Study of possibility of determination of high cobalt content in titanium-based alloys by photometric method

Goundobin N.V., Titov V.I., Pilipenko L.V.
Goundobin N.V., Titov V.I., Pilipenko L.V. Study of possibility of determination of high cobalt content in titanium-based alloys by photometric method // Proceedings of VIAM. 2015. No. 2. DOI: 10.18577/2307-6046-2015-0-2-6-6. URL: https://www.viam-works.ru/en/journal/2015/2/6
Abstract

A possibility of photometric determination of cobalt content in titanium-based alloys within the concentration range of 6–12% mass. was studied. Ethylene diamine (EDA) was used as reactant. The studies were focused on factors of stability in time and selectivity of the reaction of Co with EDA and its influence on light absorption of EDA in combination with some elements contained in the alloys, which form colored EDA (Ni, Cu, Cr) or colorless (Zn, Mo, V, Sn) soluble complexes. It was established that the color of a complex with EDA was stable within several hours. Reaction sensitivity is 0.1 microgram of Co in 1 milliliter of solution. The light absorption of cobalt has its maximum at λ=360 nm. In order to prevent precipitation of titanium, potassium pyrophosphate was applied, since it forms with titanium soluble complexes, which do not affect changes in optical density of Co+EDA complex. This work resulted in the development of a technique for a direct photometric determination of hig

