacionnoj spektrometrii plameni [Schemes of excitation of monooxides of rare earth elements in laser induced molecular ionizatsionnoy flame spectrometry] // Zhurnal prikladnoj spektroskopii. 2006. T. 73. №4. S. 544–546.
  12. Gajduk O.V., Pantaler R.P., Blank A.B. Fotometricheskoe opredelenie mikrogrammovyh kolichestv Ce (IV) tropeolinom 00 [Photometric definition of microgram quantities of Ce (IV) by tropeolin 00] // Zavodskaya laboratoriya. Diagnostika materialov. 2006. T. 72. №5. S. 12–14.
  13. Guzik T.V., Maluka L.M. Kosvennoe redoks-potenciometricheskoe opredelenie ceriya (IV) [Indirect redox-potentiometer definition of cerium (IV)] // Izvestiya vysshih uchebnyh zavedenij. Ser.: Himiya i himicheskaya tehnologiya. 2010. T. 53. №11. S. 32–35.
  14. Chumakova N.L., Smirnova E.V. Opredelenie lantana, ceriya, neodima, itterbiya i ittriya v geologicheskih probah s ispolzovaniem mnogokanalnogo analizatora atomno-jemissionnyh spektrov [Definition of lanthanum, cerium, neodima, ytterbium and yttrium in geological tests with use of the multi-channel analyzer of nuclear emission spectrums] // Zavodskaya laboratoriya. Diagnostika materialov. 2010. T. 76. №3. S. 3–8.
  15. Savvin S.B., Krivenkova N.P., Geller A.B., Mihajlova A.V. Novyj sposob probopodgotovki dlya opredeleniya ceriya v materialah jenergeticheskogo mashinostroeniya [New way of probopodgotovka for cerium definition in materials of power mechanical engineering] // Tyazheloe mashinostroenie. 2012. №9. S. 3–5.