The influence of alloying elements and structural factors on the resistance of magnesium alloys

Frolov A.V., Mukhina I.Y., Duyunova V.A., Uridiya Z.P.
Frolov A.V., Mukhina I.Y., Duyunova V.A., Uridiya Z.P. The influence of alloying elements and structural factors on the resistance of magnesium alloys // Proceedings of VIAM. 2015. No. 9. DOI: 10.18577/2307-6046-2015-0-9-7-7. URL: https://www.viam-works.ru/en/journal/2015/9/7
Abstract

With the progress of engineering, the operating temperature of articles was greatly increased; therefore, creation of casting magnesium alloys with high strength and heat-resistant characteristics is very an urgent task, to which researchers are faced. Provision of high strength and heat resistant properties of cast magnesium alloys can be achieved due to alloying with promising elements, including selection and optimization of thermal processing conditions. An integrated doping of several rare-earth metals of yttrium (Y, Nd) and cerium (Ce, La, Pr) subgroups in different proportions can be perspective. Expensive rare-earth metals such as erbium, gadolinium, samarium and others can be tested as microadditives improving heat-resistant characteristics of the alloy. In this article some peculiarities of behavior of cast magnesium alloys at elevated temperatures and the influence of doping on their properties were considered. It shows the influence of temperature and duration of soaking du

Reference list
  1. Kablov E.N. Osnovnye itogi i napravlenija razvitija materialov dlja perspektivnoj aviacionnoj tehniki [The main results and the directions of development of materials for perspective aviation engineering] /V sb.: 75 let. Aviacionnye materialy. Izbrannye trudy «VIAM» 1932–2007: Jubilejnyj nauch.-tehnich. sb. M.: VIAM. 2007 S. 20–26.
  2. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitija materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative development of VIAM Federal State Unitary Enterprise of GNTs Russian Federation on implementation «The strategic directions of development of materials and technologies of their processing for the period till 2030»] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  3. Kornysheva I.S., Volkova E.F., Goncharenko E.S., Muhina I.Ju. Perspektivy primenenija magnievyh i litejnyh aljuminievyh splavov [Perspectives of application of magnesium and cast aluminum alloys] //Aviacionnye materialy i tehnologii. 2012. №S. S. 212–222.
  4. Volkova E.F., Muhina I.Ju. Novye materialy na magnievoj osnove i vysokoresursnye tehnologii ih proizvodstva [New materials on magnesian basis and high-resource technologies of their production] //Tehnologija legkih splavov. 2007. №2. S. 28–34.
  5. Muhina I.Ju., Dujunova V.A., Frolov A.V., Uridija Z.P. Vlijanie legirovanija RZM na zharoprochnost' litejnyh magnievyh splavov [Influence of alloying of RZM on thermal stability of cast magnesium alloys] //Metallurgija mashinostroenija. 2014. №5. S. 34–38.
  6. Leonov A.A., Dujunova V.A., Stupak E.V., Trofimov N.V. Lit'e magnievyh splavov v razovye formy, poluchennye novymi metodami [Molding of magnesium alloys in the one-time forms received by new methods] //Trudy VIAM. 2014. №12. St. 01 (viam-works.ru).
  7. Uridija Z.P., Muhina I.Ju., Dujunova V.A., Kosarina E.I. Kontrol' kachestva lit'ja iz magnievyh splavov i sposoby vosstanovlenija germetichnosti otlivok [Molding quality control from magnesium alloys and ways of recovery of tightness of otlivka] //Trudy VIAM. 2014. №12. St. 04 (viam-works.ru).
  8. Erasov V.S., Nuzhnyj G.A., Grinevich A.V., Terehin A.L. Treshhinostojkost' aviacionnyh materialov v processe ispytanija na ustalost' [Treshchinostoykost of aviation materials in the course of fatigue test] //Trudy VIAM. 2013. №10. St. 06 (viam-works.ru).
  9. Salli I.V. Fizicheskie osnovy formirovanija struktury splavov [Physical bases of forming of structure of alloys]. M.: Metallurgizdat. 1963. 219 s.
  10. Mоtt N.F. A theory of work-hardening of metals II: flow without slip-lines, recovery and creep //Philos. Mag. 1953. V. 44. P. 742–765.
  11. Splav na osnove magnija i izdelie, vypolnennoe iz nego [Magnesium-based alloy and the product which has been executed of it]: pat. 2318031 Ros. Federacija; opubl. 27.02.08.
  12. Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace materials science] //Vse materialy: Jenciklopedicheskij spravochnik. 2008. №3. S. 2–14.
  13. Umanskij Ja.S., Kishkin S.T. i dr. Fizicheskoe metallovedenie [Physical metallurgical science]. M.: Metallurgizdat. 1955. 721 s.
  14. Chabina E.B., Alekseev A.A., Filonova E.V., Lukina E.A. Primenenie metodov analiticheskoj mikroskopii i rentgenostrukturnogo analiza dlja issledovanija strukturno-fazovogo sostojanija materialov [Application of methods of analytical microscopy and the rentgenostrukturny analysis for research of structural and phase condition of materials] //Trudy VIAM. 2013. №5. St. 06 (viam-works.ru).
  15. Muhina I.Ju. Struktura i svojstva novyh litejnyh magnievyh splavov [Structure and properties of new cast magnesium alloys] //Litejnoe proizvodstvo. 2011. №12. S. 12–14.
  16. Rohlin L.L. Magnievye splavy, soderzhashhie redkozemel'nye metally [The magnesium alloys containing rare earth metals]. M.: Nauka. 1980. 190 s.
  17. Grube К., Davis A., Eastwood L.W. Alloying of magnesium alloys //Proc. ASTM. 1950. V. 50. P. 965–988.
  18. Fljus dlja plavki magnievyh splavov [Gumboil for melting of magnesium alloys]: pat. 2283887 Ros. Federacija; opubl. 20.09.06.
  19. Murphy A.L, Payne R.I. M. High-strength light alloys //J. Inst. Metals. 1946. V. 75. №3. P. 105–127.
  20. Kablov E.N., Ospennikova O.G., Vershkov A.V. Redkie metally i redkozemel'nye jelementy – materialy sovremennyh i budushhih vysokih tehnologij [Rare metals and rare earth elements – materials of modern and future high technologies] //Trudy VIAM. 2013. №2. St. 01 (viam-works.ru).
  21. Leontis T.E., Feisel D.H. Use rare-earth metals in alloying //J. Metals. 1957. V. 9. №10. P. 1245–1252.
  22. Kablov E.N. Shestoj tehnologicheskij uklad [Sixth technological way] //Nauka i zhizn'. 2010. №4. S. 2–7.
  23. Pashak J.F., Leontis Т.Е. Magnesium alloys containing rare earth metals //Trans. Metallurg. Soc. AIME. 1960. V. 218. №1. P. 102–107.