Influence of vacuum annealing on structure of ion-plasma coatings made with double aluminizing technology

Matveev P.V., Budinovskiy S.A.
Matveev P.V., Budinovskiy S.A. Influence of vacuum annealing on structure of ion-plasma coatings made with double aluminizing technology // Proceedings of VIAM. 2016. No. 3. DOI: 10.18577/2307-6046-2016-0-3-8-8. URL: https://www.viam-works.ru/en/journal/2016/3/8
Abstract

Influence of vacuum annealing on structure of ion-plasma VSDP-4+VSDP-23 coating made with double aluminizing technology is researched. Coatings made with intermediate heat-treatment are compared to those with increased amount of aluminum alloy sprayed at once. The advantage of standard annealing with the temperature not exceeding 1050 °С is shown. It is also shown that addition of intermediate heat treatment doesn’t influence much on the structure of coating.

Reference list
  1. Kablov E.N., Ospennikova O.G., Bazyleva O.A. Materialy dlja vysokoteplonagruzhennyh detalej gazoturbinnyh dvigatelej [Materials for the high-heatloaded details of gas turbine engines] //Vestnik MGTU im. N.E. Baumana. Ser. «Mashinostroenie». 2011. №SP4. S. 13–19.
  2. Bazyleva O.A., Arginbaeva E.G., Turenko E.Yu. Zharoprochnye litejnye intermetallidnye splavy [Heat resisting cast intermetallic alloys] //Aviacionnye materialy i tehnologii. 2012. №S. S. 57–60.
  3. Budinovskij S.A., Mubojadzhjan S.A., Gajamov A.M. Sovremennoe sostojanie i osnovnye tendencii razvitija vysokotemperaturnyh teplozashhitnyh pokrytij dlja rabochih lopatok turbin aviacionnyh GTD [Current state and the main tendencies of development of high-temperature heat-protective coverings for working blades of turbines of aviation GTE] // Aviacionnaja promyshlennost. 2008. №4. S. 33–37.
  4. Kablov E.N., Mubojadzhjan S.A. Ionnoe travlenie i modificirovanie poverhnosti otvetstvennyh detalej mashin v vakuumno-dugovoj plazme [Ion etching and modifying of surface of responsible details of machines in vacuum and arc plasma] // Vestnik MGTU im. N.E. Baumana. Ser. «Mashinostroenie». 2011. №SP2. S. 149–163.
  5. Kablov E.N., Mubojadzhjan S.A. Teplozashhitnye pokrytija dlja lopatok turbin vysokogo davlenija perspektivnyh GTD [Heat-protective coverings for blades of high-pressure turbines of perspective GTE] // Metally. 2012. №1. S. 5–13.
  6. Budinovskij S.A., Kablov E.N., Mubojadzhjan S.A. Primenenie analiticheskoj modeli opredelenija uprugih naprjazhenij v mnogoslojnoj sisteme pri reshenii zadach po sozdaniju vysokotemperaturnyh zharostojkih pokrytij dlja rabochih lopatok aviacionnyh turbin [Application of analytical model of determination of elastic stresses in multi-layer system at the solution of tasks on creation of high-temperature heat resisting coverings for working blades of aviation turbines] // Vestnik MGTU im. N.E. Baumana. Ser. «Mashinostroenie». 2011. №SP2. S. 26–37.
  7. Kablov E.N., Muboyadzhyan S.A. Zharostojkie i teplozashhitnye pokrytiya dlya lopatok turbiny vysokogo davleniya perspektivnyh GTD [Heat resisting and heat-protective coverings for turbine blades of high pressure of perspective GTE] //Aviacionnye materialy i tehnologii. 2012. №S. S. 60–70.
  8. Kablov E.N., Mubojadzhjan S.A., Budinovskij S.A., Lucenko A.N. Ionno-plazmennye zashhitnye pokrytija dlja lopatok gazoturbinnyh dvigatelej [Ion-plasma protecting covers for blades of gas turbine engines] // Metally. 2007. №5. S. 23–34.
