Abstract

Different methods of suppression of spectrum interferences and their efficiency in case of 4% (mass.) content of interference-causing elements were described. Content of Cu, Zn, Se, Ag and Cd in Nb-based alloy was determined by the inductively coupled plasma mass spectrometry method (IСP-MS). An effect of the interference-causing alloying elements (Ti, Cr, Zr and Mo) on the results of determination was investigated. The correctness of this measurement technique was controlled by the «added–found» method. Correction of spec-tral interferences at the addition of interference-causing elements in the test solution allowed to improve the accuracy of measurements and to assess the degree of the effect of mass-spectral interferences for each element to be determined. The use of a collision-reaction cell allowed to reduce the mass-spectral interferences of elements at determination of Cu, Zn, Ag and Cd and, respectively, their detection limits by one or two orders of magnitude as compared to t

Reference list
  1. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitija materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative development of VIAM Federal State Unitary Enterprise of GNTs Russian Federation on implementation «The strategic directions of development of materials and technologies of their processing for the period till 2030»] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  2. Kablov E.N., Ospennikova O.G., Vershkov A.V. Redkie metally i redkozemel'nye jelementy – materialy sovremennyh i budushhih vysokih tehnologij [Rare metals and rare earth elements – materials of modern and future high technologies] //Trudy VIAM. 2013. №2. St. 01 (viam-works.ru).
  3. Lomberg B.S., Ovsepjan S.V., Bakradze M.M., Mazalov I.S. Vysokotemperaturnye zharoprochnye nikelevye splavy dlja detalej gazoturbinnyh dvigatelej [High-temperature heat resisting nickel alloys for details of gas turbine engines] //Aviacionnye materialy i tehnologii. 2012. №S. C. 52–57.
  4. Kablov E.N., Bondarenko Ju.A., Echin A.B., Surova V.A. Razvitie processa napravlennoj kristallizacii lopatok GTD iz zharoprochnyh splavov s monokristallicheskoj i kompozicionnoj strukturoj [Development of process of the directed crystallization of blades of GTD from hot strength alloys with single-crystal and composition structure] //Aviacionnye materialy i tehnologii. 2012. №1. S. 3–8.
  5. Min P.G., Sidorov V.V. Rafinirovanie othodov zharoprochnogo nikelevogo splava ZhS32-VI ot primesi kremnija v uslovijah vakuumnoj indukcionnoj plavki [Refinement of waste of heat resisting ZhS32-VI nickel alloy from silicon impurity in the conditions of vacuum induction melting] //Trudy VIAM. 2014. №9. St. 01 (viam-works.ru).
  6. Min P.G., Sidorov V.V. Opyt pererabotki litejnyh othodov splava ZhS32-VI na nauchnoproizvodstvennom komplekse VIAM po izgotovleniju lityh prutkovyh (shihtovyh) zagotovok [Experience of processing of foundry waste of alloy ZhS32-VI on VIAM scientific-industrial complex on manufacturing of cast bar (blend) preparations] //Aviacionnye materialy i tehnologii. 2013. №4. S. 20–25.
  7. Kablov E.N., Lomberg B.S., Ospennikova O.G. Sozdanie sovremennyh zharoprochnyh materialov i tehnologij ih proizvodstva dlja aviacionnogo dvigatelestroenija [Creation of modern heat resisting materials and technologies of their production for aviation engine building] //Kryl'ja Rodiny. 2012. №3–4. S. 34–38.
  8. Kablov E.N., Svetlov I.L., Efimochkin I.Ju. Vysokotemperaturnye Nb–Si-kompozity [High-temperature Nb-Si-composites] //Vestnik MGTU im. N.Je. Baumana. Ser. «Mashi-nostroenie». 2011. №SP2. S. 164–173.
  9. Bewlay B.P., Jackon M.R., Zhao H.C. etal. Ultrahigh-Temperature Nb-Silicide-Based Composites //Mrs. Bulletin. Spt. 2003.P. 646–653.
  10. Svetlov I.L., Abuzin Ju.A., Babich B.N. i dr. Vysokotemperaturnye Nb–Si-kompozity, uprochnennye silicidami niobija [The high-temperature Nb-Si-composites strengthened by silicides of niobium] //Zhurnal funkcional'nyh materialov. 2007. T. 1. №2. S. 48–52.
  11. High Temperature Niobium alloy: pat. №7632455 US; pabl. 15.12.2009.
  12. Hu J., Wang H. Determination of Trace Elements in Super Alloy by ICP-MS //Mikrochim. Acta. 2001. V. 137. P. 149–155.
  13. Pupyshev A.A., Jepova E.N. Spektral'nye pomehi poliatomnyh ionov v metode mass-spektrometrii s induktivno svjazannoj plazmoj [Spectral hindrances of polynuclear ions in mass-spectrometry method with inductively connected plasma] //Analitika i kontrol'. 2001. T.5. №4. S. 335–369.
  14. Lejkin A.Ju., Jakimovich P.V. Sistemy podavlenija spektral'nyh interferencij v mass-spektrometrii s induktivno svjazannoj plazmoj [Systems of suppression of spectral interferences in mass-spectrometry with inductively connected plasma] //Zhurnal analiticheskoj himii. 2012. T. 67. №8. S. 752–762.
  15. MI 1.2.052–2013 «Metodika izmerenij massovoj doli primesej R, Mn, Fe, Cu, Zn, Ga, As, Se, Ag, Cd, Sn, Sb, Te, Tl, Pb, Bi v nikelevyh splavah metodom mass-spektrometrii s induktivno svjazannoj plazmoj» [«Measurement technique of mass fraction of impurity P, Mn, Fe, Cu, Zn, Ga, As, Se, Ag, CDs, Sn, Sb, Te, Tl, Pb, Bi in nickel alloys mass-spectrometry method with inductively connected plasma»]. M.: VIAM. 2013.
  16. Smirnova E.V., Lozhkin V.I. O vybore analiticheskih izotopov redkozemel'nyh jelementov v metode mass-spektrometrii s induktivno svjazannoj plazmoj [About choice of analytical isotopes of rare earth elements in mass-spectrometry method with inductively connected plasma] //Analitika i kontrol'. 2004. T. 8. №4. S. 329–338.
  17. Pupyshev A.A., Surikov V.T. Mass-spektrometrija s induktivno svjazannoj plazmoj. Obrazovanie ionov [Mass-spectrometry with inductively connected plasma. Formation of ions]. Ekaterinburg: UrO RAN. 2006. 276 s.
  18. Pupyshev A.A., Danilova D.A. Ispol'zovanie atomno-jemissionnoj spektrometrii s induktivno svjazannoj plazmoj dlja analiza materialov i produktov chernoj metallurgii [Use of nuclear and emission spectrometry with inductively connected plasma for the analysis of materials and products of ferrous metallurgy] //Analitika i kontrol'. 2007. T. 11. №2–3. S. 131–181.
  19. Aries S., Valladon M. et al. A routine method for oxide and hydroxide interference correction in ICP-MS chemical analysis of environmental and geological samples //Geostandards Newsletter. 2000. V. 24. P. 19–31.