Estimation of annular stiffness of PCM rings by acoustic resonance method
Nikitin E.K., Burkhan O.L., Postnov V.I. Estimation of annular stiffness of PCM rings by acoustic resonance method // Proceedings of VIAM. 2015. No. 6. DOI: 10.18577/2307-6046-2015-0-6-12-12. URL: https://www.viam-works.ru/en/journal/2015/6/12
Abstract
Measurements of parameters of an acoustic signal excited by own mechanical oscil-lations of a ring made from fiber-reinforced plastics under mechanical impact were carried out; then the annular stiffness of ring was calculated. The method is based on excitation of acoustic signal oscillations, which depend on strength characteristics of the PCM ring.
Reference list
- Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strate-gicheskih napravlenij razvitija materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative development of VIAM Federal State Unitary Enterprise of GNTs Russian Federation on implementation «The strategic directions of development of materials and technologies of their processing for the period till 2030»] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
- Kablov E.N. Rossii nuzhny materialy novogo pokolenija [Materials of new generation are necessary to Russia] //Redkie zemli. 2014. №3. S. 8–13.
- Sokolov I.I., Raskutin A.E. Ugleplastiki i stekloplastiki novogo pokolenija [Ugleplastiki and fibreglasses of new generation] //Trudy VIAM. 2013. №4. St. 09 (viam-works.ru).
- Timoshkov P.N., Kogan D.I. Sovremennye tehnologii proizvodstva polimernyh kompozicionnyh materialov novogo pokolenija [Modern production technologies of polymeric composite materials of new generation] //Trudy VIAM. 2013. №4. St. 07 (viam-works.ru).
- Turchenkov V.A., Baranov D.E., Gagarin M.V., Shishkin M.D. Metodicheskij podhod k provedeniju jekspertizy materialov [Methodical approach to carrying out examination of materials] //Aviacionnye materialy i tehnologii. 2012. №1. S. 47–53.
- Rabinovich A.L. Vvedenie v mehaniku armirovannyh polimerov [Introduction in mechanics of the reinforced polymers]. M.: Nauka. 1970. 482 s.
- Kablov E.N. Himija v aviacionnom materialovedenii [Chemistry in aviation materials sci-ence] //Rossijskij himicheskij zhurnal. 2010. T. LIV. №1. S. 3–4.
- Murashov V.V., Rumjancev A.F., Ivanova G.A., Fajzrahmanov N.G. Diagnostika struktury, sostava i svojstv polimernyh kompozicionnyh materialov [Diagnostics of structure, structure and properties of polymeric composite materials] //Aviacionnye materialy i tehnologii. 2008. №1. S. 17–24.
- Murashov V.V. Opredelenie fiziko-mehanicheskih harakteristik i sostava polimernyh kompozicionnyh materialov akusticheskimi metodami [Definition of physicomechanical characteristics and composition of polymeric composite materials acoustic methods] //Aviacionnye materialy i tehno-logii. 2012. №S. S. 465–475.
- Murashov V.V. Nerazrushajushhij kontrol' zagotovok i detalej iz uglerod-uglerodnogo kompozicionnogo materiala dlja mnogorazovogo kosmicheskogo korablja «Buran» [Non-destructive testing of preparations and details from carbon-carbon composite material for the reusable «Buran» spacecraft] //Trudy VIAM. 2013. №4. St. 05 (viam-works.ru).
- Savel'ev I.V. Kurs obshhij fiziki [Course the general physics]. T. 1. M.: Fizika. 1970. S. 263–265.
- GOST R 54560–2011 Truby i detali truboprovodov iz reaktoplastov, armirovannyh steklovoloknom [Pipes and details of pipelines from the thermosets reinforced by fiber glass].