Shchepilov A.V., Muboyadzhyan S.A., Gorlov D.S., Konnova V.I. Investigation of the ion-plasma coatings influence on damping capacity of «alloy-coating» composition during testing on vibrodynamic bench // Proceedings of VIAM. 2015. No. 4. DOI: 10.18577/2307-6046-2015-0-4-8-8. URL: https://www.viam-works.ru/en/journal/2015/4/8
Abstract

The possibility of using ion-plasma coatings deposited by high energy vacuum-plasma technology to reduce the free end oscillations amplitude of VT6 titanium alloy samples during testing on vibrodynamic bench at resonance conditions by the first bending mode is hereby shown. The coatings based on pure Ti, Zr, Cr, Ni, Al, Cu metals deposited on the MAP-3 unit under modes enabling the coating growth in the range of 19–73 g/m2 while the tempera-ture of ion and radiation heating does not exceed tempering temperature of the VT6 titanium alloy is investigated. The tests on the damping capacity of applied coatings were performed. It is established that aluminum coating has the best properties.

Reference list
  1. Muravchenko F.M., Sheremet'ev A.V. Aktual'nye problemy dinamiki, prochnosti i nadezhnosti sovremennyh aviadvigatelej [Actual problems of dynamics, durability and reliability of modern aircraft engines] //Vibracii v tehnike i tehnologijah. 2001. №4(20). S. 2–5.
  2. Shorr B.F., Serebrjakov N.N. Raschetno-jeksperimental'nyj analiz amplitudno-zavisimyh harakteristik dempfirovanija v detaljah i materialah [The rated and experimental analysis of amplitude and dependent characteristics of damping in details and materials] //Problemy mashinostroenija i nadezhnosti mashin. 2011. №3. S. 91–99.
  3. Sordelet D.J., Kim J.S., Besser M.F. Dryslidin go fpolygrainedquasicrystalinne and crystalline
  4. Al–Cu–Fe alloys //Mat. Res. Soc. Symp. Poc. 1999. V. 553. P. 459–470.
  5. Paton B.E., Movchan B.A. Composite Materials Deposited from the Vapour Phase in Vacuum Soviet Technologies Review //Weld and Surfacing. 1991. V. 2. P. 43–64.
  6. Mubojadzhjan S.A., Pomelov Ja.A. Zashhitnye pokrytija dlja lopatok kompressora GTD [Protecting covers for GTD compressor blades] /V sb.: Aviacionnye materialy i tehnologii. Vyp. «Vysokozharoprochnye materialy dlja sovremennyh i perspektivnyh gazoturbinnyh dvigatelej i progressivnye tehnologii ih proizvodstva» M.: VIAM. 2003. S. 116–131.
  7. Sposob poluchenija litogo trubnogo katoda iz splavov na osnove aljuminija dlja ionno-plazmennogo nanesenija pokrytij [Way of receiving the cast pipe cathode from alloys on the basis of aluminum for ion-plasma drawing coverings]: pat. 2340426 Ros. Federacija; opubl. 16.04.2007.
  8. Sposob poluchenija lityh trubnyh izdelij iz splavov na osnove nikelja i/ili kobal'ta [Way of receiving cast tubular goods from alloys on the basis of nickel and/or cobalt]: pat. 2344019 Ros. Federacija; opubl. 16.04.2007.
  9. Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [The strategic directions of development of materials and technologies of their processing for the period till 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  10. Kablov E.N., Ospennikova O.G., Bazyleva O.A. Materialy dlja vysokoteplonagruzhennyh detalej gazoturbinnyh dvigatelej [Materials for the high-heatloaded details of gas turbine engines] //Vestnik MGTU im. N.Je. Baumana. Ser. «Mashinostroenie». 2011. №SP2. S. 13–19.
  11. Ustanovka dlja nanesenija zashhitnyh pokrytij [Installation for drawing protecting covers]: pat. 2318078 Ros. Federacija; opubl. 26.06.2006.
  12. Kashapov O.S., Pavlova T.V., Nochovnaja N.A. Vlijanie rezhimov termicheskoj obrabotki na strukturu i svojstva zharoprochnogo titanovogo splava dlja lopatok KVD [Influence of modes of thermal processing on structure and property of heat resisting titanium alloy for KVD blades] //Aviacionnye materialy i tehnologii. 2010. №2. S. 8–14.
