The ways of increasing in fire safety of fibrous heat insulation materials (review)
UDC
614.814.41:66.045.3
DOI
10.18577/2307-6046-2015-0-12-9-9
Article PDF (Russian)
(633.31 KB)
How to cite
Ivakhnenko Yu.A., Varrik N.M. The ways of increasing in fire safety of fibrous heat insulation materials (review) // Proceedings of VIAM. 2015. No. 12. DOI: 10.18577/2307-6046-2015-0-12-9-9. URL: https://www.viam-works.ru/en/journal/2015/12/9
Keywords
thermal insulation, fire barrier, fire blocking, acoustical insulation mat, fire barrier film laminate, heat-resistant fiber.
Abstract
The article contains the review and analysis of methods of increasing in fire safety of fibrous thermal insulation. Permanent growing requirements to service properties of heat-insulating materials are caused by the progress in such areas of the industry, as transport, aviation, energy, chemical, oil-extracting and others, and also need of providing operation safety of machines and mechanisms. A number of new heat-insulating systems is developed for implementation of fire safety requirements of new aviation rules. New types of protective coatings meeting the modern requirements of aviation rules are developed.
Reference list
- Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative developments of FSUE «VIAM» SSC of RF on realization of «Strategic directions of the development of materials and technologies of their processing for the period until 2030»] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
- Kablov E.N. Materialy dlya izdeliya «Buran» – innovacionnye resheniya formirovaniya shestogo tehnologicheskogo uklada [Materials for «Buran» spaceship – innovative solutions of formation of the sixth technological mode] //Aviacionnye materialy i tehnologii. 2013. №S1. S. 3–9.
- Strelnikov S.V., Zastrogina O.B., Veshkin E.A., Shvets N.I. K voprosu o sozdanii vysokoeffektivnyh tehnologij izgotovleniya panelej interera v krupnoserijnom proizvodstve [To a question of creation of highly effective manufacturing techniques of panels of an interior in a large-lot production] //Aviacionnye materialy i tehnologii. 2011. №4. S. 18–24.
- Ivahnenko Yu.A., Babashov V.G., Zimichev A.M., Tinyakova E.V. Vysokotemperaturnye teploizolyacionnye i teplozashhitnye materialy na osnove volokon tugoplavkih soedinenij [High-temperature heat insulating and heat-protective materials on the basis of fibers of high-melting connections] //Aviacionnye materialy i tehnologii. 2012. №S. S. 380–386.
- Kablov E.N., Shchetanov B.V., Ivahnenko Yu.A., Balinova Yu.A. Perspektivnye armiruyushhie vysokotemperaturnye volokna dlya metallicheskih i keramicheskih kompozicionnyh materialov [Perspective reinforcing high-temperature fibers for metal and ceramic composite materials] //Trudy VIAM. 2013. №2. St. 05 (viam-works.ru).
- Aviacionnye pravila AP-25. Normy letnoj godnosti samoletov transportnoj kategorii [Aviation rules AP-25. Standards of the flight validity of airplanes of transport category]. M.: Letno-issled. in-t im. M.M. Gromova. 1994. 321 s.
- Varrik N.M. Termostojkie volokna i teplozvukoizolyacionnye ognezashhitnye materialy [Heat-resistant fibers and heat and sound insulating fireproof materials] //Trudy VIAM. 2014. №6. St. 07 (viam-works.ru).
- Burn through resistant systems for transportation, especially aircraft: pat. 6565040 US; publ. 20.05.2003.
- Composite laminate for a thermal and acoustic insulation blanket: pat. 8292027 US; publ. 23.10.2012.
- Fire barrier film laminate: pat. 7767597 US; publ. 03.08.2010.
- Modularized insulation systems, apparatus and methods: pat. 7083147 US; publ. 01.08.2006.
- Laminate sheet material for fare barrier applications: pat. 6670291 US; publ. 30.12.2003.
- Flexible composite multiple layer fire resistant insulation structure: pat. 8062985 US; publ. 22.11.2011.
- Balinova Yu.A., Kirienko T.A. Nepreryvnye vysokotemperaturnye oksidnye volokna dlya teplozashhitnyh, teploizolyacionnyh i kompozicionnyh materialov [Continuous high-temperature oxide fibers for heat-protective, heatinsulating and composite materials] //Vse materialy. Enciklopedicheskij spravochnik. 2012. №4. S. 24–29.
- Sposob polucheniya vysokotemperaturnogo volokna na osnove oksida alyuminiya [Way of receiving high-temperature fiber on the basis of aluminum oxide]: pat. 2212388 Ros. Federatsiya; opubl. 20.09.2003. Byul. №34. 6 s.
- Aviacionnye materialy: Spravochnik v 12-ti tomah. T. 9. Teplozashhitnye, teploizoljacionnye i kompozicionnye materialy, vysokotemperaturnye nemetallicheskie pokrytiya [Aviation materials: The directory in 12 vol. Vol. 9. Heat-protective, heat insulating and composite materials, high-temperature nonmetallic coatings]. M.: VIAM. 2011. S. 31.
- Babashov V.G., Warrik N.M. Vysokotemperaturnyj gibkij voloknistyj teploizolyacionnyj material [High-temperature flexible fibrous insulation material] //Trudy VIAM. 2015. №1. St. 03 (viam-works.ru).
- Ivahnenko Yu.A., Kuzmin V.V., Bespalov A.S. Sostoyanie i perspektivy razvitiya teplozvukoizolyacionnyh pozharobezopasnyh materialov [Condition and perspectives of development of heat sound-proof fireproof materials] //Problemy bezopasnosti poletov. 2014. №7. S. 27–30.
- Zimichev A.M., Warrik N.M. K voprosu primeneniya diskretnyh volokon iz tugoplavkih oksidov dlya formirovaniya serdechnika termostojkih uplotnitelnyh shnurov [On the issue of application of discrete fibers of refractory oxides to form cores of heat-resistant sealing cords] //Trudy VIAM. 2015. №2. St. 07 (viam-works.ru).