Development of the measurement procedure for determination of mass fraction of surface and dissolved hydrogen in aluminum and low aluminum alloys by heating in inert gas argon
UDC
669.715:669.788
DOI
10.18577/2307-6046-2015-0-11-8-8
Article PDF (Russian)
(531.2 KB)
How to cite
Mekhanik E.A., Rastegayeva G.Yu. Development of the measurement procedure for determination of mass fraction of surface and dissolved hydrogen in aluminum and low aluminum alloys by heating in inert gas argon // Proceedings of VIAM. 2015. No. 11. DOI: 10.18577/2307-6046-2015-0-11-8-8. URL: https://www.viam-works.ru/en/journal/2015/11/8
Abstract
Investigation of simultaneous determination of content of surface and dissolved hy-drogen in aluminum and low aluminum alloys was provided by method of heating in an inert gas of argon in electrode impulse furnace of analyzer Leco RHEN-602 followed by detection in the conductivity cell. Operation modes of electrode impulse furnace, allowing complete extraction of surface hydrogen at the first step, and then extraction of dissolved hydrogen from aluminum and low aluminum alloy, were chosen. The measurement procedure was developed using the results of the determination of surface and dissolved hydrogen in different aluminum alloys.
Reference list
- Kablov E.N. Osnovnye itogi i napravleniya razvitiya materialov dlya perspektivnoj aviacionnoj tehniki [The main results and the directions of development of materials for the perspective aircraft equipment] /V sb. 75 let. Aviacionnye materialy. Izbrannye trudy «VIAM» 1932–2007: Jubilejnyj nauch.-tehnich. sb. M.: VIAM. 2007. S. 20–26.
- Kablov E.N. Innovacionnye razrabotki FGUP «VIAM» GNC RF po realizacii «Strategicheskih napravlenij razvitiya materialov i tehnologij ih pererabotki na period do 2030 goda» [Innovative development of FSUE «VIAM» SSC of RF on realization of «Strategic directions of development of materials and technologies of their processing for the period until 2030»] //Aviacionnye materialy i tehnologii. 2015. №1 (34). S. 3–33.
- Kornysheva I.S., Volkova E.F., Goncharenko E.S., Muhina I.Ju. Perspektivy primeneniya magnievyh i litejnyh alyuminievyh splavov [Prospects of application of magnesian and foundry aluminum alloys] //Aviacionnye materialy i tehnologii. 2012. №S. S. 212–222.
- Antipov V.V. Strategiya razvitiya titanovyh, magnievyh, berillievyh i alyuminievyh splavov [Strategy of development of titanic, magnesian, beryllium and aluminum alloys] //Aviacionnye materialy i tehnologii. 2012. №S. S. 157–167.
- Kablov E.N., Ospennikova O.G., Vershkov A.V. Redkie metally i redkozemelnye elementy – materialy sovremennyh i budushhih vysokih tehnologij [Rare metals and rare-earth elements – materials for modern and future high technologies] //Trudy VIAM. 2013. №2. St. 01 (viam-works.ru).
- Goncharenko E.S., Trapeznikov A.V., Ogorodov D.V. Litejnye alyuminievye splavy (k 100-letiju so dnja rozhdenija M.B. Altmana) [Aluminum casting alloys (on the 100th anniversary of the birth of M. B. Altman)] //Trudy VIAM. 2014. №4. St. 02 (viam-works.ru).
- Antipov V.V., Senatorova O.G., Tkachenko E.A., Vahromov R.O. Alyuminievye deformiruemye splavy [Aluminum deformable alloys] //Aviacionnye materialy i tehnologii. 2012. №S. S. 167–182.
- Kablov E.N. Korroziya ili zhizn [Corrosion or life] //Nauka i zhizn. 2012. №11. S. 16–21.
- Kablov E.N. Aviakosmicheskoe materialivedenie [Aerospace materials science] //Vse materialy. Entsiklopedicheskiy spravochnik. 2008. №3. S. 2–14.
- Tarasov Yu.M., Antipov V.V. Novye materialy VIAM – dlya perspektivnoj aviacionnoj tehkniki proizvodstva OAO «OAK» [The VIAM new materials – for perspective aviation engineering of production of JSC «OAK»] //Aviacionnye materialy i tehnologii. 2012. №2. S. 5–6.
- Fridlyander I.N., Grushko O.E., Antipov V.V., Kolobnev N.I., Hokhlatova L.B. Aluminiy-litievye splavy [Aluminum-lithium alloys] /V kn.: 75 let Aviatsionnye materialy. Izbrannye Trudy «VIAM» 1932–2007: Yubileynyi nauch.-tehnich. sb. М.: VIAM. 2007. S. 163–171.
- Kablov E.N. Sovremennye materialy – osnova innovatsionnoy modernizatsii Rossii [Modern materials – basis of innovative modernization of Russia] //Metally Evrazii. 2012. №3. S. 10–15.
- Kablov E.N., Lukin V.I., Zhegina I.P., Ioda E.N., Loskutov V.M. Osobennosti I perspektivy svarki alyuminiy-litievyh splavov [Features and perspectives of welding of alyuminiylitiyevy alloys] /V sb. Aviatsionnye materialy i tehnologii. Vyp.: «Tehnologiya proizvodstva aviatsionnyh metallicheskih materilov». M.: VIAM. 2002. S. 3–12.
- Antipov V.V., Kolobnev N.I., Hohlatova L.B. Razvitie alyuminijlitievyh splavov i mnogostupenchatyh rezhimov termicheskoj obrabotki [Development aluminum lithium alloys and multistage modes of thermal processing] //Aviacionnye materialy i tehnologii. 2012. №S. S. 183–195.
- Klochkova Ju.Ju., Grushko O.E., Lancova L.P., Burlyaeva I.P., Ovsyannikov B.V. Osvoenie v promyshlennom proizvodstve polufabrikatov iz perspektivnogo aljuminijlitievogo splava V-1469 [Development in industrial production of semi-finished products from perspective alyuminiylitiyevy alloy V-1469] //Aviacionnye materialy i tehnologii. 2011. №1. S. 8–12.