Abstract

The article describes experience on application of semiproducts made of high-modulus Al–Be–Mg alloys (ABM) in experimental structures. An experimental work on production of the wing spoiler skin from ABM1 alloy for An-72 aircraft was carried out under scientific supervision of Academician I.N. Friedlander and Doctor of Science (Tech.) K.P. Yatsenko at Voskresensk experimental and technological center of VIAM in cooperation with Antonov Design Bureau. A fuselage section from ABM1 alloy was produced together with A.S. Yakovlev Design Bureau. TSNIIMV (now JSC «Composite») produced ABM1 alloy pipe weldments which are used by S.A. Lavochkin Design Bureau for production of solar battery modules of «Venera» spacecraft (from 5 to 16) and «Vega» series.

Reference list
  1. Fridljander I.N., Jacenko K.P., Terent'eva T.E., Hilkovskij-Sergeev N.A. Berillij – material sovremennoj tehniki [Beryllium – the material of modern technology]: Sprav. izd. M.: Metallurgija. 1992. 128 s.
  2. Fridljander I.N., Jacenko K.P., Bykov V.M., Matveev O.V., Molchanova L.V., Fokanov A.N. Berillievo-aljuminievye splavy i ih fiziko-mehanicheskie i jekspluatacionnye svojstva [Beryllium-aluminum alloys, and their physical, mechanical and performance properties] /V sb. tezisov dokladov I Vsesojuznogo soveshhanija «Metalloopticheskie jelementy iz berillija». Kiev. 1985. S. 11–12.
  3. Bogdanov B.V., Proskurjakov G.V., Kolganov I.N., Fokanov A.N. O vozmozhnosti ispol'zovanija splava ABM1 v silovyh konstrukcijah izdelij [The possibility of using the alloy ABM1 in power product design] //Aviacionnaja promyshlennost'. 1988. №8. S. 12.
  4. Fridlyander I.N., Sister V.G., Grushko O.E., Berstenev V.V., Sheveleva L.M., Ivanova L.A. Aluminum alloys: promising materials in the automotive industry //Metal Science and Heat Treatment. 2002. Т. 44. №9–10. P. 365–370.
  5. Fridljander I.N. Berillievye splavy – perspektivnoe napravlenie ajerokosmicheskogo materialovedenija [Beryllium alloys – a promising direction of Aerospace Materials] //Vse materialy. Jenciklopedicheskij spravochnik. 2009. №1. S. 6–10.
  6. Solncev S.S., Rozenenkova V.A., Mironova N.A., Kas'kov V.S. Kompleksnaja sistema zashhity berillija ot okislenija [A comprehensive system of protection against oxidation of beryllium] //Aviacionnye materialy i tehnologii. 2010. №1. S. 12–16.
  7. Rozenenkova V.A., Solncev S.S., Mironova N.A. Kompleksnaja zashhita berillievyh splavov ot okislenija i sublimacii toksichnyh parov berillija [Comprehensive protection against oxidation of beryllium alloys and beryllium sublimation toxic fumes] //Trudy VIAM. 2013. №5. St. 03 (viam-works.ru).
  8. Kablov E.N., Solncev S.S., Rozenenkova V.A., Mironova N.A. Kompozicionnye steklometallicheskie pokrytija dlja zashhity berillija pri vysokih temperaturah [Glass-metal composite coating to protect the beryllium at high temperatures] //Steklo i keramika. 2012. №4. S. 12–15.
  9. Dospehi dlja «Burana». Materialy i tehnologii VIAM dlja MKS «Jenergija–Buran» [Armor for "Buran". Materials and technologies for the ISS VIAM «Energia–Buran»] /Pod obshh. red. E.N. Kablova. M.: Fond «Nauka i zhizn'». 2013. 128 s.
  10. Kas'kov V.S. Berillij – konstrukcionnyj material dlja mnogorazovoj kosmicheskoj sistemy [Beryllium – construction material for reusable space system] //Trudy VIAM. 2013. №3. St. 03 (viam-works.ru).
  11. Fokanov A.N. Izgotovlenie svarnoj konstrukcii iz splava ABM1 [Manufacturing of welded alloy ABM1] //Aviacionnaja promyshlennost'. 1987. №7. S. 60–61.
  12. Fokanov A.N., Kuznecova E.A., Popov V.D., Kurochko R.S. Svarivaemost' splava ABM1 so splavom 1201 [Weldability ABM1 alloy to alloy 1201] //Svarochnoe proizvodstvo. 1984. №1. S. 17–19.
  13. Fokanov A.N., Pastuh M.N., Kurochko R.S. Svarivaemost' splava ABM1 so splavom AMg6 [Weldability of the alloy to alloy ABM1 AMg6] //Svarochnoe proizvodstvo. 1982. №9. S. 22–24.
  14. Kas'kov V.S. Berillij i materialy na ego osnove [Beryllium and materials on its basis] //Aviacionnye materialy i tehnologii. 2012. №S. S. 222–226.
  15. Kablov E.N. Strategicheskie napravlenija razvitija materialov i tehnologij ih pererabotki na period do 2030 goda [Strategic directions of development of materials and technologies to process them for the period up to 2030] //Aviacionnye materialy i tehnologii. 2012. №S. S. 7–17.
  16. Kas'kov V.S., Iljushin V.N., Tebjakin A.V. Stabil'nost' prochnostnyh harakteristik splava VAB-1, poluchennogo suspenzionnym lit'em [The stability of the strength characteristics of the alloy of the PSA-1 prepared by casting a slurry] //Metallurgija mashinostroenija. 2008. №6. S. 44–47.
  17. Antipov V.V., Kolobnev N.I., Hohlatova L.B. Razvitie aljuminijlitievyh splavov i mnogostupenchatyh rezhimov termicheskoj obrabotki [Development alyuminiylitievyh alloys and multi-heat treatment] //Aviacionnye materialy i tehnologii. 2012. №S. S. 183–195.
  18. Fridljander I.N., Chuistov K.V., Berezina A.L., Kolobnev N.I., Koval' Ju.N. Aljuminij-litievye splavy. Struktura i svojstva [Aluminum-lithium alloys. Structure and Properties]. K.: Naukova dumka. 1992.
  19. Antipov V.V., Senatorova O.G., Tkachenko E.A., Vahromov R.O. Aljuminievye deformiruemye splavy [Aluminium wrought alloys] //Aviacionnye materialy i tehnologii. 2012. №S. S. 167–182.
  20. Gorbunov P.Z., Tebjakin A.V. Kriterii ajeromobil'nosti beralmetov – materialov aviakosmicheskoj tehniki [Criteria airmobile beralmetov - aerospace materials]. M.: Poligraf servis. 2008. 84 s.