Heat treatment influence on characteristics of welding joints of high-strength aluminum-lithium alloys

Lukin V.I., Ioda E.N., Panteleev M.D., Skupov A.A.
Lukin V.I., Ioda E.N., Panteleev M.D., Skupov A.A. Heat treatment influence on characteristics of welding joints of high-strength aluminum-lithium alloys // Proceedings of VIAM. 2015. No. 4. DOI: 10.18577/2307-6046-2015-0-4-6-6. URL: https://www.viam-works.ru/en/journal/2015/4/6
Abstract

It was determined that the maximum level of strength is achieved after full heat treatment (quenching and artificial ageing) after welding. Heat treatment of welded joints made by friction stir welding leads to structural heterogeneity alignment and removal of weakening of the heat affected zone. After-welding modes of heat treatment do not practically influence the protective properties of non-metallic inorganic coatings.

Reference list
  1. Kablov E.N., Lukin V.I., Ospennikova O.G. Perspektivnye aljuminievye splavy i tehnologii ih soedinenija dlja izdelij aviakosmicheskoj tehniki [Perspective aluminum alloys and technologies of their connection for products of aerospace equipment] /V sb. Tezisov dokladov II Mezhdunarodnoj konf. «Aljuminij–21/Svarka i pajka». 2012. S. 8.
  2. Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace materials science] //Vse materialy. Jenciklopedicheskij spravochnik. 2008. №3. S. 2–14.
  3. Kablov E.N. Sovremennye materialy – osnova innovacionnoj modernizacii Rossii [Modern materials – basis of innovative modernization of Russia] //Metally Evrazii. 2012. №3. S. 10–15.
  4. Panin V.E., Kablov E.N., Pochivalov Ju.I., Panin S.V., Kolobnev N.I. Vlijanie nanostrukturirovanija poverhnostnogo sloja aljuminij-litievogo splava 1424 na mehanizmy deformacii, tehnologicheskie harakteristiki i ustalostnuju dolgovechnost'. Povyshenie plastichnosti i tehnologicheskih harakteristik [Influence of nanostructuring surface layer aluminum-lithium alloy 1424 on deformation mechanisms, technical characteristics and fatigue life. Increase of plasticity and technical characteristics] //Fizicheskaja mezomehanika. 2012. T. 15. №6. S. 107–111.
  5. Antipov V.V., Senatorova O.G., Tkachenko E.A., Vahromov R.O. Aljuminievye deformiruemye splavy [Aluminum deformable alloys] //Aviacionnye materialy i tehnologii. 2012. №S. S. 167–182.
  6. Fridljander I.N., Chuistov K.V., Berezina A.L., Kolobnev N.I., Koval' Ju.N. Aljuminij-litievye splavy. Struktura i svojstva [Aluminum-lithium alloys. Structure and properties]. K.: Naukova dumka. 1992.
  7. Fridlyander I.N., Sister V.G., Grushko O.E., Berstenev V.V., Sheveleva L.M., Ivanova L.A. Aluminum alloys: promising materials in the automotive industry //Metal Science and Heat Treatment. 2002. Т. 44. №9–10. P. 365–370.
  8. Klochkova Ju.Ju., Grushko O.E., Lancova L.P., Burljaeva I.P., Ovsjannikov B.V. Osvoenie v promyshlennom proizvodstve polufabrikatov iz perspektivnogo aljuminijlitievogo splava V-1469 [Development in industrial production of semi-finished products from perspective alyuminiylitiyevy alloy V-1469] //Aviacionnye materialy i tehnologii. 2011. №1. S. 8–12.
  9. Klochkov G.G., Grushko O.E., Klochkova Ju.Ju., Romanenko V.Ju. Promyshlennoe osvoenie vysokoprochnogo splava V-1469 sistemy Al–Cu–Li–Mg [Industrial development of V-1469 high-strength alloy of Al–Cu–Li–Mg system] //Trudy VIAM. 2014. №7. St. 01 (viam-works.ru).
  10. Samorukov M.L. Analiticheskij podhod k matematicheskomu modelirovaniju temperaturnoj sostavljajushhej rotacionnoj svarki treniem [Analytical approach to mathematical modeling of temperature component of rotational friction bonding] //Trudy VIAM. 2013. №9. St. 03 (viam-works.ru).
  11. Lukin V.I., Ospennikova O.G., Ioda E.N., Panteleev M.D. Svarka aljuminievyh splavov v aviakosmicheskoj promyshlennosti [Welding of aluminum alloys in the aerospace industry] //Svarka i diagnostika. 2013. №2. S. 47–52.
  12. Lukin V.I., Ioda E.N., Bazeskin A.V. i dr. Povyshenie nadezhnosti svarnyh soedinenij iz vysokoprochnogo aljuminievo-litievogo splava V-1461 [Increase of reliability of welded connections from high-strength aluminum-lithium alloy V-1461] //Svarochnoe proizvodstvo. 2010. №11. S. 14–17.
  13. Petrovic M., Veljic D., Rakin M., Radovic N., Sedmak A., Bajic N. Friction-stir welding of high-strength aluminium alloys and a numerical simulation of plunge stage //Materials in technology. 2012. V. 46. №3. P. 215–221.
  14. Silis M.I., Eliseev A.A., Silis V.Je. i dr. Osobennosti struktury svarnyh soedinenij aljuminievyh splavov, poluchennyh frikcionnoj svarkoj [Features of structure of welded compounds of the aluminum alloys received by frictional welding] //MiTOM. 2009. №4. S. 34–39.
  15. Lukin V.I., Ioda E.N., Bazeskin A.V. i dr. Osobennosti formirovanija svarnogo soedinenija pri svarke treniem s peremeshivaniem aljuminievogo splava V-1469 [Features of forming of welded connection at friction bonding with V-1469 aluminum alloy hashing] //Svarochnoe proizvodstvo. 2012. №6. S. 30–36.
  16. Antipov V.V., Kolobnev N.I., Hohlatova L.B. Razvitie aljuminijlitievyh splavov i mnogostupenchatyh rezhimov termicheskoj obrabotki [Development of alyuminiylitiyevy alloys and multistage modes of thermal processing] //Aviacionnye materialy i tehnologii. 2012. №S. S. 183–195.
  17. Oglodkov M.S., Hohlatova L.B., Kolobnev N.I. i dr. Vlijanie termomehanicheskoj obrabotki na svojstva i strukturu splava sistemy Al–Cu–Mg–Li–Zn [Influence of thermomechanical processing on properties and Al–Cu–Mg–Li–Zn system alloy structure] //Aviacionnye materialy i tehnologii. 2010. №4. S. 7–11.
  18. Zhilikov V.P., Karimova S.A., Leshko S.S., Chesnokov D.V. Issledovanie dinamiki korrozii aljuminievyh splavov pri ispytanii v kamere solevogo tumana (KST) [Research of dynamics of corrosion of aluminum alloys when testing in the salt spray chamber (KST)] //Aviacionnye materialy i tehnologii. 2012. №4. S. 18–22.