Brazing the beryllium window in copper frame by silver brazing alloy

Fokanov A.N., Podurazhnaya V.F., Tebyakin А.V., Kas’kov V.S.
Fokanov A.N., Podurazhnaya V.F., Tebyakin А.V., Kas’kov V.S. Brazing the beryllium window in copper frame by silver brazing alloy // Proceedings of VIAM. 2016. No. 11. DOI: 10.18577/2307-6046-2016-0-11-1-1. URL: https://www.viam-works.ru/en/journal/2016/11/1
Keywords
brazing, beryllium windows, copper, silver brazing alloy, structure, vacuum density.
Abstract

The article shows the results of research on brazing the beryllium window in a copper frame by the silver 72Ag–28Cu Cusil hard brazing alloy and study of the structure and vacuum density of the brazing joint. Manufacturing techniques and preparations of products for the brazing were developed, brazing modes on the flat simulator and the bent beryllium window were chosen. A batch of bent brazing beryllium windows which successfully passed tests for vacuum density after heating to 650°C during 0,5 h was made. The structure of brazing joints of beryllium with copper was analyzed. In microstructure of brazing the zone of fusing of beryllium and brazing alloy with partial dissolution of beryllium in brazing alloy is registered as well as Cusil brazing zone with copper dissolution. In zone of fusing of beryllium with Cusil two transitional layers in the form of intermetallic phases are observed. In the zone of Cusil brazing alloy there is the presence of Ag–Cu alloy with different concentra

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33. DOI: 10.18577/2071-9140-2015-0-1-3-33.
  2. Kablov E.N. Strategicheskie napravleniya razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda [The strategic directions of development of materials and technologies of their processing for the period to 2030] // Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  3. Istoriya aviatsionnogo materialovedeniya. VIAM – 80 let: gody i lyudi / pod obshch. red. E.N. Kablova [History of aviation materials science. VIAM – 80 years: years and people / gen. ed/ by E.N.Kablov]. M.: VIAM, 2012. S. 173–180.
  4. Berilliy – konstruktsionnyy material XXI veka [Beryllium – constructional material of the XXI century] // Aviacionnye materialy i tehnologii: nauch.-tekhnich. sb. / pod obshch. red. E.N. Kablova. M.: VIAM, 2000. 136 s.
  5. Antipov V.V. Strategiya razvitiya titanovyh, magnievyh, berillievyh i alyuminievyh splavov [Strategy of development of titanium, magnesium, beryllium and aluminum alloys] //Aviacionnye materialy i tehnologii. 2012. №S. S. 157–167.
  6. Kaskov V.S. Berillij i materialy na ego osnove [Beryllium and materials on its basis] // Aviacionnye materialy i tehnologii. 2012. №S. S. 222–226.
  7. Fokanov A.N., Kaskov V.S., Podurazhnaya V.F. Pajka berilliya so splavom monel pri izgotovlenii rentgenovskih okon [Beryllium brazing with monel alloy in production x-ray windows] // Trudy VIAM: elektron. nauch.-tekhnich. zhurn. 2014. №8. St. 02. Available at: http://www.viam-works.ru (accessed: April 13, 2016). DOI: 10.18577/2307-6046-2014-0-8-2-2.
  8. Fokanov A.N., Kaskov V.S., Podurazhnaya V.F., Zhirnov A.D. Payka berilliya s konstruktsionnymi metallami [The beryllium soldering with constructional metals] // Aktualnye voprosy aviatsionnogo materialovedeniya: tez. dokl. Mezhdunar. nauch.-tekhnich. konf. M., 2007. S. 53.
  9. Pripoy na osnove medi: pat. 2279957 Ros. Federatsiya [Solder on the basis of copper: stalemate. 2279957 Rus. Federation]; zayavl. 21.12.04; opubl. 20.07.06. Byul. №20.
  10. Spravochnik po payke / pod red. I.E. Petrunina [The directory on the soldering / ed. by I.E. Petrunin]. M.: Mashinostroenie, 1984. 400 s.
  11. Lashko S.V., Lashko N.F. Payka metallov [Soldering of metals]. M.: Mashinostroenie, 1988. 376 s.
  12. Goldberg A. Joining of Beryllium. Lawrence Livermore National Laboratory. Livermore. 2006. P. 1–47. Available at: https://e-reports-ext.llnl.gov/pdf/330011.pdf (accessed: April 13, 2016).
  13. Kalin B.A., Fedotov V.T., Sevryukov O.N. Razrabotka i primenenie bystrozakalennykh splavov dlya payki i plakirovaniya konstruktivnykh elementov atomnoy tekhniki [Development and application of the fast-tempered alloys for the soldering and sheathing of constructive elements of nuclear equipment]. Available at: http://www.gidropress.podolsk.ru (accessed: April 13, 2016).
  14. Kalin B.A., Fedotov V.T., Sevryukov O.N., Grigor'ev A.E. i dr. Amorfnye lentochnye pripoi dlya vysokotemperaturnoy payki. Opyt razrabotki tekhnologii i primeneniya [Amorphous tape solders for the high-temperature soldering. Experience of development of technology and application] // Svarochnoe proizvodstvo. 1996. №1. S. 15–19.
  15. Papin P.A., Field R.D. and Javernick D.A. Characterization of Beryllium Copper Intermetallic Phases at a Beryllium Braze Interface by EPMA and TEM // Microscopy and Microanalysis. Vol. 11: Supplement S02. August, 2005. P. 1852–1853. Available at: http://www.journals.cambridge.org (accessed: April 13, 2016).