Film resin infusion as an advanced method for out-of-autoclave processing of polymer composites

Timoshkov P.N., Platonov A.A., Khrulkov A.V.
Timoshkov P.N., Platonov A.A., Khrulkov A.V. Film resin infusion as an advanced method for out-of-autoclave processing of polymer composites // Proceedings of VIAM. 2015. No. 5. DOI: 10.18577/2307-6046-2015-0-5-9-9. URL: https://www.viam-works.ru/en/journal/2015/5/9
Keywords
RFI
Abstract

A rapid increase in the portion of polymer composite materials (PCM) in structures of civil aircraft occurred in the 2000-s, allowed to increase significantly reliability and service life of aviation equipment and to reduce its weight. However, there was a vital problem to reduce the cost of PCM structures, which always were more expensive than similar parts made of metal. In many ways, the high cost of PCM products depends on high labor- and power consumption of autoclave technology, which at present is most widely used in the aircraft industry, as well as by high costs of relevant equipment. In recent years, VIAM actively develops the out-of-autoclave production of PCM parts. The results of the works performed by VIAM to develop PCM-based woven fillers produced by impregnation with film binder are described. Comparative elastic-strength characteristics of the produced carbon fiber-reinforced plastic are given.

Reference list
  1. Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [The strategic directions of development of materials and technologies of their processing for the period till 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  2. Dushin M.I., Hrul'kov A.V., Platonov A.A., Ahmadieva K.R. Bezavtoklavnoe formovanie ugleplastikov na osnove prepregov, poluchennyh po rastvornoj tehnologii [Bezavtoklavnoye formation ugleplastikov on the basis of the prepregs received on solution technology] //Aviacionnye materialy i tehnologii. 2012. №2. S. 43–48.
  3. Hrul'kov A.V., Dushin M.I., Popov Ju.O., Kogan D.I. Issledovanija i razrabotka avtoklavnyh i bezavtoklavnyh tehnologij formovanija PKM [Researches and development of avtoklavny and bezavtoklavny technologies of formation of PKM] //Aviacionnye materialy i tehnologii. 2012. №S. S. 292–301.
  4. Chursova L.V., Dushin M.I., Kogan D.I., Panina N.N., Kim M.A., Gurevich Ja.M., Platonov A.A. Plenochnye svjazujushhie dlja RFI-tehnologii [Film binding for RFI technology] //Rossijskij himicheskij zhurnal. 2010. №1. S. 63–66.
  5. Babin A.N. Svjazujushhie dlja polimernyh kompozicionnyh materialov novogo pokolenija [Binding for polymeric composite materials of new generation] //Trudy VIAM. 2013. №4 (viam-works.ru).
  6. Postnova M.V., Postnov V.I. Opyt razvitija bezavtoklavnyh metodov formovanija PKM [Experience of development of bezavtoklavny methods of formation of PKM] //Trudy VIAM. 2014. №4. St. 06 (viam-works.ru).
  7. Sposob poluchenija kompozicionnogo materiala [Way of receiving composite material]: pat. №2246379 Ros. Federacija; opubl. 25.02.2004.
  8. Kablov E.N., Starcev O.V., Krotov A.S., Kirillov V.N. Klimaticheskoe starenie kompozicionnyh materialov aviacionnogo naznachenija. I. Mehanizmy starenija [Climatic aging of composite materials of aviation assignment. I. Aging mechanisms] //Deformacija i razrushenie materialov. 2010. №11. S. 19–27.
  9. Kablov E.N., Starcev O.V., Krotov A.S., Kirillov V.N. Klimaticheskoe starenie kompozicionnyh materialov aviacionnogo naznachenija. III. Znachimye faktory starenija [Climatic aging of composite materials of aviation assignment. III. Significant factors of aging] //Deformacija i razrushenie materialov. 2011. №1. S. 34–40.
  10. Kirillov V.N., Starcev O.V., Efimov V.A. Klimaticheskaja stojkost' i povrezhdaemost' polimernyh kompozicionnyh materialov, problemy i puti reshenija [Climatic firmness and damageability of polymeric composite materials, problems and solutions] //Aviacionnye materialy i tehnologii. 2012. №S. S. 412–423.
  11. Meljohina M.I., Kavun N.S., Rakitina V.P. Jepoksidnye stekloplastiki s uluchshennoj vlago- i vodostojkost'ju [Epoxy fibreglasses with improved vlago-and water resistance] //Aviacionnye materialy i tehnologii. 2013. №2. S. 29–31.
  12. Dushin M.I., Muhametov R.R., Platonov A.A., Merkulova Ju.I. Issledovanie fil'tracionnyh harakteristik armirujushhih napolnitelej i svjazujushhih pri razrabotke tehnologii bezavtoklavnogo formovanija polimernyh kompozicionnyh materialov [Research of filtrational characteristics of reinforcing fillers and binding when developing technology of bezavtoklavny formation of polymeric composite materials] //Aviacionnye materialy i tehnologii. 2013. №2. S. 22–25.
  13. Platonov A.A., Kogan D.I., Dushin M.I. Izgotovlenie trehmernoarmirovannyh PKM metodom propitki plenochnym svjazujushhim [Manufacturing of trekhmernoarmirovanny PKM by method of impregnation by the film binding] //Plasticheskie massy. 2013. №12. S. 56–61.