Reference list
  1. Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih perera-botki na period do 2030 goda [Strategic directions of development of materials and technologies to process them for the period up to 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  2. Kablov E.N. Sovremennye materialy – osnova innovacionnoj modernizacii Rossii [Modern materials – the basis of innovative modernization of Russia] //Metally Evrazii. 2012. №3. S. 10–15.
  3. Kablov E.N. K 80-letiju VIAM [On the 80th anniversary of VIAM] //Zavodskaja laboratorija. Diagnostika materialov. 2012. T. 78. №5. S. 79–82.
  4. Horev A.I., Belov S.P., Glazunov S.G. Metallovedenie titana i ego splavov [Physical metallurgy of titanium and its alloys]. M.: Metallurgija. 1992. 352 s.
  5. Antashev V.G., Nochovnaja N.A., Shirjaev A.A., Izotova A.Ju. Perspektivy razrabotki novyh titanovyh splavov [Prospects for the development of new titanium alloys] //Vestnik MGTU im. N.Je. Baumana. Ser. «Mashinostroenie». 2011. №S2. S. 60–67.
  6. Nochovnaja N.A., Ivanov V.I., Alekseev E.B., Kochetkov A.S. Puti optimizacii jekspluatacionnyh svojstv splavov na osnove intermetallidov titana [Ways to optimize the performance properties of intermetallic alloys based on titanium] //Aviacionnye materialy i tehnologii. 2012. №S. S. 196–206.
  7. Nochovnaja N.A., Alekseev E.B., Jasinskij K.K., Kochetkov A.S. Specifika plavki i sposoby poluchenija slitkov intermetallidnyh titanovyh splavov s povyshennym soderzhaniem niobija [Specificity of fusion and methods for producing ingots of titanium intermetallic alloys with higher niobium content] //Vestnik MGTU im. N.Je. Baumana. Ser. «Mashinostroenie». 2011. №S2. S. 53–59.
  8. Nochovnaja N.A., Skvorcova S.V., Anishhuk D.S., Alekseev E.B., Panin P.V., Umarova O.Z. Otrabotka tehnologii poluchenija opytnogo zharoprochnogo splava na osnove intermetallida Ti2AlNb [Development of the technology for producing test superalloy based intermetallic Ti2AlNb] //Titan. 2013. №4. S. 24–29.
  9. Nochovnaja N.A., Antashev V.G., Shirjaev A.A., Alekseev E.B. Issledovanie vlijanija rezhimov izotermicheskogo deformirovanija i termicheskoj obrabotki na strukturu i mehanicheskie svojstva opytnogo zharoprochnogo Ti-splava [The study on the effect of isothermal deformation and heat treatment on the structure and mechanical properties of Ti-experienced heat-resistant alloy] //Tehnologija legkih splavov. 2012. №4. S. 92–98.
  10. Horev A.I. Fundamental'nye i prikladnye raboty po konstrukcionnym titanovym splavam i perspektivnye napravlenija ih razvitija [Fundamental and applied research in structural titanium alloys and future directions of their development] //Trudy VIAM. 2013. №2. St. 04 (viam-works.ru).
  11. Kashapov O.S., Novak A.V., Nochovnaja N.A., Pavlova T.V. Sostojanie, problemy i perspektivy sozdanija zharoprochnyh titanovyh splavov dlja detalej GTD [Status, problems and prospects of creating heat-resistant titanium alloys for GTD parts] //Trudy VIAM. 2013. №3. St. 02 (viam-works.ru).
  12. Nochovnaja N.A., Panin P.V., Kochetkov A.S., Bokov K.A. Sovremennye zharoprochnye splavy na osnove gamma-aljuminida titana: perspektivy razrabotki i primenenija [Modern heat-resistant alloys based on gamma titanium aluminide: development and application prospects] //MiTOM. 2014. №7. S. 23–27.
  13. Kablov D.E., Panin P.V., Shirjaev A.A., Nochovnaja N.A. Opyt ispol'zovanija vakuumno-dugovoj pechi ALD VAR L200 dlja vyplavki slitkov zharoprochnyh splavov na osnove aljuminidov titana [Experience in the use of vacuum-arc furnace ALD VAR L200 for melting ingots of high-temperature alloys based on titanium aluminides] //Aviacionnye materialy i tehnologii. 2014. №2. S. 27–33.
  14. Nochovnaja N.A., Panin P.V. Analiz ostatochnyh makronaprjazhenij v svarnyh soedinenijah titanovyh splavov raznyh klassov [Analysis of residual macroscopic stresses in welded joints of titanium alloys of different classes] //Trudy VIAM. 2014. №5. St. 02 (viam-works.ru).
  15. Panin P.V., Shirjaev A.A., Dzunovich D.A. Postroenie temperaturno-koncentracionnoj diagrammy fazovogo sostava titanovogo splava VT6, dopolnitel'no legirovannogo vodorodom [Construction of the temperature-concentration phase diagram of the titanium alloy BT6 additionally doped with hydrogen] //Tehnologija mashinostroenija. 2014. №3. S. 5–9.
  16. Il'in A.A., Skvorcova S.V., Dzunovich D.A., Panin P.V., Shalin A.V. Vlijanie parametrov termicheskoj i termomehanicheskoj obrabotki na teksturoobrazovanie v listovyh polufabrikatah iz titanovyh splavov [Influence of parameters of thermal and thermomechanical processing on texture formation in leaf semi-finished products from titanium alloys] //Tehnologija mashinostroenija. 2012. №8. S. 8–12.
  17. Kovtunov A.I., Mjamin S.V. Issledovanie tehnologicheskih i mehanicheskih svojstv sloistyh titanoaljuminievyh kompozicionnyh materialov, poluchennyh zhidkofaznym sposobom [Investigation of processing and mechanical properties titanoalyuminievyh layered composite material obtained by the liquid phase method] //Aviacionnye materialy i tehnologii. 2013. №1. S. 9–13.
  18. OST 90136–96. Splavy nikelevye zharoprochnye. Metody opredelenija kobal'ta [Alloys of nickel superalloys. Methods for determination of cobalt].
  19. Kanaev N.A. Uskorennoe opredelenie redkozemel'nyh metallov v splavah [Fast determination of rare earth metals in alloys]. M.: Metallurgija. 1971. 220 s.
  20. Flashka G.F., Shvarcenbah G.M. Kompleksonometricheskoe titrovanie [Complexometric titrations]. M.: Himija. 1970. 360 s.
  21. Jurist I.M. Polijetilenpoliamin kak maskirujushhij reagent pri kompleksonometricheskom opredelenii svinca [Polyethylenepolyamine as a masking reagent in complexometric determination of lead] //Zavodskaja laboratorija. 1968. T. 34. №5. S. 539–540.