Electrical resistivity of pure titanium after severe plastic deformation as a function of temperature

Berezovsky V.V., Bazaleeva O.K., Kalashnikov V.S.
Berezovsky V.V., Bazaleeva O.K., Kalashnikov V.S. Electrical resistivity of pure titanium after severe plastic deformation as a function of temperature // Proceedings of VIAM. 2015. No. 3. DOI: 10.18577/2307-6046-2015-0-3-5-5. URL: https://www.viam-works.ru/en/journal/2015/3/5
Abstract

A temperature dependence of the electrical resistivity of commercially pure titanium after severe plastic deformation was shown as a function of temperature within the range of -100/+100°С. A temperature dependence of electrical resistivity of commercially pure titanium in annealed state was offered as a measurement control technique.

Reference list
  1. Kablov E.N. Strategicheskie napravlenii razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [Strategic directions of development of materials and technologies to process them for the period up to 2030] //Aviacionnye materialy i tehnologii. 2012. №S. C. 7–17.
  2. Kablov E.N., Shhetanov B.V., Grashhenkov D.V. i dr. Metallomatrichnye kompozicionnye mate-rialy na osnove Al‒SiC [Metal matrix composites based on Al–SiC] //Aviacionnye materialy i tehnologii. 2012. №S. S. 373–380.
  3. Kablov E.N. Aviakosmicheskoe materialovedenie [Aerospace materials] //Vse materialy. Jenciklopedicheskij spravochnik. 2008. №3. S. 2–14.
  4. Krasnov E.I., Shtejnberg A.S., Shavnev A.A., Berezovskij V.V. Issledovanie sloistogo metallicheskogo kompozicionnogo materiala sistemy Ti–TiAl3 [Investigation metal laminate composite systems Ti–TiAl3] //Aviacionnye materialy i tehnologii. 2013. №3. S. 16–19.
  5. Grinevich A.V., Lucenko A.N., Karimova S.A. Raschetnye harakteristiki metallicheskih materialov s uchetom vlazhnosti [Design characteristics of metallic materials with the humidity] //Trudy VIAM. 2014. №7. Ct. 10 (viam-works.ru).
  6. Kablov E.N., Grashhenkov D.V., Shhetanov B.V. i dr. Metallicheskie kompozicionnye materialy na osnove Al–SiC dlja silovoj jelektroniki [Metal composite materials on the basis of Al–SiC power electronics] //Mehanika kompozicionnyh materialov i konstrukcij. 2012. T. 2. №3. S. 359–368.
  7. Grishina O.I., Kochetov V.N., Shavnev A.A., Serpova V.M. Aspekty primenenija vysokoproch-nyh i vysokomodul'nyh voloknistyh metallicheskih kompozicionnyh materialov aviacionnogo naznachenija (obzor) [Aspects of the use of high-strength and high-fiber metal composites aviation applications (review)] //Trudy VIAM. 2014. №10. St. 05 (viam-works.ru).
  8. Milejko S.T. Kompozity i nanostruktury [Composites and nanostructures] //Kompozity i nanostruktury. 2009. №1. S. 6–37.
  9. Sharkeev Ju.P., Eroshenko A.Ju., Bratchikov A.D. i dr. Struktura i mehanicheskie svojstva nanostrukturirovannogo titana posle dorekristallizacionnyh otzhigov [Structure and mechanical properties of nanostructured titanium after annealing dorekristallizatsionnyh] //Fizicheskaja me-zomehanika. 2005. T. 8. Spec. vyp. S. 91–94.
  10. Kurzina I.A., Kozlov Je.V., Sharkeev Ju.P. i dr. Nanokristallicheskie intermetallidnye i nitridnye struktury, formirujushhiesja pri ionno-plazmennom vozdejstvii [Nanocrystalline intermetallic and nitride structures, which are formed in ion-plasma exposure]. Tomsk: Izd-vo NTL. 2008. 324 s.
  11. Sharkeev Yu.P., Legostaeva E.V., Eroshenko A.Yu. et al. The Structure and Physical and Mechanical Properties of a Novel Biocomposite Material, Nanostructured Titanium-Calcium-Phosphate Coating //Composite Interfaces. 2009. V. 16. P. 535–546.
  12. Eroshenko A.Ju., Sharkeev Ju.P., Tolmachev A.I. i dr. Struktura i svojstva ob#emnogo ul'tramelkozernistogo titana, poluchennogo abc-pressovaniem i prokatkoj [The structure and properties of bulk ultrafine titanium obtained abc-pressing and rolling] //Perspektivnye materialy. 2009. №7. S. 107–112.
  13. Sharkeev Ju.P., Polenichkin V.K. Perspektivy primenenija ul'tramelkozernistogo titana v stomatologii [Prospects for the use of ultrafine titanium in dentistry] //Perspektivnye materialy. 2009. №7. S. 372–377.
  14. Chawla N., Chawla K.K. Metal Matrix Composites /In: Springer Sience+Business Media. 2006. P. 401.
  15. Kablov E.N., Grashchenkov D.V., Isaeva N.V., Solntsev S.St. Perspective high-temperature ceramic composite materials //Russian Journal of General Chemistry. 2011. V. 81. №5. S. 986–991.