Investigation of an impact of a negative electric potential of the substrate on deposition rate of multicomponent nickel coatings on the surface of cast heat-resistant nickel alloys

Smirnov A.A., Budinovskiy S.A., Matveev P.V.
Smirnov A.A., Budinovskiy S.A., Matveev P.V. Investigation of an impact of a negative electric potential of the substrate on deposition rate of multicomponent nickel coatings on the surface of cast heat-resistant nickel alloys // Proceedings of VIAM. 2015. No. 2. DOI: 10.18577/2307-6046-2015-0-2-5-5. URL: https://www.viam-works.ru/en/journal/2015/2/5
Abstract

An impact of a negative electrical potential (voltage) of the substrate on deposition rate of multicomponent Ni-based coatings produced by the cathodic arc physical vacuum deposition from the surface of cathodes made of nickel-based alloys with additives of chromium, aluminum, tantalum, rhenium, yttrium, hafnium on the surface of specimens of various cast heat-resistant nickel alloys was investigated. It was shown that the maximum etching rate could be achieved in case of applying of 350 V potential to a substrate. The threshold values of spray voltage for all compositions of heat-resistant materials tested in this study were determined. An influence of the chemical composition of the plasma formed in vacuum from the cathode surface on the sputtering threshold was stated depending on the content of chromium and high-melting point elements in the cathode.

