Polyimide fiberglass plastic with lower curing temperature

Davydova I.F., Kavun N.S.
Davydova I.F., Kavun N.S. Polyimide fiberglass plastic with lower curing temperature // Proceedings of VIAM. 2015. No. 2. DOI: 10.18577/2307-6046-2015-0-2-8-8. URL: https://www.viam-works.ru/en/journal/2015/2/8
Abstract

The research was focused on modification of the polyimide binding material SP-97s. The character of transformations in the binder, which contents modifying additives of different types, was studied on the stage of material forming. The optimum amount of modifiers was determined and effectiveness of each of them with the purpose to decrease curing temperature of binder down to 170°C was estimated taking into account the properties of fiberglass plastics. The composition of modifying binder was established, polyimide fiberglass plastic STP-97K was developed and its properties were studied. It was demonstrated that lowering of the curing temperature does not cause a significant change of properties of the material in different operational conditions.

Reference list
  1. Poliimidnye kompozicionnye materialy: struktura, svojstva, tehnologija [Polyimide composites: Structure, properties and technology] /Pod obshh. red. A.A. Berlina. SPb.: Professija. 2008. 512 s.
  2. Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [Strategic directions of development of materials and technologies to process them for the period up to 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  3. Barbot'ko S.L. Pozharobezopasnost' aviacionnyh materialov [Fire safety of aviation materials] //Aviacionnye materialy i tehnologii. 2012. №S. S. 431–439.
  4. Davydova I.F., Kablov E.N., Kavun N.S. Termostojkie negorjuchie poliimidnye steklotekstolity dlja izdelij aviacionnoj i raketnoj tehniki [Heat-resistant polyimide incombustible Fiberglass products for the aviation and rocketry] //Vse materialy. Jenciklopedicheskij spravochnik. 2009. №7. S. 2–11.
  5. Mihajlin Ju.A. Termoustojchivye polimery i polimernye materialy [Thermostable polymers and polymeric materials]. SPb.: Professija. 2006. 256 s.
  6. Kondratenko A.N., Golubkova T.A. Polimernye kompozicionnye materialy v izdelijah zarubezhnoj raketno-kosmicheskoj tehniki (obzor) [Polymer composite materials in products abroad rocket and space technology (review)] //Konstrukcii iz kompozicionnyh materialov. 2009. №2. S. 24–34.
  7. Guljaev I.N., Vlasenko F.S., Zelenina I.V., Raskutin A.E. Napravlenija razvitija termostojkih ugleplastikov na osnove poliimidnyh i geterociklicheskih polimerov [Direction of the heat-resistant carbon-fiber-based polyimide and heterocyclic polymers] //Trudy VIAM. 2014. №1. St. 04 (viam-works.ru).
  8. Muhametov R.R., Ahmadieva K.R., Chursova L.V., Kogan D.I. Novye polimernye svjazujushhie dlja perspektivnyh metodov izgotovlenija konstrukcionnyh voloknistyh PCM [New polymeric binders for advanced manufacturing methods of structural fiber PCM] //Aviacionnye materialy i tehnologii. 2011. №2. S. 38–42.
  9. Kablov E.N. K 80-letiju VIAM [On the 80th anniversary of VIAM] //Zavodskaja laboratorija. Diagnostika materialov. 2012. T. 78. №5. S. 79–81.
  10. Svetlichnyj V.M., Kudrjavcev V.V. Polimery i problema sozdanija sovremennyh konstrukcionnyh materialov [Polymers and the problem of creation of modern construction materials] //Vysokomolekuljarnye soedinenija. Ser. B. 2003. T. 45. №6. S. 35–39.
  11. Davydova I.F., Kavun N.S. Stekloplastiki – mnogofunkcional'nye kompozicionnye ma-terialy [GRP – multifunctional composite materials] //Aviacionnye materialy i tehnologii. 2012. №S. S. 253–260.
  12. Davydova I.F., Kavun N.S. Stekloplastiki v konstrukcijah aviacionnoj i raketnoj tehniki [GRP in the construction of aircraft and missile technology] //Steklo i keramika. 2012. №4. S. 1–7.
  13. Kablov E.N. Materialy i himicheskie tehnologii dlja aviacionnoj tehniki [Materials and chemical technologies, aircraft] //Vestnik Rossijskoj akademii nauk. 2012. T. 82. №6. S. 520–530.
  14. Poliimidnoe svjazujushhee dlja armirovannyh plastikov, prepreg na ego osnove i izdelie, vypolnennoe iz nego [Polyimide binder for reinforced plastics, the prepreg and it is based on a product made of it]: pat. №2394857 Ros. Federacija; opubl. 07.05.2009.
  15. Mihajlin Ju.A. Konstrukcionnye polimernye kompozicionnye materialy [Structural polymer composite materials]. M.: Izd-vo «NOT». 2008. 615 s.
  16. Davydova I.F., Kavun N.S. Issledovanie stojkosti poliimidnogo steklotekstolita STP-97K k agressivnym sredam [Investigation of resistance polyimide fiberglass STP-97K to aggressive environments] //Vse materialy. Jenciklopedicheskij spravochnik. 2011. №9. S. 42–44.
  17. Davydova I.F., Kavun N.S. Ognestojkie stekloplastiki v konstrukcijah motogondol dvigatelej samoletov [Fire-resistant fiberglass structures aircraft engine nacelles] //Vse materialy. Jenciklopedicheskij spravochnik. 2011. №7. S. 16–20.
  18. Vavilova M.I., Kavun N.S. Svojstva i osobennosti armirujushhih stekljannyh napolnitelej, ispol'zuemyh dlja izgotovlenija konstrukcionnyh stekloplastikov [Properties and characteristics of reinforcing glass fillers used for the manufacture of structural fiberglass] //Aviacionnye materialy i tehnologii. 2014. №3. S. 33–37.