Titov V.I., Goundobin N.V., Pilipenko L.V.
Titov V.I., Goundobin N.V., Pilipenko L.V. Development of a method for determination of phosphorus in the solder VPr18 // Proceedings of VIAM. 2015. No. 11. DOI: 10.18577/2307-6046-2015-0-11-11-11. URL: https://www.viam-works.ru/en/journal/2015/11/11
Abstract

In this paper, the possibility for determination of small amounts of phosphorous in the lead-based VPr18 solder used for soldering wires is shown. Small amounts of phosphorous additives can improve corrosion resistance and strength of the material. Thus solder can operate up to temperatures of 270°C. Welding and solder quality depend on the solder composition by major alloying and impurity elements. In this connection it is necessary to clearly regulate the chemical composition of solders and control the content of chemical elements in their composition. A method of determination of small amounts (0,007 wt. %) of phosphorus in the solder VPr18 was developed. When the content of of phosphorus in the the solder material is large it is necessary to build another calibration graph.

Reference list
  1. Rylnikov V.S., Lukin V.I. Pripoi, primenyaemye dlya pajki materialov aviacionnogo naznacheniya [Solders used for soldering materials aviation application] //Trudy VIAM. 2013. №8. St. 02 (viam-works.ru).
  2. Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative development of FSUE «VIAM» SSC of RF on realization of «Strategic directions of development of materials and technologies of their processing for the period until 2030»] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
  3. Kablov E.N., Mubojadzhjan S.A. Zharostojkie i teplozashhitnye pokrytiya dlya lopatok turbiny vysokogo davleniya perspektivnyh GTD [Heat-resistant and heat-shielding coverings for shovels of the turbine of a high pressure of perspective GTE] //Aviacionnye materialy i tehnologii. 2012. №S. S. 60–70.
  4. Kablov E.N., Bondarenko Ju.A., Echin A.B., Surova V.A. Razvitie processa napravlennoj kristallizacii lopatok GTD iz zharoprochnyh splavov s monokristallicheskoj i kompozicionnoj strukturoj [Development of process of the directed crystallization of shovels of GTE of heat resisting alloys with single-crystal and composite structure] //Aviacionnye materialy i tehnologii. 2012. №1. S. 3–8.
  5. Kablov E.N., Evgenov A.G., Rylnikov V.S., Afanasev-Hodykin A.N. Issledovanie melkodispersnyh poroshkov pripoev dlya diffuzionnoj vakuumnoj pajki, poluchennyh metodom atomizacii rasplava [Research of fine powders of the solders for the diffusive vacuum soldering received by a fusion atomization method] //Vestnik MGTU im. N.Je. Baumana. Ser. «Mashinostroenie». 2011. №SP2. S. 79–87.
  6. Sorokin L.I. Svarivaemost zharoprochnyh splavov, primenjaemyh v aviacionnyh gazoturbinnyh dvigatelyah [The weldability of the heat resisting alloys applied in aviation gas-turbine engines] //Svarochnoe proizvodstvo. 1997. №4. S. 4–11.
  7. Lukin V.I., Semenov V.N., Starova L.L. i dr. Obrazovanie gorjachih treshhin pri svarke zharoprochnyh splavov [Formation of hot cracks when welding heat resisting alloys] //MiTOM. 2007. №12. S. 7–14.
  8. Rylnikov V.S. Voprosy po pajke, reshennye v processe izgotovleniya izdeliya «Buran» [Some problems of brazing solved in the course of manufacture of «Buran» reusable spaceship] //Aviacionnye materialy i tehnologii. 2013. №S1. S. 33–34.
  9. Lukin V.I., Banas I.P., Kovalchuk V.G., Golev E.V. Argono-dugovaja svarka vysokoprochnoj cementuemoj stali VNS-63 [TIG welding of high-strengthened cemented steel VNS-63] //Trudy VIAM. 2013. №8. St. 01 (viam-works.ru).
  10. Afanasev-Hodykin A.N., Lukin V.I., Rylnikov V.S. Vysokotehnologichnye polufabrikaty zharoprochnyh pripoev (lenty i pasty na organicheskom svyazujushhem) [Hi-tech semi-finished high-temperature solders (tape and paste on an organic)] //Trudy VIAM. 2013. №9. St. 02 (viam-works.ru).
  11. Rylnikov V.S., Afanasev-Hodykin A.N., Galushka I.A. Tehnologiya pajki konstrukcii tipa «blisk» iz raznoimennyh splavov [Technology of braze design type «blisk» from dissimilar alloys] //Trudy VIAM. 2013. №10. St. 02 (viam-works.ru).
  12. Rylnikov V.S., Afanasev-Hodykin A.N., Krasikov M.I. Issledovanie remontnoj tehnologii ispravleniya defektov pajanyh soedinenij toplivnyh kollektorov [Research of repair technology of defects correction of soldered joints of fuel collector] //Trudy VIAM. 2013. №12. St. 02 (viam-works.ru).
  13. Khorunov V.F., Maksimova S.V. Paika zharoprochnykh splavov na sovremennom etape [The soldering of hot strength alloys at the present stage] //Svarochnoe proizvodstvo. 2010. №10. S. 24–27.
  14. Lukin V.I., Banas I.P., Kovalchuk V.G., Golev E.V. Argono-dugovaya svarka visokoprochnoi cementuemoy staly VNS-63 [Argon-arc welding of high-strength VNS-63 cemetey steel] // Trudy VIAM. 2013. №8. St. 01 (viam-works.ru).
  15. Krivusha L.S., Sukhomlin M.M., Vorobev G.M. Problema kachestva payanykh soedineniy I razrabotka pripoev [Problem of quality of sweated connections and development of solders] //Avtomatocheskaya svarka. 2005. №3. S. 48–53.