Reference list
  1. Plazmennye uskoriteli [Plasma accelerators] /Pod red. L.A. Arcimovicha. M.: Mashinostroenie. 1973. 312 s.
  2. Dorodnov A.M., Petrosov V.A. O fizicheskih principah i tipah vakuumnyh tehnologicheskih plazmennyh ustrojstv [On the physical principles and types of vacuum plasma technology devices] //Zhurnal tehnicheskoj fiziki. 1981. T. 51. №3. S. 504–524.
  3. Grigorov A.I., Dorodnov A.M., Kiselev N.D. Nekotorye fizicheskie osnovy ustanovki PUSK 77-1 dlja nanesenija iznosostojkih pokrytij [Some physical basics of installing START 77-1 for hardfacing] //Tehnologija avtomobilestroenija. 1978. №6. S. 10–15.
  4. Padalka V.G., Tolok V.T. Metody plazmennoj tehnologii vysokih jenergij [Methods of plasma technology of high-energy] //Atomnaja jenergija. 1978. T. 44. №5. S. 476–478.
  5. Ustanovka IJeT-842 («Bulat») [Installing IET-842 («Bulat»)] //Jelektrotehnicheskaja promyshlennost'. Ser. Jelektrotermija. 1980. №3 (211). S. 15–16.
  6. Kimblin S.U. Jerozija jelektrodov i ionizacionnye processy v prijelektrodnyh oblastjah vakuumnyh dug i pri atmosfernom davlenii [Erosion electrodes and ionization processes in the electrode regions of vacuum arcs and at atmospheric pressure] /V kn. Jeksperimental'nye issledovanija plazmotronov. Per. s angl. Novosibirsk: Nauka. 1977. S. 226–253.
  7. Shott L. Jelektricheskie zondy [Electrical probes]. Per. s angl. M.: Mip. 1971. S. 459–505.
  8. Lunev V.M., Ovcharenko V.D., Horoshih V.M. Issledovanie nekotoryh harakteristik plazmy vakuumnoj metallicheskoj dugi. Chast' I [Study of some characteristics of the plasma vacuum arc metal] //Zhurnal tehnicheskoj fiziki. 1977. T. 47. №7. S. 1486–1490.
  9. Aksenov I.I., Padalka V.G., Horoshih V.M. Issledovanie plazmy stacionarnogo vakuumnogo dugovogo razrjada. Chast' II. Vlijanie integral'noj temperatury katoda [Investigation of stationary plasma vacuum arc discharge. Part II. Effect of integrated cathode temperature] //Teplofizika vysokih temperatur. 1983. T. 21. №4. S. 646–651.
  10. Lunev V.M., Padalka V.G., Horoshih V.M. Issledovanie nekotoryh harakteristik plazmy vakuumnoj metallicheskoj dugi [Study of some characteristics of the plasma vacuum arc metal]. Chast' II //Zhurnal tehnicheskoj fiziki. 1977. T. 47. №7. C. 1491–1495.
  11. Aksenov I.I., Padalka V.G., Horoshih V.M. Issledovanie plazmy stacionarnogo vakuumnogo dugovogo razrjada. Chast' I. Formirovanie potokov plazmy [Investigation of stationary plasma vacuum arc discharge. Part I. Formation of plasma flows] //Teplofizika vysokih temperatur. 1983. T. 21. №2. S. 219–223.
  12. Petrushin N.B., Ospennikova O.G., Visik E.M., Rassohina L.I., Timofeeva O.B. Zharoprochnye nikelevye splavy nizkoj plotnosti [Heat-resistant nickel alloys, low density] //Litejnoe proizvodstvo. 2012. №6. S. 5–11.
  13. Gerasimov V.V., Visik E.M., Bakerin S.V. Izgotovlenie protjazhennyh lityh zagotovok iz splava VKNA-1V napravlennoj kristallizaciej [Manufacturing extended cast billets alloy VKNA-1B directional solidification] //Litejnoe proizvodstvo. 2011. №10. S. 36–39.
  14. Povarova K.B., Bazyleva O.A., Drozdov A.A., Alad'ev N.A., Samsonov M.A. Issledovanie malociklovoj ustalosti pri komnatnoj temperature splava na osnove intermetallida Ni3Al tipa VKNA-25 [Investigation of low cycle fatigue at room temperature alloy based on the intermetallic compound Ni3Al type VKNA-25] //Metally. 2012. №6. S. 70–81.
  15. Budinovskij S.A., Mubojadzhjan S.A., Gajamov A.M., Kos'min A.A. Zharostojkie ionno-plazmennye pokrytija dlja lopatok turbin iz nikelevyh splavov, legirovannyh reniem [Heat-resistant ion-plasma coatings for turbine blades of nickel alloys doped with rhenium] //MiTOM. 2008. №6. S. 31–36.
  16. Kuznecov V.P., Lesnikov V.P., Konakova I.P., Petrushin N.V., Mubojadzhjan S.A. Struktura i fazovyj sostav monokristallicheskogo splava VZhM-4 s gazocirkuljacionnym zashhitnym pokrytiem [The structure and phase composition of the single crystal alloy VZHM-4 with a gas circulation protective coating] //MiTOM. 2011. №3. S. 28–32.
  17. Morozova G.I., Timofeeva O.B., Petrushin N.V. Osobennosti struktury i fazovogo sostava vysokorenievogo nikelevogo zharoprochnogo splava [Features of the structure and phase composition vysokorenievogo nickel superalloy] //MiTOM. 2009. №2. S. 10–16.
  18. Kablov E.N., Petrushin N.V., Svetlov I.L., Demonis I.M. Nikelevye litejnye zharoprochnye splavy novogo pokolenija [Casting nickel superalloys new generation] //Aviacionnye materialy i tehnologii. 2012. №S. S. 36–52.
  19. Kablov E.N., Mubojadzhjan S.A. Zharostojkie i teplozashhitnye pokrytija dlja lopatok turbiny vysokogo davlenija perspektivnyh GTD [Heat-resistant and heat-resistant coatings for high-pressure turbine blades promising GTD] //Aviacionnye materialy i tehnologii. 2012. №S. S. 60–70.
  20. Matveev P.V., Budinovskij S.A., Mubojadzhjan S.A., Kos'min A.A. Zashhitnye zharostojkie pokrytija dlja splavov na osnove intermetallidov nikelja [Protective coatings for heat-resistant alloys based on nickel intermetallic] //Aviacionnye materialy i tehnologii. 2013. №2. S. 12–15.
  21. Kablov E.N., Muboyadzhyan S.A. Heat-resistant coatings for the high-pressure turbine blades of promising gtes //Russian metallurgy (Metally). 2012. №1. P. 1–7.
  22. Muboyadzhyan S.A., Kablov E.N. Vacuum plasma technique of protective coatings production of complex alloys //МиТОМ. 1995. №2. С. 15–18.
  23. Kablov E.N., Mubojadzhjan S.A., Budinovskij S.A., Lucenko A.N. Ionno-plazmennye zashhitnye pokrytija dlja lopatok gazoturbinnyh dvigatelej [Ion-plasma protective coatings for gas turbine engine blades] //Metally. 2007. №5. S. 23–34.
  24. Kablov E.N., Gerasimov V.V., Visik E.M., Demonis I.M. Rol' napravlennoj kristallizacii v resursosberegajushhej tehnologii proizvodstva detalej GTD [The role of directional solidification in the resource-saving technology of production of gas-turbine] //Trudy VIAM. 2013. №3. St. 01 (viam-works.ru).
  25. Mubojadzhjan S.A., Lucenko A.N., Aleksandrov D.A., Gorlov D.S. Issledovanie vozmozhnosti povyshenija sluzhebnyh harakteristik lopatok kompressora GTD metodom ionnogo modificirovanija poverhnosti [Possibility of increasing the service characteristics of the compressor blades of GTE ion surface modification] //Trudy VIAM. 2013. №1. St. 02 (viam-works.ru).
  26. Mubojadzhjan S.A., Budinovskij S.A., Gajamov A.M., Smirnov A.A. Poluchenie keramicheskih teplozashhitnyh pokrytij dlja rabochih lopatok turbin aviacionnyh GTD magnetronnym metodom [Preparation of ceramic thermal barrier coatings for turbine blades working GTE magnetron sputtering] //Aviacionnye materialy i tehnologii. 2012. №4. S. 3–8.
  27. Kablov E.N., Mubojadzhjan S.A., Budinovskij S.A., Pomelov Ja.A. Ionno-plazmennye zashhitnye pokrytija dlja lopatok gazoturbinnyh dvigatelej [Ion-plasma protective coatings for gas turbine engine blades] //Konversija v mashinostroenii. 1999. №2. S. 42–47.
  28. Budinovskij S.A., Matveev P.V., Smirnov A.A. Issledovanie zharostojkosti litejnyh zharoprochnyh nikelevyh splavov v oblasti temperatur 1000–1200°C [Investigation of the heat resistance of the casting heat-resistant nickel alloys in the temperature range 1000–1200°C] //Aviacionnaja promyshlennost'. 2014. №2. S. 48–52.
  29. Smirnov A.A., Budinovskij S.A. Analiz jevoljucii normal'nyh naprjazhenij v sisteme «splav–pokrytie» v oblasti temperatur do 1200°C [Analysis of the evolution of normal stresses in the system «alloy-coating» at temperatures up to 1200°C] //Aviacionnye materialy i tehnologii. 2014. №2. S. 8–14.