Development and research of porous fiber metal materials for sound-absorbing elements and abradable seals of gas turbine engines
UDC
66.017:621.775.8
DOI
10.18577/2307-6046-2016-0-11-2-2
Article PDF (Russian)
(717.4 KB)
How to cite
Farafonov D.P., Migunov V.P. Development and research of porous fiber metal materials for sound-absorbing elements and abradable seals of gas turbine engines // Proceedings of VIAM. 2016. No. 11. DOI: 10.18577/2307-6046-2016-0-11-2-2. URL: https://www.viam-works.ru/en/journal/2016/11/2
Keywords
metal fibers, porous fiber metal materials, abradable seals, sound-proof designs, heat resistance.
Abstract
In the article the main results of research of high-temperature materials developed by FSUE «VIAM» produced from the metal fibers intended for application as essentially new abraded seals of air-gas channel and sound-absorbing materials of gas turbine engines are presented. The work is executed within the implementation of the complex scientific directions: 9.7. «High-temperature deformable alloys and the composite materials strengthened by high-melting metal fibers and particles, abraded sealing materials» and 15.7. «Porous fiber metal materials for sound-proof designs» («The strategic directions of materials and technologies of their processing development for the period till 2030»)
Reference list
- Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
- Kablov E.N. Strategicheskie napravleniya razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda [The strategic directions of development of materials and technologies of their processing for the period to 2030] // Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
- Migunov V.P., Farafonov D.P. Issledovanie osnovnyh ekspluatacionnyh svojstv novogo klassa uplotnitelnyh materialov dlya protochnogo trakta GTD [Research of the main operational properties of new class of sealing materials for flowing path of GTE] // Aviacionnye materialy i tehnologii. 2011. №3. S. 15–20.
- Migunov V.P., Farafonov D.P., Degovets M.L., Stupina T.I. Uplotnitelnye materialy dlya protochnogo trakta GTD [Sealing materials for flowing path of GTE] // Aviacionnye materialy i tehnologii. 2012. №S. S. 94–97.
- Migunov V.P., Farafonov D.P., Degovec M.L. Istiraemyj uplotnitelnyj material na osnove volokon iz mednyh splavov [Abradable sealing material made of fibers from copper alloys] // Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №9. St. 04. Available at: http://viam-works.ru (accessed: March 30, 2016). DOI: 10.18577/2307-6046-2014-0-9-4-2.
- Farafonov D.P., Degovets M.L., Serov M.M. Issledovanie svojstv i tehnologicheskih parametrov polucheniya metallicheskih volokon dlya istiraemyh uplotnitelnyh materialov aviacionnyh GTD [The investigation of the properties and technological parameters producing metallic fibers for abradable sealing materials of aircraft GTE] //Trudy VIAM: elektron. nauch.-tehnich. zhurn. 2014. №7. St. 02 Available at: http://viam-works.ru (accessed: March 30, 2016). DOI: 10.18577/2307-6046-2014-0-7-2-2.
- Sobolev A.F., Ushakov V.G., Filippova R.D. Zvukopogloshchayushchie konstruktsii gomogennogo tipa dlya kanalov aviatsionnykh dvigateley [Sound-proof designs of homogeneous type for channels of aircraft engines] // Akusticheskiy zhurnal. 2009. T. 55. №6. S. 749–759.
- Khaletskiy Yu.D. Effektivnost kombinirovannykh glushiteley shuma aviatsionnykh dvigateley [Efficiency of the combined silencers of noise of aircraft engines] // Akusticheskiy zhurnal. 2012. T. 58. №4. S. 556–562.
- Sun F.G., Chen H.L., Wu J.H., Feng K. Sound absorbing characteristics of fibrous metal materials at high temperatures // Appl. Acoust. 2010. V. 711. P. 221–235.
- Smarsly W., Zheng N., Buchheim C.S., Nindel C., Silvestro C., Sporer D., Tuffs M., Schreiber K., Langlade-Bomba C., Andersen O., Goehler H., Simms N.J., McColvin G. Advanced High Temperature Turbine Seals Materials and Designs // Material Science Forum. 2005. V. 492–493.P. 21–26.
- Simms N.J., Norton J.F., McColvin G. Performance of candidate gas turbine abradeable seal materials in high temperature combustion atmospheres // Materials and Corrosion. 2005. V. 56. P. 765–777.
- Serov M.M., Borisov B.V. Poluchenie metallicheskikh volokon i poristykh materialov iz nikh metodom ekstraktsii visyashchey kapli rasplava [Receiving metal fibers and porous materials from them method of ekstraktsiya of hanging drop rasplava] // Tekhnologiya legkikh splavov. 2007. №3. C. 62–65.
- Bazyleva O.A., Arginbaeva E.G., Turenko E.Yu. Vysokotemperaturnye intermetallidnye splavy dlya detaley GTD [The high-temperature intermetallic alloys for parts of gas-turbine engines] // Aviacionnye materialy i tehnologii. 2013. №3. S. 26–31.
- Buntushkin V.P., Kablov E.N., Bazyleva O.A., Morozova G.I. Splavy na osnove alyuminidov nikelya [Alloys on the basis of nickel aluminides] // MiTOM. 1999. №1. S. 32–34.
- Kablov E.N., Solntsev S.S., Rozenenkova V.A., Mironova N.A. Sovremennye polifunktsionalnye vysokotemperaturnye pokrytiya dlya nikelevykh splavov, uplotnitelnykh metallicheskikh voloknistykh materialov i berillievykh splavov [Modern multifunctional high temperature coatings for nickel alloys, sealing metal fibrous materials and beryllium alloys] // Novosti materialovedeniya. Nauka i tekhnika: elektron. nauch.-tekhnich. zhurn. 2013. №1. St. 05. Available at: http://www.materialsnews.ru (accessed: March 30, 2016).
- Solntsev S.S., Rozenenkova V.A., Mironova N.A., Gavrilov S.V. Vysokotemperaturnye tonkoplenochnye pokrytiya dlya uplotnitelnyh materialov iz metallicheskih volokon [High-temperature thin-film coverings for sealing materials from metal fibers] // Aviacionnye materialy i tehnologii. 2012. №1. S. 30–36.
- Felten E.J. Use of Platinum and Rhodium to Improve Oxide Adherence on Ni–8Cr–6Al Alloys // Oxidation of Metals. 1976. V. 10. №l. P. 23–28.
- Allam I.M., Akuezue H.C., Whittle D.P. Influence of Small Pt Additions on Al2O3 Scale Adherence // Oxidation of Metals.1980. V. 14. №6. P. 517–530.
- Heidloff A.J., Tang Z., Zhang F., Gleeson B.C. A Сombined Mapping Process for the Development of Platinum-modified Ni-based Superalloys // JOM. 2010. V. 62. P. 48–53.
- Ballard D.L., Plichak А.L. The use of Precious-metal-modified Nickel-based Superalloys for Thin Gage Apllications // JOM. 2010. V. 62. P. 45–47.
- Amano T., Takezawa Y., Shiino A., Shishido T. Surface morphology of scale on FeCrAl (Pd, Pt, Y) alloys // Journal of alloys and Compounds. 2008. V. 452. Issue 1. P. 16–22.
- Amano T. High-temperature oxidation of FeCrAl (Y, Pt) alloys in oxygen-water vapour // Materials at high temperatures. 2011. V. 28. Issue 4. P. 342–348.
- Amano T. High-temperature oxidation resistance of Al2O3-forming heat-resisting alloys with noble metal and rare earth additions // Materials and Corrosion. 2011. V. 62. №7. P. 659–667.