Chabina E.B., Lomberg B.S., Filonova E.V., Ovsepyan S.V., Bakradze M.M. Change of structural and phase condition of heat resisting deformable nickel alloy at alloying tantalum and rhenium // Proceedings of VIAM. 2015. No. 9. DOI: 10.18577/2307-6046-2015-0-9-3-3. URL: https://www.viam-works.ru/en/journal/2015/9/3
Abstract
Change of structural and phase condition of heat resisting deformable nickel alloy for disks of the turbines ЭК151 is investigated at additional alloying by rhenium and tantalum. It is established that the alloying rhenium of alloy ЭК151 leads to essential decrease in diffusion activity of principal alloying elements and additional solid solution strengthening. The alloying of alloy ЭК151 tantalum increases quantity of strengthening γ'-phase, promotes forming more thermodynamic steady carbides and particles of γ'-phase.
Reference list
- Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitija materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative development of VIAM Federal State Unitary Enterprise of GNTs Russian Federation on implementation «The strategic directions of development of materials and technologies of their processing for the period to 2030»] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
- Bokshtejn S.Z., Kishkin S.T., Shalin R.E. Strukturnaja stabil'nost' konstrukcionnyh materialov [Structural stability of constructional materials] /V sb. Aviacionnye materialy na rubezhe XX–XXI vekov. M.: VIAM. 1994. S. 547–553.
- Supersplavy II [Superalloys II] /Pod red. Ch.T. Simsa, N.S. Stoloffa, U.K. Hagelja. M.: Metallurgija. 1995. Kn. 1. 384 s.
- Chabina E.B., Filonova E.V., Lomberg B.S., Bakradze M.M. Struktura sovremennyh deformiruemyh nikelevyh splavov [Structure of modern deformable nickel alloys] //Vse materialy. Jenciklopedicheskij spravochnik. 2012. №6. S. 22–27.
- Lomberg B.S., Ovsepjan S.V., Bakradze M.M., Mazalov I.S. Vysokotemperaturnye zharoprochnye nikelevye splavy dlja detalej gazoturbinnyh dvigatelej [High-temperature heat resisting nickel alloys for details of gas turbine engines] //Aviacionnye materialy i tehnologii. 2012. №S. S. 52–57.
- Lomberg B.S., Ovsepjan S.V., Bakradze M.M. Novyj zharoprochnyj nikelevyj splav dlja diskov gazoturbinnyh dvigatelej i gazoturbinnyh ustanovok [New heat resisting nickel alloy for disks of gas turbine engines and gas turbine units] //Materialovedenie. 2010. №7. S. 24–28.
- Lomberg B.S., Ovsepjan S.V., Limonova E.N., Letnikov M.N., Bakradze M.M., Chabina E.B., Latyshev V.B. Zharoprochnye nikelevye splavy dlja diskov GTD. Zharoprochnye svarivaemye splavy dlja detalej gorjachego trakta GTD [Heat resisting nickel alloys for disks GTD. Heat resisting welded alloys for details of hot path of GTD] /V sb. tezisov Mezhdunarodnoj nauchn.-tehnich. konf. «Aktual'nye voprosy aviacionnogo materialovedenija». M.: VIAM. 2007. S. 19–20.
- Lomberg B.S., Ovsepjan S.V., Latyshev V.B., Chabina E.B. Zharoprochnye deformiruemye splavy dlja gorjachego trakta gazoturbinnyh dvigatelej (GTD) [Heat resisting deformable alloys for hot path of gas turbine engines (GTD)] /V kn. 75 let. Aviacionnye materialy. Izbrannye trudy «VIAM» 1932–2007»: Jubilejnyj nauch.-tehnich. M.: VIAM. 2008. S. 59–64.
- Chabina E.B., Filonova E.V., Lomberg B.S., Morozova G.I. Jevoljucija struktury i fazovogo sostava deformiruemyh zharoprochnyh nikelevyh splavov dlja diskov GTD s uslozhneniem ih legirovanija [Evolution of structure and phase composition of deformable heat resisting nickel alloys for disks GTD with complication of their alloying] //MiTOM. 2015. №3 (717). S. 8–12.
- Lomberg B.S., Ovsepjan S.V., Bakradze M.M. Osobennosti legirovanija i termicheskoj obrabotki zharoprochnyh nikelevyh splavov dlja diskov gazoturbinnyh dvigatelej novogo pokolenija [Features of alloying and thermal processing of heat resisting nickel alloys for disks of gas turbine engines of new generation] //Aviacionnye materialy i tehnologii. 2010. №2. S. 3–8.
- Lomberg B.S., Bakradze M.M., Chabina E.B., Filonova E.V. Vlijanie mikrolegirujushhih jelementov na strukturno-fazovuju stabil'nost' i svojstva zharoprochnogo deformiruemogo splava (pri dlitel'nyh narabotkah) [Influence of microdoping elements on structural and phase stability and property of heat resisting deformable alloy (at long practices)] //Metallurg. 2013. №9. S. 93–97.
