Abstract

The paper provides an overview of scientific and technical literature in the field of advanced technologies for the production of metal matrix composite based on aluminum alloys reinforced with continuous or discontinuous alumina fibers. The main processing methods of receiving this class of materials, their advantages and shortcomings are shown. The paper provides on physical-mechanical properties of metal composite materials on the basis of aluminum alloys reinforced by aluminum oxide fibers. All leading countries in the world are engaged in development of metal matrix composite based on aluminum alloy reinforced with continuous and discontinuous fibers of Al2O3. Space and military agencies demonstrate a particular interest in such developments Tendencies of development of technological approaches to production of metal matrix composite based on the aluminum alloys reinforced by aluminum oxide fibers are revealed.

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] // Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N. Strategicheskie napravleniya razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda [The strategic directions of development of materials and technologies of their processing for the period to 2030] // Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  3. Kablov E.N., Ospennikova O.G., Bazyleva O.A. Materialy dlya vysokonagruzhennyh detalej gazoturbinnyh dvigatelej [Материалы для высоконагруженных деталей газотурбинных двигателей] // Vestnik MGTU im. N.E. Baumana. 2011. №SP2. S. 13–19.
  4. Tarasov Yu.M., Antipov V.V. Novye materialy VIAM – dlya perspektivnoj aviacionnoj tehkniki proizvodstva OAO «OAK» [The VIAM new materials – for perspective aviation engineering of production of JSC «OAK»] // Aviacionnye materialy i tehnologii. 2012. №2. S. 5–6.
  5. Sorokin O.Yu., Grashhenkov D.V., Solntsev S.St., Evdokimov S.A. Keramicheskie kompozicionnye materialy s vysokoj okislitelnoj stojkostyu dlya perspektivnyh letatelnyh apparatov (obzor) [Ceramic composite materials with high oxidation resistance for the novel aircrafts (review)] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №6. St. 08. Available at: http://www.viam-works.ru (accessed: March 18, 2016). DOI: 10.18577/2307-6046-2014-0-6-8-8.
  6. Kablov E.N., Shchetanov B.V., Grashhenkov D.V., Shavnev A.A., Nyafkin A.N. Metallomatrichnye kompozicionnye materialy na osnove Al–SiC [Metalmatrix composite materials on the basis of Al–SiC] // Aviacionnye materialy i tehnologii. 2012. №S. S. 373–380.
  7. Method of making fiber reinforced aluminum matrix composite: pat. 6460597 US; publ. 08.10.02. 13 p.
  8. Metal matrix composite wires, cables, and method: pat. 6344270 US; publ. 05.02.02. 15 p.
  9. Metal matrix composites, and methods for making the same: pat. 2006021729 US; publ. 02.02.06. 11 p.
  10. Method of making metal matrix composites: pat. 6485796 US; publ. 26.11.02. 20 р.
  11. Method for making metal cladded metal matrix composite wire: pat. 7131308 US. publ. 07.11.06. 20 р.
  12. Aluminum matrix composite wire: pat. 6913838 US; publ. 05.07.05. 22 р.
  13. Fiber reinforced aluminum matrix composite with improved interfacial bonding: pat. 5435374 US; publ. 25.07.95. 8 р.
  14. In-situ strengthened metal matrix composite: pat. 2219169 CA; publ. 25.04.98. 8 р.
  15. Methods of fabricating nozzle plates 2006026328 WO; publ. 09.03.2006. 10 р.
  16. Faserformkoerper and process for its manufacture and use of formkoerpers to manufacture faserverstaerkter aluminum castings: pat. 4123677 DE; publ. 21.01.93. 8 р.
  17. Preparation of yogurt containing confectionery pieces and product thereof: pat. 2006165844 US; publ. 27.07.06. 8 р.
  18. Preparation method for light high-strength and high-tenacity aluminum-matrix composite material: pat. 102168214B CN; publ. 17.07.13. 13 р.
  19. Brake facing made of magnesium borate crystal whisker and ceramic particle reinforced aluminium base composite material and its preparation process: pat. 1414132 CN; publ. 30.04.03. 11 р.
  20. Lin GENG, Hong-yu XU, Kuai YU, Hong-lin WANG. Aging behavior of Al2O3 short fiber reinforced Al–Cu alloy composites // Transactions of Nonferrous Metals Society of China. 2007. V. 17. Issue 5. P. 1018–1021.