  9. Budinovskij S.A. Primenenie analiticheskoj modeli opredelenija uprugih mehanicheskih i termicheskih naprjazhenij v mnogoslojnoj sisteme v reshenii zadach po sozdaniju zharostojkih aljuminidnyh pokrytij [Application of analytical model of determination of elastic mechanical and thermal stresses in multi-layer system in the solution of tasks on creation of heat resisting alyuminidny coverings] // Uprochnjajushhie tehnologii i pokrytija. 2013. №3. S. 3–11.
  10. Budinovskij S.A., Muboyadzhjan S.A., Gajamov A.M., Matveev P.V. Razrabotka ionno-plazmennyh zharostojkih metallicheskih sloev teplozashhitnyh pokrytij dlja ohlazhdaemyh rabochih lopatok turbin [Development of ion-plasma heat resisting metal layers of heat-protective coverings for cooled working blades of turbines] // MiTOM. 2013. №11. S. 16–21.
  11. Muboyadzhyan S.A., Budinovskij S.A., Gayamov A.M., Matveev P.V. Vysokotemperaturnye zharostojkie pokrytiya i zharostojkie sloi dlya teplozashhitnyh pokrytij [High-temperature heat resisting coverings and heat resisting layers for heat-protective coverings] //Aviacionnye materialy i tehnologii. 2013. №1. S. 17–20.
  12. Matveev P.V., Budinovskij S.A., Muboyadzhyan S.A., Kosmin A.A. Zashhitnye zharostojkie pokrytiya dlya splavov na osnove intermetallidov nikelya [High-temperature coatings for intermetallic nickel-based alloys] //Aviacionnye materialy i tehnologii. 2013. №2. S. 12–15.
  13. Budinovskij S.A., Smirnov A.A., Matveev P.V., Chubarov D.A. Razrabotka teplozashhitnyh pokrytij dlja rabochih i soplovyh lopatok turbiny iz zharoprochnyh i intermetallidnyh splavov [Development of thermal barrier coatings for rotor and nozzle turbine blades made of nickel-base super- and intermetallic alloys] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2015. №4. St. 05. Available at: http://www.viam-works.ru (accessed: June 03, 2015). DOI: 10.18577/2307-6046-2015-0-4-5-5.
  14. Matveev P.V., Budinovskij S.A. Issledovanie svojstv zashhitnyh zharostojkih pokrytij dlya intermetallidnyh nikelevyh splavov tipa VKNA dlya rabochih temperatur do 1300°C [Research of the properties of protective heat-resistant coating for intermetallic nickel alloys operating at temperatures up to 1300°C] // Aviacionnye materialy i tehnologii. 2014. №3. S. 22–26.
  15. Chubarov D.A., Matveev P.V. Novye keramicheskie materialy dlya teplozashhitnyh pokrytij rabochih lopatok GTD [New ceramic materials for thermal barrier coating using in GTE turbine blades] // Aviacionnye materialy i tehnologii. 2013. №4. S. 43–46.
  16. Muboyadzhyan S.A., Budinovskij S.A., Gayamov A.M., Smirnov A.A. Poluchenie keramicheskih teplozashhitnyh pokrytij dlya rabochih lopatok turbin aviacionnyh GTD magnetronnym metodom [Receiving ceramic heat-protective coatings for working blades of turbines of aviation GTD magnetronny method] // Aviacionnye materialy i tehnologii. 2012. №4. S. 3–8.
  17. Mumm D.R., Evans A.G., Spitsberg I.T. Characterization Of A Cyclic Displacement Instability For A Thermally Grown Oxide In A Thermal Barrier System // Acta Materials. 2001. V. 49. P. 2329–2340.
  18. Haynes J.A., Pint B.A., Porter W.D., Wright I.G. Comparison of thermal expansion and oxidation behavior of various high-temperature coating materials and superalloys // Materials at high temperatures. 2004. V. 21 (2). Р. 87–94.
  19. Rabiel A., Evans A.G. Failure Mechanisms Associated With The Thermally Grown Oxide In Plasma-Sprayed Thermal Barrier Coatings // Acta Materials. 2000. V. 48. P. 3963–3976.
  20. Matveev P.V., Budinovskij S.A., Chubarov D.A. Tehnologiya polucheniya ionno-plazmennyh zharostojkih podsloev s povyshennym soderzhaniem alyuminiya dlya perspektivnyh TZP [Technology for production of ion-plasma heat-resistant bonding sub-layers with increased aluminum content for advanced TBCs] // Aviacionnye materialy i tehnologii. 2014. №S5. S. 56–60.