Research of material inhomogeneity of reference samples made of wrought Ni-based superalloy VZH175-ID

Eroshkin S.G., Orlov G.V.
Eroshkin S.G., Orlov G.V. Research of material inhomogeneity of reference samples made of wrought Ni-based superalloy VZH175-ID // Proceedings of VIAM. 2015. No. 8. DOI: 10.18577/2307-6046-2015-0-8-11-11. URL: https://www.viam-works.ru/en/journal/2015/8/11
Abstract

Methods of spectral analysis are widely used at production of Ni-based superalloys to determine the chemical composition of the melt. Certified reference samples of material composition (CRMs) are used for plotting of calibration curves to make quantitative spectral analysis. Uncertainty of the certified values of CRMs affects significantly on the accuracy of quantitative analysis. The uncertainty of the inhomogeneity of the CRM composition is one of the components of the total uncertainty of the CRM certified value. In this work, a study of inhomogeneity of wrought Ni-based superalloy VZH175-ID was carried out with the use of X-ray fluorescence spectroscope S8 Tiger and measurement conditions were selected. The standard uncertainty of the heterogeneity was estimated. It was shown that the obtained level of the standard uncertainty of heterogeneity allows the usage of CRM material for development and production of state standard reference samples (SCRM) of the approved type.

Reference list
  1. Kablov E.N., Ospennikova O.G., Bazyleva O.A. Materialy dlja vysokoteplonagruzhennyh detalej gazoturbinnyh dvigatelej [Materials for the high-heatloaded details of gas turbine engines] //Vestnik Moskovskogo gosudarstvennogo tehnicheskogo universiteta im. N.Je. Baumana. Ser. «Mashinostroenie». 2011. №SP2. S. 13–19.
  2. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitija materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative development of VIAM Federal State Unitary Enterprise of GNTs Russian Federation on implementation «The strategic directions of development of materials and technologies of their processing for the period till 2030»] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  3. Kablov E.N., Ospennikova O.G., Sidorov V.V., Rigin V.E., Kablov D.E. Osobennosti tehno-logii vyplavki i razlivki sovremennyh litejnyh vysokozharoprochnyh nikelevyh splavov [Features of smelting technology and razlivka of modern cast high-heat resisting nickel alloys] //Vestnik Moskovskogo gosudarstvennogo tehnicheskogo universiteta im. N.Je. Baumana. Ser. «Mashinostroenie». 2011. №SP2. S. 68–78.
  4. Kablov E.N., Sidorov V.V., Kablov D.E. i dr. Sovremennye tehnologii poluchenija prutkovyh zagotovok iz litejnyh zharoprochnyh splavov novogo pokolenija [Modern technologies of receiving bar preparations from foundry hot strength alloys of new generation] //Aviacionnye materialy i tehnologii. 2012. №S. S. 97–105.
  5. Istorija aviacionnogo materialovedenija. VIAM – 80 let: gody i ljudi [History of aviation materials science. VIAM – 80 years: years and people] /Pod. obshh. red. E.N. Kablova. M.: VIAM. 2012. S. 181–196.
  6. Sposob lit'ja diskovyh i kol'cevyh zagotovok iz zharoprochnyh trudnodeformiruemyh splavov na nikelevoj osnove [Way of molding of disk and ring preparations from heat resisting trudnodeformiruyemy nickel-based alloys]: pat. 2422244 Ros. Federacija; opubl. 28.10.2009.
  7. Kablov E.N. Razrabotki VIAM dlja gazoturbinnyh dvigatelej i ustanovok [Development of VIAM for gas turbine engines and installations] //Kryl'ja Rodiny. 2010. №4. S. 31–33.
  8. Kablov E.N., Petrushin N.V., Svetlov I.L., Demonis I.M. Nikelevye litejnye zharoprochnye splavy novogo pokolenija [Nickel foundry hot strength alloys of new generation] //Aviacionnye materialy i tehnologii. 2012. №S. C. 36–51.
  9. Jerhardt H. Rentgenofluorescentnyj analiz. Primenenie v zavodskih laboratorijah [Rentgenofluorestsentny analysis. Application in factory laboratories]. M.: Metallurgija, 1985. 256 s.
  10. Juing G.V. Instrumental'nye metody himicheskogo analiza [Tool methods of chemical analysis]. M.: Mir. 1989. 608 s.
  11. Afonin V.P., Komjak N.I., Nikolaev V.I., Plotnikov R.I. Rentgenofluorescentnyj analiz [Rentgenofluorestsentny analysis]. Novosibirsk: Nauka. 1991. 173 s.
  12. Oreshnikova E.G. Spektral'nyj analiz [Spectrum analysis]. M.: Vysshaja shkola, 1982. 375 s.
  13. Kablov E.N., Morozov G.A., Krutikov V.N., Muravskaja N.P. Attestacija standartnyh obrazcov sostava slozhnolegirovannyh splavov s primeneniem jetalona [Certification of standard samples of structure of complex-alloyed alloys using standard] //Aviacionnye materialy i tehnologii. 2012. №2. C. 9–11.
  14. Letov A.F., Karachevcev F.N., Gundobin N.V., Titov V.I. Razrabotka standartnyh obrazcov sostava splavov aviacionnogo naznachenija [Development of standard samples of structure of alloys of aviation assignment] //Aviacionnye materialy i tehnologii. 2012. №S. C. 393–398.
  15. GOST 8.315. Standartnye obrazcy sostava i svojstv veshhestv i materialov. Osnovnye polozhenija [Standard samples of structure and properties of substances and materials. Basic provisions].
  16. Turchenkov V.A., Baranov D.E., Gagarin M.V., Shishkin M.D. Metodicheskij podhod k prove-deniju jekspertizy materialov [Methodical approach to carrying out examination of materials] //Aviacionnye materialy i tehnologii. 2012. №1. S. 47–53.
  17. Federal'nyj zakon ot 26 ijulja 2008 g. №102-FZ «Ob obespechenii edinstva izmerenij». St. 12 «Utverzhdenie tipa standartnyh obrazcov ili tipa sredstv izmerenij» [The federal law from July 26, 2008 of No. 102-FZ «About ensuring unity of measurements». Art. 12 «The statement like standard samples or type of measuring instruments»].
  18. GOST 8.531–2002 Standartnye obrazcy sostava monolitnyh i dispersnyh materialov. Sposoby ocenivanija odnorodnosti [Standard samples of structure of monolithic and disperse materials. Ways of estimation of uniformity].
  19. R 50.2.058–2007 Ocenivanie neopredelennosti attestovannyh znachenij standartnyh obrazcov [Estimation of uncertainty of the certified values of standard samples].
  20. Smagunova A.N., Kozlov V.A. Primery primenenija matematicheskoj teorii jeksperimenta v rentgenofluorescentnom analize [Examples of application of the mathematical theory of experiment in the rentgenofluorestsentny analysis]. Irkutsk: IGU. 1990. 232 s.