- Chabina E.B., Filonova E.V., Lomberg B.S., Zajcev D.V. Osobennosti formirovanija struktury vysokozharoprochnogo nikelevogo splava pri kompleksnom mikrolegirovanii lantanoidami [Features of forming of structure of high-heat resisting nickel alloy at complex microalloying lanthanoids] //Metally. 2014. №6. S. 62–69.
- Kablov E.N., Ospennikova O.G., Lomberg B.S. Kompleksnaja innovacionnaja tehnologija iz-otermicheskoj shtampovki na vozduhe v rezhime sverhplastichnosti diskov iz superzharoprochnyh splavov [Complex innovative technology of isothermal punching on air in mode of superplasticity of disks from superhot strength alloys] //Aviacionnye materialy i tehnologii. 2012. №S. S. 129–141.
- Lomberg B.S., Bakradze M.M., Chabina E.B., Filonova E.V. Vzaimosvjaz' struktury i svojstv vysokozharoprochnyh nikelevyh splavov dlja diskov gazoturbinnyh dvigatelej [Interrelation of structure and properties of high-heat resisting nickel alloys for disks of gas turbine engines] //Aviacionnye materialy i tehnologii. 2011. №2. S. 25–30.
- Bakradze M.M., Ovsepjan S.V., Shugaev S.A., Letnikov M.N. Vlijanie rezhimov zakalki na strukturu i svojstva shtampovok diskov iz zharoprochnogo nikelevogo splava JeK151-ID [Influence of modes of tempering on structure and property of punchings of disks from heat resisting EK151-ID nickel alloy] //Trudy VIAM. 2013. №9. St. 01 (viam-works.ru).
- Morozova G.I. Kompensacija disbalansa legirovanija zharoprochnyh nikelevyh splavov [Compensation of imbalance of alloying of heat resisting nickel alloys] //MiTOM. №12. 2012. S. 52–56.
- Kablov E.N., Bronfin M.B. Jeffekt S.T. Kishkina, ili pochemu struktura zharoprochnyh nikelevyh splavov dolzhna byt' geterofaznoj [Kishkina or why the structure of heat resisting nickel alloys has to be heterophase] /V sb. Litejnye zharoprochnye splavy. Jeffekt S.T. Kishkina: nauchn.-tehn. sb.; Pod. red. E.N. Kablova. M.: Nauka. 2006. S. 7–14.
- Skljarenko V.G., Moiseev N.V., Gerasimov V.V., Petrushin N.V., Chabina E.B. Razrabotka tehnologii formirovanija reglamentirovannoj struktury v shtampovkah diskov ih slitkov vysokogradientnoj kristallizacii splava JeK151 [Development of technology of forming of the regulated structure in punchings of disks of their ingots of high-gradient crystallization of alloy ЭК151] /V sb. tezisov Mezhdunarodnoj nauchn.-tehnich. konf. «Aktual'nye voprosy aviacionnogo materialovedenija». M.: VIAM. 2007. S. 70–71.
- Kablov E.N., Petrushin N.V., Vasilenok L.B., Morozova G.I. Renij v zharoprochnyh nikelevyh splavah dlja lopatok gazovyh turbin (prodolzhenie) [Reny in heat resisting nickel alloys for blades of gas turbines (continuation)] //Materialovedenie. 2000. №3. S. 38–43.
- Kablov E.N. Fiziko-himicheskie i tehnologicheskie osobennosti sozdanija zharoprochnyh splavov, soderzhashhih renij [Physical and chemical and technological features of creation of the hot strength alloys, containing reniye] //Vestnik Moskovskogo universiteta. Ser. 2: Himija. 2005. T. 46. №3. S. 155–167.
- Bakradze M.M., Lomberg B.S., Ovsepjan S.V., Chabina E.B., Filonova E.V. Vlijanie renija na fazovyj sostav i svojstva zharoprochnogo deformiruemogo splava na nikelevoj osnove dlja diskov turbin GTD [Influence of reniye on phase structure and property of heat resisting deformable nickel-based alloy for disks of turbines GTD] //Materialovedenie. 2015. №1. S. 38–44.
- Fizicheskoe metallovedenie. T. 1. Atomnoe stroenie metallov i splavov [Physical metallurgical science. T. 1. Nuclear structure of metals and alloys] /Pod red. R.U. Kana, P. Haazena. M.: Metallurgija. 1987. 639 s.
- Chabina E.B., Alekseev A.A., Filonova E.V., Lukina E.A. Primenenie metodov analiticheskoj mikroskopii i rentgenostrukturnogo analiza dlja issledovanija strukturno-fazovogo sostojanija materialov [Application of methods of analytical microscopy and the rentgenostrukturny analysis for research of structural and phase condition of materials] //Trudy VIAM. 2013. №5. St. 06 (viam-works.ru).
- Golikov I.N., Maslenkov S.B. Dendritnaja likvacija v staljah i splavah [Dendritic segregation in stalyakh and alloys]. M.: Metallurgija. 1977. 223 s.