  13. Splav na osnove titana [Titanium-based alloy]: pat. 2426808 Ros. Federacija; opubl. 20.08.2011.
  14. Sibileva S.V., Karimova S.A. Obrabotka poverhnosti titanovyh splavov s cel'ju obespechenija adgezionnyh svojstv [Surface treatment of titanium alloys for the purpose of ensuring adhesive properties] //Aviacionnye materialy i tehnologii. 2013. №S2. S. 25–35.
  15. Mubojadzhjan S.A. Osobennosti osazhdenija iz dvuhfaznogo potoka mnogokomponentnoj plazmy vakuumno-dugovogo razrjada, soderzhashhego mikrokapli isparjaemogo materiala [Features of sedimentation from diphasic flow of multicomponent plasma of the vacuum arc discharge containing microdrops of evaporated material] //Metally. 2008. №2. C. 20–34.
  16. Mubojadzhjan S.A., Aleksandrov D.A., Gorlov D.S. Nanoslojnye uprochnjajushhie pokrytija dlja zashhity stal'nyh i titanovyh lopatok kompressora GTD [Nanolayer strengthening coverings for protection of steel and titanic compressor blades of GTD] //Aviacionnye materialy i tehnologii. 2011. №3. S. 3–8.
  17. Mubojadzhjan S.A., Aleksandrov D.A., Gorlov D.S. i dr. Zashhitnye i uprochnjajushhie ionno-plazmennye pokrytija dlja lopatok i drugih otvetstvennyh detalej kompressora GTD [Protective and strengthening ion-plasma coverings for blades and other responsible details of the GTD compressor] //Aviacionnye materialy i tehnologii. 2012. №S. S. 71–81.
  18. Kablov E.N., Mubojadzhjan S.A., Budinovskij S.A., Pomelov Ja.A. Ionno-plazmennye zashhitnye pokrytija dlja lopatok gazoturbinnyh dvigatelej [Ion-plasma protecting covers for blades of gas turbine engines] //Konversija v mashinostroenii. 1999. №2. S. 42–47.
  19. Muboyadzhyan S.A., Kablov E.N. Vacuum plasma technique of protective coatings pro-duction of complex alloys //МiТОМ. 1995. №2. С. 15–18.
  20. Kablov E.N., Mubojadzhjan S.A., Budinovskij S.A., Lucenko A.N. Ionno-plazmennye zashhitnye pokrytija dlja lopatok gazoturbinnyh dvigatelej [Ion-plasma protecting covers for blades of gas turbine engines] //Metally. 2007. №5. S. 23–34.
  21. Kablov E.N., Ospennikova O.G., Vershkov A.V. Redkie metally i redkozemel'nye jelementy – materialy sovremennyh i budushhih vysokih tehnologij [Rare metals and rare earth elements – materials of modern and future high technologies] //Trudy VIAM. 2013. №2. St. 01 (viam-works.ru).
  22. Kablov E.N., Mubojadzhjan S.A. Ionnoe travlenie i modificirovanie poverhnosti otvetstvennyh detalej mashin v vakuumno-dugovoj plazme [Ion etching and modifying of surface of responsible details of machines in vacuum and arc plasma] //Vestnik MGTU im. N.Je. Baumana. Ser. «Mashinostroenie». 2011. №SP2. S. 149–163.
  23. Becofen S.Ja., Smirnov V.G., Ashmarin A.A., Shaforostov A.A. Kolichestvennye metody opisanija tekstury i anizotropii svojstv splavov na osnove titana i magnija [Quantitative methods of the description of structure and anisotropy of properties of titanium-based alloys and magnesium] //Titan. 2010. №2. S. 16–22.
  24. Ustinov A.I., Movchan B.A., Skorodzievskij V.S. Issledovanie dempfirujushhej sposobnosti ploskih obrazcov iz titanovogo splava Ti–6%Al–4%V s pokrytijami iz olova i ittrija [Research of damping capacity of flat samples from Ti–6%Al–4%V titanium alloy with coverings from tin and yttrium] //Problemy prochnosti. 2001. №4. S. 55–61.
  25. Ustinov A.I. Dissipativnye svojstva nanostrukturirovannyh materialov [Dissipative properties of the nanostructured materials] //Problemy prochnosti. 2008. №5. S. 96–104.